Effect of CaO and Hot Rolling on the High Temperature Oxidation of Magnesium Alloys  

Xu, Chunyu (School of Advanced Materials Science and Engineering, Sungkyunkwan University)
Trung, Trinh Van (School of Materials Science and Engineering, University of Ulsan)
Won, Sung-Bin (School of Advanced Materials Science and Engineering, Sungkyunkwan University)
Lee, Dong-Bok (School of Advanced Materials Science and Engineering, Sungkyunkwan University)
Publication Information
Journal of the Korean institute of surface engineering / v.45, no.4, 2012 , pp. 155-161 More about this Journal
Abstract
Magnesium alloys of AZ31, AZ31 + (0.5, 1, 1.5)wt.% CaO were cast, hot rolled, and oxidized between 450 and $650^{\circ}C$ in atmospheric air. The added CaO enabled to cast the AZ31 alloy in air. It decomposed and precipitated along the grain boundaries of the AZ31 alloy as $Al_2Ca$. The more the amount of CaO was, the more $Al_2Ca$ formed. The oxidation limit was about $450^{\circ}C$ for the AZ31 alloy. But, It increased to $650^{\circ}C$ in the CaO-added alloys. Hot rolling destroyed the precipitates that formed along the grain boundaries of the AZ31 alloy. During oxidation, MgO oxide scales that incorporated CaO formed at the outer surface of the formed oxide layer.
Keywords
Magnesium alloys; AZ31; CaO; Oxidation;
Citations & Related Records
Times Cited By KSCI : 1  (Citation Analysis)
연도 인용수 순위
1 K. U. Kainer and F. von Buch, Magnesium-Alloys and Technology, K. U. Kainer (Ed.), Wiley-VCH, Germany (2003) 1.
2 W. Ha, J. E. Lee, Y. J. Kim, Mater. Sci. Forum, 475-479 (2005) 2543.   DOI
3 F. C. Erickson, J. F. King, T. Mellerud, Foundry Management & Technology, 126 (1998) 38.
4 J. R. Liu, H. K. Chen, L. Zhao, W. D. Huang, Corros. Sci., 51 (2009) 129.   DOI   ScienceOn
5 M. Sakamoto, S. Akiyama, J. Mater. Sci. Lett., 16 (1997) 1048.   DOI   ScienceOn
6 H. K. Kim, B. H. Seong, G. H. Van, D. H. Kim, Y. R. Seong, S. G. Lim, J. Kor. Foundrymen's Soc., 32 (2012) 75.   DOI
7 B. H. Choi, B. S. You, W. W. Park, I. M. Park, J. Kor. Inst. Met. & Mater., 42 (2004) 673.
8 B. S. You, M. H. kim, W. W. Park, I. S. Chung, J. Kor. Inst. Met. & Mater., 39 (2001) 446.
9 S. L. Cheng, G. C. Yang, J. F. Fan, Y. J. Li, Y. H. Zhou, Trans. Nonferr. Met. Soc. China, 19 (2009) 299.   DOI   ScienceOn
10 T. S. Shih, J. H. Wang, K. Z. Chong, Mater. Chem. Phys., 85 (2004) 302.   DOI   ScienceOn
11 S. K. Kim, Magnesium Alloy and Manufacturing Method Thereof, Kor. Patent 10-1147671 (2011).
12 S. H. Ha, J. K. Lee, H. H. Jo, S. B. Jung, S. K. Kim, Rare Metals, 25 (2006) 150.
13 S. K. Kim, J. K. Lee, Y. O. Yoon, H. H. Jo, J. Mater. Process. Tech., 187-188 (2007) 757.   DOI   ScienceOn
14 D. I. Jang, J. K. Lee, D. U. Kim, S. K. Kim, Trans. Nonferr. Met. Soc. China, 19 (2009) s76.   DOI
15 J. K. Lee, S. K. Kim, Trans. Nonferr. Met. Soc. China, 21 (2011) s23.   DOI   ScienceOn
16 M. Yang, F. Pan, R. Cheng, A. Tang, Mater. Sci. Eng. A, 491 (2008) 440.   DOI   ScienceOn
17 C. Xu, B. Lu, Z. Lu, W. Liang, J. Rare Earth., 26 (2008) 604.   DOI
18 J. H. Kim, N. E. Kang, C. D. Yim, B. K. Kim, Mater. Sci. Eng. A, 525 (2009) 18.   DOI
19 F. Czerwinski, Acta Mater., 50 (2002) 2639.   DOI
20 R. Ninomiya, T. Ojiro, K. Kubota, Acta Metall. Mater., 43 (1995) 669.   DOI
21 B. S. You, W. W. Park, I. S. Chung, Scripta Mater., 42 (2000) 1089.   DOI   ScienceOn
22 Y. Yin, B. B. Argent, J. Phase Equilib., 14 (1993) 588.   DOI