In this paper, we fabricated flexible CNT/PVDF piezoelectric composite device by introducing CNTs (carbon nanotubes) into PVDF (poly-vinylidene fluoride) solution using spray coating technique. Flexible PEDOT:PSS conducting polymer was used as electrodes. We tried to improve the piezoelectric performance from the CNT/PVDF composite film by increasing the portion of the ${\beta}$-phase PVDF in the film. We confirmed the structural conformation of the CNT/PVDF composite film as a function of CNT concentration by using FT-IR (fourier transform infra-red). As increasing CNT concentration, portion of the ${\beta}$-phase PVDF and resulting piezoelectric performance increased in the CNT/PVDF composite film. We found that CNTs introduced were played as seeds for formation of the ${\beta}$-phase PVDF in the CNT/PVDF composite film and resulting improvement of the piezoelectric performance.
Keywords
Formation of the ${\beta}$-phase PVDF; CNTs introduced as seeds; Improvement of piezoelectric performance;
Citations & Related Records
Times Cited By KSCI : 1  (Citation Analysis)
연도 인용수 순위
1 R. Yang, Y. Qin, C. Li, G. Zhu, and Z. L. Wang, Nano Lett., 9, 1201 (2009). [DOI: http://dx.doi.org/10.1021/nl803904b]   DOI
2 X. Chen, S. Xu, N. Yao, and Y. Shi, Nano Lett., 10, 2133 (2010). [DOI: http://dx.doi.org/10.1021/nl100812k]   DOI
3 A. M. Vinogradov, V. H. Schmidt, G. F. Tuthill, and G. W. Bohannan, Mech. Mater., 36, 1007 (2004). [DOI: http://dx.doi.org/10.1016/j.mechmat.2003.04.002]   DOI
4 P. Ueberschlag, Sensor Review, 21, 118 (2001). [DOI: http://dx.doi.org/10.1108/02602280110388315]   DOI
5 W. Ma, J. Zhang, S. Chen, and X. Wang, J. Macromol. Sci. Phys., B47, 434 (2008). [DOI: http://dx.doi.org/10.1080/00222340801954811]
6 B. Mohammadi, A. A. Yousefi, and S. M. Bellah, Polym. Test., 26, 42 (2007). [DOI: http://dx.doi.org/10.1016/j.polymertesting.2006.08.003]   DOI
7 S.A.C. Carabineiro, M.F.R. Pereira, J. N. Pereira, C. Caparros, V. Sencadas, and S. L. Mendez, Nanoscale Res. Lett., 6, 1 (2011).
8 E. E. Shafee, M. E. Gamal, and M. Isa, J. Polym. Res., 19, 1 (2012). [DOI: http://dx.doi.org/10.1007/s10965-011-9805-1]   DOI
9 L. Li, B. Li, M. A. Hood, and C. Y. Li, Polymer, 50, 953 (2009). [DOI: http://dx.doi.org/10.1016/j.polymer.2008.12.031]   DOI
10 J. J. Peterson, M. Werre, Y. C. Simon, E. B. Coughlin, and K. R. Carter, Macromolecules, 42, 8594 (2009). [DOI: http://dx.doi.org/10.1021/ma901703r]   DOI
11 S. Lee, J. Korean Inst. Electr. Electron. Mater. Eng., 28, 462 (2015). [DOI: http://dx.doi.org/10.4313/JKEM.2015.28.7.462]