Browse > Article
http://dx.doi.org/10.12989/sem.2020.74.6.747

Temperature development and cracking characteristics of high strength concrete slab at early age  

Wu, Chung-Hao (Department of Civil Engineering, Chung Yuan Christian University)
Lin, Yu-Feng (Department of Civil Engineering, Chienkuo Technology University)
Lin, Shu-Ken (Department of Civil Engineering, National Chung Hsing University)
Huang, Chung-Ho (Department of Civil Engineering, National Taipei University of Technology)
Publication Information
Structural Engineering and Mechanics / v.74, no.6, 2020 , pp. 747-756 More about this Journal
Abstract
High-strength concrete (HSC) generally is made with high amount of cement which may release large amount of hydration heat at early age. The hydration heat will increase the internal temperature of slab and may cause potential cracking. In this study, slab specimens with a dimension of 600 × 600 × 100 mm were cast with concrete incorporating silica fume for test. The thermistors were embedded in the slabs therein to investigate the interior temperature development. The test variables include water-to-binder ratio (0.25, 0.35, 0.40), the cement replacement ratio of silica fume (RSF; 5 %, 10 %, 15 %) and fly ash (RFA; 10 %, 20 %, 30 %). Test results show that reducing the W/B ratio of HSC will enhance the temperature of first heat peak by hydration. The increase of W/B decrease the appearance time of second heat peak, but increase the corresponding maximum temperature. Increase the RSF or decrease the RFA may decrease the appearance time of second heat peak and increase the maximum central temperature of slab. HSC slab with the range of W/B ratio of 0.25 to 0.40 may occur cracking within 4 hours after casting. Reducing W/B may lead to intensive cracking damage, such as more crack number, and larger crack width and length.
Keywords
high-strength concrete; silica fume; fly ash; temperature development; cracking;
Citations & Related Records
Times Cited By KSCI : 6  (Citation Analysis)
연도 인용수 순위
1 ACI Committee 363 (1992), "State-of-the-Art Report on High-Strength Concrete - ACI 363R," USA
2 Al-Fadhala, M. and Hover, K.C. (2001), "Rapid evaporation from freshly cast concrete and the Gulf environment," Cement Build. Mater., 15, 1-7. https://doi.org/10.1016/S0950-0618(00)00064-7.   DOI
3 Al-gburi, M. (2015), "Restraint Effects in Early Age Concrete Structures", Ph.D. Thesis, Lulea Tekniska Universitet.
4 Cha, S.L., Lee, Y., An, G.H. and Kim, J.K., (2016), "Prediction of thermal stress in concrete structures with various restraints using thermal stress device," Comput. Concrete, 17(2), 173-188. https://doi.org/10.12989/cac.2016.17.2.173.   DOI
5 Chen, H.J., Liu, T.H. and Tang, C.W. (2008), "Numerical modeling of drying shrinkage behavior of self-compacting concrete," Comput. Concrete, 5(5), 435-448. https://doi.org/10.12989/cac.2008.5.5.435.   DOI
6 Davis, H.E. (1940), "Autogenous volume change of concrete", Proceeding of the 43th Annual American Society for Testing Materials, 1103-1113.
7 Freedman, S. (1970), "High strength concrete", Modern Concrete, 34(6), 6-10.
8 Gedam, B.A., Bhandari, N.M. and Upadhyay, A. (2014), "An apt material model for drying shrinkage and specific creep of HPC using artificial neural network", Structural Eng. Mech., 52(1), 97-113. http://dx.doi.org/10.12989/sem.2014.52.1.097.   DOI
9 Geng, Y., Li, X.Y., Xue, S.D., Li, J.U. and Song, Y.J. (2018), "Early-age thermal analysis and strain monitoring of massive concrete structures," Comput. Concrete, 21(3), 279-289. https://doi.org/10.12989/cac.2018.21.3.279.   DOI
10 Holt, E. and Leivo, M. (2004), "Cracking risks associated withos.early age shrinkage," Cement Concrete Compos., 26, 521-530. https://doi.org/10.1016/S0958-9465(03)00068-4.   DOI
11 Huo, X.S. and Wong, L.U. (2006), "Experimental study of early-age behavior of high performance concrete deck slabs under different curing methods", Cement Build. Mater., 20(10), 1049-1056. https://doi.org/10.1016/j.conbuildmat.2005.04.001.   DOI
12 Jiang, C.H., Yang, Y., Ni, T. and Wang, X.D. (2015), "Correlating strength of concrete to its early-age temperature rise", Mag. Concrete Res., 67(23), 1274-1286. https://doi.org/10.1680/macr.14.00216.   DOI
13 Langan, B.W., Weng, K. and Ward, M.A. (2002), "Effect of silica fume and fly ash on heat of hydration of Portland cement," Cement Concrete Res., 32(7), 1045-1051. https://doi.org/10.1016/S0008-8846(02)00742-1.   DOI
14 Li, G.D., Wang, Z.L. and Zhao, W.P. (2016), "Early-age autogenous shrinkage and stress characteristics of high-performance concrete at the mesoscopic level", Mag. Concrete Res., 68(16), 809-822. https://doi.org/10.1680/jmacr.15.00183.   DOI
15 Yoo, D.Y., Min, K.H., Lee, J.H. and Yoon, Y.S. (2014), "Shrinkage and cracking of restrained ultra-high-performance fiber-reinforced concrete slabs at early age", Construt. Build. Mater., 73, 357-365. https://doi.org/10.1016/j.conbuildmat.2014.09.097   DOI
16 Mehta, P.K. (1986), Concrete-Strength; Properties, and Materials, 187-191. Prentice-Hall, Inc. Englewood Cliffs, NJ, USA.
17 Mindess, S., Young, J.F. and Darwin, D. (2002), Concrete, Second Ed., 417-418. Prentice-Hall, Inc. Englewood Cliffs, NJ, USA.
18 Mindess, S., Young, J.F. and Darwin, D. (2003), Concrete, Second Ed., Parson Education, Inc., NJ, USA, 57-65. Prentice-Hall, Inc. Englewood Cliffs, NJ, USA.
19 Park, J.J., Yoo, D.Y., Kim, S.W. and Yoon, Y.S. (2014), "Autogenous shrinkage of ultra high performance concrete considering early age coefficient of thermal expansion", Struct. Eng. Mech., 49(6), 763-773. https://doi.org/10.12989/sem.2014.49.6.763.   DOI
20 Park, J.S., Kim, Y.J., Cho, J.R. and Jeon, S.J. (2015), "Early-age strength of ultra-high performance concrete in various curing conditions", Mater., 8(8), 5537-5553. https://doi.org/10.3390/ma8085261.   DOI