Strengthening Treatment of Aged Hanji with Water Soluble Polymers  

Kim, Kang-Jae (Dept. of Wood Science and Technology, College of Agriculture and Life Science, Kyungpook National University)
Lee, Min-Hyung (Dept. of Wood Science and Technology, College of Agriculture and Life Science, Kyungpook National University)
Eom, Tae-Jin (Dept. of Wood Science and Technology, College of Agriculture and Life Science, Kyungpook National University)
Publication Information
Journal of Korea Technical Association of The Pulp and Paper Industry / v.43, no.5, 2011 , pp. 1-10 More about this Journal
Abstract
In this study, 13 water soluble polymers(6 natural polymer, 7 synthetic polymer) were treated on Hanji. Mechanical properties, morphology and oxidation index with thermal aging were measured on the aged Hanji, dewaxed Hanji and polymer treated Hanji. 3 natural polymer(such as CMC, EC, MC) and 3 synthetic polymers(such as PVA 1500, 2000, PEG 1500) treated Hanji had higher strength than other polymer treated Hanji. The oxidation index of 3% methyl cellulose solution treated Hanji did a little increase with thermal aging. Finally, methyl cellulose was found to be the most efficient method for strengthening the dewaxed Hanji. The best aging safety and thermal stability were obtained at the methyl cellulose 3% water solution.
Keywords
Hanji; Strengthening treatment; aging; water soluble polymer; cellulose derivatives; methyl cellulose;
Citations & Related Records
Times Cited By KSCI : 3  (Citation Analysis)
연도 인용수 순위
1 Cho, J.H., Kim, K.J., Eom, T.J., Non-constructive analysis for the cover and inner paper in the Taebaeksan volume of Joseon Dynasty annals, J. Korea TAPPI, 42(3): 28-36(2010).
2 Baker, C., Methylcellulose & sodium carboxymethylcellulose: Use in paper conservation, The Book and Paper Group ANNUAl, Vol. 1, The American Institute for Conservation(1982).
3 Franciska, R.L., Maria, T., Paper conservation using aqueous solutions of calcium hydroxide/methylcellulose 2, The influence of accelerated ageing temperature on properties of treated paper, Restaurator, 24: 178-188(2003).
4 Seki, M., Sonoda, N., Morita, T., Okayama, T., A new technique for strengthening book papers using cellulose derivatives, Restaurator, 26: 239-249(2005).
5 Kang, K.H., Kim, H.J., Studies on the reinforcement treatment of aged Hanji using cellulose derivative solutions, J. Korea TAPPI, 43(2): 40-48(2011).
6 Kim, K.J., Eom, T.J., Ageing behavior of beeswax coated Hanji(I) - Thermal ageing test of beeswax coated Hanji -, J. Korea TAPPI, 42(2): 46-52 (2010).
7 Ashori, A., Harun, J., Raverty, W.D., Yusoff, M.N.M., Effect of accelerated aging on properties of kenaf (Hibiscus cannabinus) paper sized with various polymers, Polymer-Plastics Technology and Engineering, 45: 213-216(2006).   DOI   ScienceOn
8 Ashori., A., Raverty., W.D., Vanderhoek., N., Ward, J.V., Surface topography of kenaf (Hibiscus cannabinus) sized papers, Bioresource Technology, 99: 404-410(2008).   DOI   ScienceOn
9 Łojewska, J., Miśkowies, P., Łojewski, T., Proniewicz, L.M., Cellulose oxidation and hydrolytic degradation: In situ FTIR approach, Polymer degradation and stability, 88: 512-520(2005).   DOI   ScienceOn
10 Tasker, S., Badyal, J.P.S., Backson, S.C.E., Richards, R.W., Hydroxyl accessibility in cellulose, Polymer, 4717-4721(1994).
11 송기중, 신병주, 박지선, 이인성, 조선왕조실록 보존을 위한 기초 조사연구(1), 서울대학교출판부, pp.1-16(2005).
12 김강재, 조선왕조실록 밀랍본의 밀랍 특성 및 열화 거동 분석, 경북대학교 석사논문, pp. 1-26(2008).