Browse > Article
http://dx.doi.org/10.5012/jkcs.2013.57.2.272

Ginger Extract as Green Corrosion Inhibitor for Steel in Sulfide Polluted Salt Water  

Fouda, Abd El-Aziz S. (Department of Chemistry, Faculty of Science, El-Mansoura University)
Nazeer, Ahmed Abdel (National Research Center, Electrochemistry and Corrosion Lab.)
Ibrahim, Mohamed (Water and waste water company)
Fakih, Mohamed (Water and waste water company)
Publication Information
Abstract
Extract of ginger has been evaluated as a green inhibitor for the corrosion of steel in sulfide polluted NaCl solution using potentiodynamic polarization, electrochemical impedance spectroscopy (EIS) and electrochemical frequency modulation (EFM) techniques. Potentiodynamic polarization measurements showed that this extract acts as a mixed type inhibitor but mainly inhibits the cathodic reaction. The inhibition efficiency was found to increase with inhibitor concentration reaching to approximately 83.9% using 250 ppm of ginger. Nyquist plots show a single capacitive loop in uninhibited and inhibited solutions. From EFM the causality factors are very close to theoretical values which indicate that the measured data are of good quality. The adsorption process of the studied extract on steel surface obeys Temkin adsorption isotherm. The results obtained from the different electrochemical techniques were in good agreement which prove the validity of these tools in measurement of corrosion rate. Ginger extract has no effect on Escherichia Coli and can be applied safely on waste water treatment plants.
Keywords
Corrosion inhibition; Steel; NaCl; $Na_2S$; Green inhibitor (ginger);
Citations & Related Records
연도 인용수 순위
  • Reference
1 El-Etre, A. Y. J. Colloid Interface Sci. 2007, 314, 578.   DOI   ScienceOn
2 El-Etre, A. Y. Appl. Surf. Sci. 2006, 252, 8521.   DOI   ScienceOn
3 Benabdellah, M.; Benkaddour, M.; Hammouti, B.; Bendahhou, M.; Aouniti, A. Appl. Surf. Sci. 2006, 252, 6212.   DOI   ScienceOn
4 Chaieb, E.; Bouyanzer, A.; Hammouti, B.; Benkaddour, M. Appl. Surf. Sci. 2005, 246, 199.   DOI   ScienceOn
5 Muller, B. Corros. Sci. 2002, 44, 1583.   DOI   ScienceOn
6 Li, Y.; Zhao, P.; Liang, Q. Hou, B. Appl. Surf. Sci. 2005, 252, 1245.   DOI   ScienceOn
7 El-Etre, A. Y.; Abdallah, M.; El-Tantawy, Z. E. Corros. Sci. 2005, 47, 385.   DOI   ScienceOn
8 Bouyanzer, Hammouti, B.; Majidi, L. Mater. Lett. 2006, 60, 2840.   DOI   ScienceOn
9 El-Etre, A. Y. Corros. Sci. 2003, 45, 2485.   DOI   ScienceOn
10 Ammar, I. A.; Darwish, S. Corros. Sci. 1967, 7, 679.
11 Fisher, H. Ann. Univ. Ferrera. Sez. 1960, 3 (Suppl. 3), 1.
12 Stupnisek-Lisac, E.; Gazivoda A.; Madzarac, M. J. Electrochim. Acta 2002, 47, 4189.   DOI   ScienceOn
13 Szklarska-Smiaiowska, Z. Electrochemical and Optical Techniques for the Study of Metallic Corrosion; Kluwer Academic: Netherlands, 1991, p 545.
14 Khamis, E. Corrosion 1990, 46, 476.   DOI
15 Ramachandran, S.; Tsai, M.; Blanco, M.; Chen, H.; Tang, W. A. Langmuir 1996, 12, 6419.   DOI   ScienceOn
16 Oguzie, E. E. Corros. Sci. 2007, 49, 1527.   DOI   ScienceOn
17 Larabi, L.; Benali, O.; M.Mekelleche, S.; Harek, Y.; J. Appl. Surf. Sci. 2006, 253, 1371.   DOI   ScienceOn
18 Lagrenee, M.; Mernari, B.; Bouanis, B.; Traisnel M.; Bentiss, F.; Corros. Sci. 2002, 44, 573.   DOI   ScienceOn
19 Bessone, J.; Mayer, C.; Tuttner, K.; Lorenz, W. J. Electrochim. Acta 1983, 28, 171.   DOI   ScienceOn
20 Epelboin, I.; Keddam M.; Takenouti, H. J. Appl. Electrochem. 1972, 2, 71.   DOI
21 Khaled, K. F. Electrochim. Acta 2008, 53, 3484.   DOI   ScienceOn
22 Khamis, E.; Bellucci, F.; Latahision, R. M.; El-Ashry E. Sh. Corrosion 1991, 47(9), 667.
23 Abdel-Rehim, S. S.; Khaled, K. F.; Abd-Elshafi, N. S. Electrochim. Acta 2006, 51(16), 3269.   DOI   ScienceOn