Influence of the Geometry of Guide Groove on Stress Corrosion Index of Rock in Double Torsion Test  

정해식 (서울대학교 지구환경시스템공학부)
미원우삼 (일본 구마모토대학 환경시스템공학과)
전석원 (서울대학교 지구환경시스템공학부)
Publication Information
Tunnel and Underground Space / v.14, no.5, 2004 , pp. 363-372 More about this Journal
Abstract
Double torsion (DT) tests were carried out to investigate the influence of the geometry of guide groove on stress corrosion index of Kumamoto andesite. The fracture toughness was measured in the constant displacement rate, which was set to 2.07 MN/m$^{3}$2/ in average regardless of crack velocity. Stress corrosion indices, n were evaluated using specimens with rectangular, circular and triangular grooves and were 37, 36 and 38 in average, respectively. The n values were constant regardless of the groove geometry, however the DT specimen with triangular groove geometry showed the largest standard deviation in the relationship between crack velocity and stress intensity factor. The DT test was found to be effective in using a rectangular-grooved specimen and the width of the groove must be greater than the average grain size of minerals.
Keywords
Andesite; Double torsion test; Fracture toughness; Stress corrosion index; Guide groove;
Citations & Related Records
연도 인용수 순위
  • Reference
1 Anderson, O.L. and P.C. Grew, 1977, Stress corrosion theory of crack propagation with applications to geophysics, Rev. Geophys. Space Phys., 15, 77-104   DOI
2 Atkinson, B.K. and P.G. Meredith, 1987, The theory of subcritical crack growth with applications to minerals and rocks, in Fracture Mechanics of Rock, edited by Atkinson, B. K., Academic press, London, 111-166
3 Evans, A.G., 1972, A method for evaluating the time dependent failure characteristics of brittle materials and its application to ploycrystalline alumina, J. Mater. Sci., 7, 1137-1146   DOI   ScienceOn
4 Fuller Jr., E.R., 1979, An evaluation of double-torsion testing : Analysis, ASTM STP, 678, 3-18
5 Trantina, G.G., 1977, Stress analysis of the double-torsion specimen, J. Am. Ceram. Soc., 60, 338-341   DOI   ScienceOn
6 Wakai, F., H. Sakuramoto, S. Sakaguchi and Y. Matsuno, 1986, Evaluation of crack propagation in ceramics by double-torsion, Zairyo, 35, 898-903 (in Japanese)
7 Obara, Y., K. Sakaguchi, T. Nakayama and K. Sugawara, 1992, Anisotropy effect on fracture toughness of rock, Proc. ISRM Symposium, Eurock '92, Telford, T., London, 7-12
8 Pletka, B.J., E.R. Fuller and B.G. Koepke, 1979, An evaluation of double-torsion testing experimental, ASTM STP, 678, 19-37
9 Speidel, M.O., 1971, Current understanding of stress corrosion crack growth in aluminum alloys, In: The theory of stress corrosion cracking in alloys, ed. Scully, J.C., North Atlantic Treaty Organization, Brussels, 289-344
10 Bruce J.G. and B.G. Koepke, 1977, Evaluation of $K_{IC}$ by the double-torsion technique, J. Am. Ceram. Soc., 60, 284-285   DOI
11 Jeong, H.S. and Y. Obara, 2002, Strength of Kumamoto andesite in non-atmospheric environments, Shigen-to-Sozai, 118, 599-604(in Japanese)   DOI   ScienceOn
12 Williams, D.P. and A.G. Evans, 1973, A simple method for studying slow crack growth, J. Test. Eval., 1, 264-270   DOI
13 Sano, O., 1988, A revision of the double-torsion technique for brittle materials, J. Mater. Sci., 23, 2505-2511   DOI   ScienceOn
14 Pabst R.F. and J. Weick, 1981, Double-torsion measurements with and without a guiding notch, J. Mater. Sci., 16, 836-838   DOI
15 Evans, A.G. and H. Johnson, 1975, The fracture stress and its dependence on slow crack growth, J. Mater. Sci., 10, 214-222   DOI   ScienceOn
16 Michalske, T.A. and S.W. Freiman, 1982, A molecular interpretation of stress corrosion in silica, Nature, 295, 511-512   DOI