Strength and durability studies on high strength concrete using ceramic waste powder  

Karthikeyan, B. (School of Civil Engineering, SASTRA University)
Dhinakaran, G. (School of Civil Engineering, SASTRA University)
Publication Information
Structural Engineering and Mechanics / v.61, no.2, 2017 , pp. 171-181 More about this Journal
Abstract
This paper summarizes the study on effect of ceramic waste powder as partial substitute to cement in binary blend and along with silica fume in ternary blend high strength concrete in normal and aggressive environments. Strength parameters such as compression & tension and durability indices such as corrosion measurement, deterioration, water absorption and porosity were studied. Ceramic waste powder was used in three different percentages namely 5, 10 and 15 with constant percentage of silica fume (1%) as substitutes to cement in ternary blend high strength concrete was investigated. After a detailed investigation, it was understood that concrete with 15% ceramic waste powder registered maximum performance. Increase of ceramic waste powder offered better resistance to deterioration of concrete.
Keywords
ceramic waste powder; $H_2SO_4$; NaCl; half cell potential; compressive strength;
Citations & Related Records
Times Cited By KSCI : 2  (Citation Analysis)
연도 인용수 순위
1 Chidambaram, N., Srikanth, J., Karthikeyan, B. and Dhinakaran, G. (2015), "Mechanical properties and micro structure characteristics of ternary blended concrete with ceramic powder and $SiO_2$", Asian J. Appl. Sci., 8(3), 304-314.
2 Ergun, A. (2011), "Effect of the usage of diatomite and waste marble powder as partial replacement of cement on the mechanical properties of concrete", Constr. Build. Mater., 25(2), 806-812.   DOI
3 Flower, D.J.M. and Sanjayan, J.G. (2007), "Green house gas emissions due to concrete manufacture", Int. J. Life Cycle Assess., 12(5), 282-288.   DOI
4 Guneyisi, E., Gesoglu, M. and Mermerdas, K. (2010), "Strength deterioration of plain and metakaolin concretes in aggressive sulfate environments", J. Mater. Civil Eng., 22(4), 403-407.   DOI
5 Halicka, A., Ogrodnik, P. and Zegardlo, B. (2013),"Using ceramic sanitary ware as concrete aggregate", Constr. Build. Mater., 48, 295-305.   DOI
6 Heidari, A. and Tavakoli, D. (2013), "A study of the mechanical properties of ground ceramic powder concrete incorporating nano-$SiO_2$ particles", Constr. Build. Mater., 38, 255-264.   DOI
7 Jaturapitakkul, C., Kiattikomol, K., Sata, V. and Leekeeratikul, T. (2004), "Use of ground coarse flu ash as a replacement of condensed silica fume in producing high-strength concrete", Cement Concrete Res., 34(4), 549-555.   DOI
8 Jaturapitakkul, C., Kiattilomol, K., Sata, V. and Leekeeratikul, T. (2004), "Use of ground coarse flyash as a replacement of condensed silica fume in producing high-strength concrete", Cement Concrete Res., 34(4), 549-555.   DOI
9 Kartikeyan, B., Sumanth, K., Harshavardhan, G., Rajasekharareddy, A. and Dhinakaran, G. (2014), "Microstructure analysis and strength properties of concrete with nano $SiO_2$", Int. J. Chem Tech. Res., 6(5), 3004-3013.
10 Khatib, J.M., Roger, M. and Clay, R.M. (2004), "Absorption characteristics of metakaolin concrete", Cement Concrete Res., 34(1), 19-29.   DOI
11 Pacheco-Torgal, F. and Jalali, S. (2010), "Reusing ceramic wastes in concrete", Constr. Build. Mater., 24(5), 832-838.   DOI
12 Pradhan, B. (2014), "Corrosion behavior of steel reinforcement in concrete exposed to composite chloride-sulfate environment", Constr. Build. Mater, 72(15), 398-410.   DOI
13 Rajamane, N.P., Peter, J.A., Dattatreya, J.K., Neelamegam, M., and Gopalakrishnan, S. (2003), "Improvement in properties of high performance concrete with partial replacement of concrete by ground granulated blast furnace slag", J. Inst. Eng. India. Civil Eng. Div., 84, 38-42.
14 Senthamarai, R.M., Devadas Manoharan, P. and Gobinath, D. (2011), "Concrete made from ceramic industry waste: Durability properties", Constr. Build. Mater., 25(5), 2413-2419.   DOI
15 Razak, H.A., Chai, M.K. and Wong, H.S. (2004), "Near surface characteristics of concrete containing supplementary cementitious materials", Cement Concrete Compos., 26(7), 883-889.   DOI
16 Saraswathy, V., Muralidharan, S., Thangavel, K. and Srinivasan, S. (2003), "Influence of activated fly ash on corrosionresistance and strength of concrete", Cement Concrete Compos., 25(7), 673-680.   DOI
17 Sayieda, R.Z., Maha R.M., Doaa, A.A. and Aya, H.M. (2015), "Alkali activated Ceramic Waste with or without two different calcium sources", Adv. Mater. Res., 4(3), 133-144.   DOI
18 Shannag, M.J. (2000), "High strength concrete containing natural pozzolan and silica fume", Cement Concrete Compos., 22(6), 399-406.   DOI
19 Sharmila, P. and Dhinakaran, G. (2015), "Effect of nano sized slag on Micro structure, Compressive Strength and durability of Concrete", Strut. Eng. Mech., 55(3), 675-686.   DOI
20 Srikanth, J., Chidambaram, N., Karthikeyan, B. and Dhinakaran, G. (2015), "Resistance to deterioration and water absorption by ternary blended concrete with ceramic powder and $SiO_2$", Int. J. Chem. Tech. Res., 8(2), 696-703.
21 Teng, S., Lim, T.Y.D. and Divsholi, B.S. (2013), "Durability and mechanical properties of high strength concrete incorporating ultra fine ground granulated blast-furnace slag", Constr. Build. Mater., 40, 875-881.   DOI
22 Vejmelkova, E., Keppert, M., Rovnanikova, P., Ondracek, M., Kersner, Z. and cerny, R. (2012), "Properties of high performance concrete containing fine-ground ceramics as supplementary cementitious material", Cement Concrete Compos, 34(1), 55-61.   DOI
23 Appa Rao, G. (2001),"Development of strength with age of mortars containing silica fume", Cem. Conc. Res, 31(8): 1141-1146.   DOI
24 American Society for Testing and Materials (ASTM), Standard Test method for Density, Absorption and voids in Hardened Concrete, ASTM C 642-13, Annual book of ASTM standards, West Conshohockers, United States.
25 American Society for Testing and Materials (ASTM), Standard Test method for Half-Cell Potentials of Uncoated Reinforcing Steel in Concrete, ASTM C 876-91,Annual book of ASTM standards, West Conshohockers, United States.
26 American Society for Testing and Materials (ASTM), Standard Test method for Measurement of Rate of Absorption of water by Hydraulic Cement Concrete, ASTM C 1585-13, Annual book of ASTM standards, West Conshohockers, United States.
27 Atis, C.D. and Bilim, C. (2007), "Wet and dry cured compressive strength of concrete containing ground granulated blast-furnace slag", Build. Environ., 42(8), 3060-3065.   DOI
28 Chalee, W., Ausapanit, P. and Jaturapitakkul, C. (2010), "Utilization of fly ash concrete in marine environment for long term design life analysis", Mater. Des., 31(3), 1242-1249.   DOI
29 Ay, N. and Unal, M. (2000), "The use of waste ceramic tile in cement production", Cement Concrete Res., 30, 497-499.   DOI
30 BS 1881-108 (1983), "Testing concrete - Method for making test cubes from fresh concrete", British Standards Institution, 2 Park Street London W1 A 2BS.
31 Cheriyan, S.G., Dhanya, B.S. and Santhanam, M. (2014), "Durability indices for concretes with different dosages of mineral admixtures", India Concrete J., 88(3), 60-68.