Degradation Behaviors of Poly(l-lactide) using Model Systems  

Min Seong-Kee (Division of Chemical Engienering, Pukyong National University)
Moon Myong-Jun (Division of Chemical Engienering, Pukyong National University)
Lee Won-Ki (Division of Chemical Engienering, Pukyong National University)
Publication Information
Journal of Environmental Science International / v.15, no.2, 2006 , pp. 177-183 More about this Journal
Abstract
The hydrolytic kinetics of biodegradable poly(l-lactide) (PLLA) have been studied by using two model systems, solution-grown single crystal (SC) and Langmuir monolayer techniques, for elucidating the mechanism for both alkaline and enzymatic degradations. The present study investigated the parameters such as degradation medium and time. The Langmuir mono layers of PLLA showed faster rates of hydrolysis when they were exposed to a basic subphase rather than they did when exposed to neutral subphase. Both degradation mediums had moderate concentrations to show a maximized activity, depending on their sizes. An alkaline degradation of SCs of PLLA showed the decrease of molecular weight of the remained crystals due to the erosion of chain-folding surface. However, the enzymatic degradation of SCs of PLLA occurred in the crystal edges thus the molecular weight of remained crystals was not changed. This behavior might be attributed to the size of enzymes which is much larger than that of alkaline ions; that is, the enzymes need larger contact area with monolayers to be activated.
Keywords
Poly(l-lactide); Langmuir monolayer; Solution-grown crystals; Degradation;
Citations & Related Records
연도 인용수 순위
  • Reference
1 Scott, G., 2002, Degradable Polymers 2nd Ed.: Kluwer Academic Publ.: London, pp. 1-13
2 Reeve, M. S., S. P. McCarthy, M. J. Downey, R. A. Gross, 1994, Polylactides stereoche­mistry: Effect on enzymatic degradability, Macromolecules, 27, 825-831   DOI
3 Fredericks, R. J., A. J. Melverger and L. J. Dolegiewtz, 1984, Morphological and structural changes in a copolymer of glycolide and lactide occurring as a result of hydrolysis, J. Polym. Sci.: Polym. Phys. Ed., 22, 57-66   DOI
4 Nakamura, T., S. Hitomi, S. Watanabe, Y. Shimizu, S. H. Hyun and Y. Ikeda, 1985, Bioabsorption of polylactides with different molecular properties, J. Biomed. Mater. Res., 23, 1115-1130   DOI   ScienceOn
5 Miyata, T. and T. Masuko, 1997, Morphology of poly(l-lactide) solution-grown crystals. poly­mer, 38, 4003-4009   DOI   ScienceOn
6 Chu, C. C., 1981, An in vitro study of the effect of buffer on the degradation of poly (glycolic acid) stutures, J. Biomed. Mater. Res., 15, 19-27   DOI   ScienceOn
7 김영욱, 조원영, 조동만, 1994, 전분충진형 생분해성 고분자의 특성, 고분자과학과 기술, 5, 19-23
8 Furukawa, T., Y. Matsusue, T. Yasunaga, Y. Shikinarni, M. Okuno and T. Nakamura, 2000, Hisomorphometric study on high-strength hydroxyapatite/poly(l-lactide) composite rods for internal fixation of bone fractures, J. Biomed. Mater. Res., 50, 410-419   DOI   ScienceOn
9 Li, S. and S. McCarthy, 1999, Influence of crystallinity and stereochemistry on the enzy­matic degradation of poly(lactide)s, Macro­molecules, 32, 4454-4456   DOI   ScienceOn
10 Lee, W. K. and J. A. Gardella, Jr., 2000, Hydrolytic kinetics of biodegradable polyester monolayers, Langmuir, 16, 3401-3406   DOI   ScienceOn
11 Nobes, G. A. R., R. H. Marchessault, H. Chanzy, B. H. Briese and D. Jendrossek, 1996, Spintering of poly(3-hydroxybutyrate) single crystals by PHB-depolymerase A from Pseudomonas lemoignei, Macromolecules, 29, 8330-8336   DOI   ScienceOn
12 Iwata, T. and Y. Doi, 1999, Crystal structure and biodegradation of aliphatic polyester crystals, Macromol. Chem. Phys., 200, 2429-­2442   DOI
13 Lee, W. K., N. Richard and J. A. Gardella, Jr., 2002, The hydrolytic degradation of polyester blend monolayers at the air/liquid interface: effects of a slowly degrading component, Langmuir, 18, 2309-2312   DOI   ScienceOn
14 Fujita, M. and Y. Doi, 2004, Annealing and melting behavior of poly(1-lactic acid) single crystals as revealed by in situ atomic force microscopy, Biomacromolecules, 4, 1301-1307   DOI   ScienceOn
15 Iwata, T., Y. Doi, F. Kohubu and S. Terarnachi, 1999, Alkaline hydrolysis of solu­tion-grown poly(3-hydroxybutyrate) single cry­stals, Macromolecules, 32, 8325-8330   DOI   ScienceOn
16 Lee, W. K., T Iwata, H. Abe and Y. Doi, 2000, Studies on the enzymatic hydrolysis of solution-grown poly[(R)- 3-hydroxybutyrate] crystals; defects in crystals, Macromolecules, 33, 9535-9541   DOI   ScienceOn
17 Roberts, G., 1990, Langmuir-Blodgett Films: Plenum Press: New York, pp.18-19
18 Eliaz, R. E. and J. Kost, 2000, Charac­terization of a polymeric PLGA-injectable implant delivery system for the controlled release of proteins, J. Biomed. Mater. Res., 50, 388-396   DOI   ScienceOn
19 Albertsson, A. C. and S. Karlsson, 1990, Degradable materials: Biodegradation and test methods for environmental and biomedical applications of polymers: CRC Press: Boca Raton, pp. 263-286
20 Albertsson, A. C., C. Barenstedt and S. Karlsson, 1992, Susceptibility of enhanced environmentally degradable polyethylene to thermal and photooxidation, Polym. Degrad. Stab., 37, 163-171   DOI   ScienceOn
21 Abe, H., H. Aoki and Y. Doi, 1998, Mor­phologies and enzymatic degradability of melt­crystallized poly(3-hydroxybutyric acid-co-6­hydroxyheanoic acid), Macromol. Symp., 130, 81-89
22 Lee, W. K., J. H. Ryou and C. S. Ha, 2003, Retardation of enzymatic degradation of microbial polyesters using surface chemistry: effect of addition of non-degradable polymers, Surface Science, 542(3), 235-243   DOI   ScienceOn
23 Mauduit, J., N. Bukh and M. Vert, 1993, Gentamycin/poly(lactic acid) blends aimed at sustained release local antibiotic therapy administered per-operatively: III The case of gentamycin sulfate in films of high and low molecular weight poly(dl-lactic acid), J. Control. Rel., 25, 43-49   DOI   ScienceOn
24 Chu, C. C., 1981, Hydrolytic degradation of poly (glycolic acid): tensile strength and crystallinity study, J. Appl. Poly. Sci., 26, 1727-1734   DOI   ScienceOn
25 강태규, 정호갑, 윤상준, 1994, 광분해성 고분자의 개발 현황, 고분자과학과 기술, 5, 24-28
26 Bergsma, J. E., W. C. de Bruijn, F. R. Rorema, R. R. M. Bos and G. Boering, 1995, Late degradation tissue response to poly (1-lactide) bone plates and screws, Biomater, 16, 25-31   DOI   ScienceOn
27 Doi, Y. and K. Fukuda, 1993, Biodegradable Plastics and Polymers: Elsevier Sci.: Am­sterdam, pp. 79-91