Browse > Article
http://dx.doi.org/10.5658/WOOD.2020.48.6.896

Chemical Properties of Artificially Buried Wood in an Intertidal Zone during the Deterioration Period  

SEO, Sujin (Department of Wood Science and Engineering, College of Agriculture and Life Sciences, Chonnam National University)
KIM, Taekjoon (National Research Institute of Maritime Cultural Heritage)
LEE, Jae-Won (Department of Wood Science and Engineering, College of Agriculture and Life Sciences, Chonnam National University)
Publication Information
Journal of the Korean Wood Science and Technology / v.48, no.6, 2020 , pp. 896-906 More about this Journal
Abstract
Wood deterioration experiments were carried out for 6 months in an intertidal zone of South Korea to monitor the changes in the chemical properties of two types of species, Korean red pine and sawtooth oak. The results of FT-IR spectra and XRD patterns have shown that the chemical properties of the wood did not change significantly during the 6-month burial period. However, the brightness of the surface decreased after burial; the value of the sawtooth oak sample was lower than that of the Korean red pine sample owing to an accumulation of inorganic compounds in cell lumen as observed by ICP analysis. Among the inorganic compounds, sodium and sulfur concentrations increased significantly over the burial period compared with the control. Further, the maximum moisture content decreased from 199% to 136% in the Korean red pine and 62% to 60% for the sawtooth oak. Nevertheless, the major chemical composition of both the wood species did not change significantly during the 6-month burial period, whereas, the crystallinity decreased with an increasing burial period owing to an accumulation of inorganic compounds in the lumen.
Keywords
waterlogged wood; deterioration; artificially buried wood; intertidal zone;
Citations & Related Records
Times Cited By KSCI : 10  (Citation Analysis)
연도 인용수 순위
1 Remazeilles, C., Leveque, F., Conforto, E., Meunier, L., Refait, P. 2019. Contribution of magnetic measurement methods to the analysis of iron sulfides in archaeological waterlogged wood-iron assemblies. Microchemical Journal 148: 10-20.   DOI
2 Sandak, A., Sandak, J., Babinski, L., Pauliny, D., Riggio, M. 2014. Spectral analysis of changes to pine and oak wood natural polymers after short-term waterlogging. Polymer Degradation and Stability 99: 68-79.   DOI
3 Segal, L., Creely, J., Martin Jr, A., Conrad, C. 1959. An empirical method for estimating the degree of crystallinity of native cellulose using the X-ray diffractometer. Textile Research Journal 29(10): 786-794.   DOI
4 Selig, M., Weiss, N., Ji, Y. 2008. Laboratory Analytical Procedure No. TP-510-42629.
5 Singh, A.P. 2012. A review of microbial decay types found in wooden objects of cultural heritage recovered from buried and waterlogged environments. Journal of Cultural Heritage 13(3): 16-20.   DOI
6 Sjostrom, E. 1981. Wood Chemistry: Fundamentals and Application. Academic press, New York.
7 Tamburini, D., Lucejko, J.J., Pizzo, B., Mohammed, M.Y., Sloggett, R., Colombini, M.P. 2017. A critical evaluation of the degradation state of dry archaeological wood from Egypt by SEM, ATR-FTIR, wet chemical analysis and Py(HMDS)-GC-MS. Polymer Degradation and Stability 146: 140-154.   DOI
8 Traore, M., Kaal, J., Cortizas, A.M. 2016. Application of FTIR spectroscopy to the characterization of archeological wood. Spectrochimica Acta Part A: Molecular and Biomolecular Spectroscopy 153: 63-70.   DOI
9 Yi, Y.H. 1997. Conservation of waterlogged wooden finds excavated in wet-site. Journal of Conservation Science 6(2): 126-140.
10 Zisi, A., Dix, J.K. 2018. Simulating mass loss of decaying waterlogged wood: A technique for studying ultrasound propagation velocity in waterlogged archaeological wood. Journal of Cultural Heritage 33: 39-47.   DOI
11 Hwang, I.W., Park, J.H., Kim, S.C. 2018. A study on the optical characteristics according to the lacquer drying conditions for the conservation of lacquerwares. Journal of the Korean Wood Science and Technology 46(56): 610-621.
12 Kim, Y-S. 2017. Current researches on the weathering of wood. Journal of the Korean Wood Science and Technology 45(5): 483-494.   DOI
13 Kim, Y-S. 2018. Current researches on the protection of exterior wood from weathering. Journal of the Korean Wood Science and Technology 46(5): 449-470.   DOI
14 Komorowicz, M., Wroblewska, H., Fojutowski, A., Kropacz, A., Noskowiak, A., Pomian, I. 2018. The impact of 5 years' underwater exposure in the Baltic Sea (Puck Bay) on selected properties of English oak wood samples. International Biodeterioration & Biodegradation 131: 40-50.   DOI
15 Korea Standards and Certifications. 2016. Determination of Moisture Content of Wood (KS F 2199).
16 Koshijima, T. 1960. Study on mannan in wood pulp. Journal of the Agricultural Chemical Society of Japan 24(7): 682-692.
17 Kundu, C., Lee, J.W. 2015. Optimization conditions for oxalic acid pretreatment of deacetylated yellow poplar for ethanol; production. Journal of Industrial and Engineering Chemical 32: 298-304.   DOI
18 Lucejko, J.J., Mattonai, M., Zborowska, M., Tamburini, D., Cofta, G., Cantisani, E., Kudela J., Cartwright C., Colombini M.P., Ribechini, E. Modugno F. 2018. Deterioration effects of wet environments and brown rot fungus Coniophora puteana on pine wood in the archaeological site of Biskupin (Poland). Microchemical Journal 138: 132-146.   DOI
19 McGee, J.K., April, G.C. 1982. Chemicals from renewable resources-hemicellulose behavior during organosolv delignification of southern yellow pine. Chemical Engineering Communications 19(1-3): 49-56.   DOI
20 Macchioni, N., Pizzo, B., Capretti, C., Giachi, G. 2012. How an integrated diagnostic approach can help in a correct evaluation state of preservation of waterlogged archaeological wooden artefacts. Journal of Archaeological Science 39(10): 3255-3263.   DOI
21 Monachon, M., Berenguer, M.A., Peleb, C., Cornet, E., Guilminot, E., Remazeilles, C., Joseph, E. 2020. Characterization of model samples simulating degradation processes induced by iron and sulfur species on waterlogged wood. Microchemical Journal 155: 104756   DOI
22 Nilsson, T., Bjordal, C. 2008. Culturing wood-degrading erosion bacteria. International Biodeterioration & Biodegradation 61(1): 3-10.   DOI
23 Oron, A., Liphschitz, N., Held, B.W., Galili, E., Klein, M., Linker, R., Blanchette, R.A. 2016. Characterization of archaeological waterlogged wooden objects exposed on the hyper-saline Dead Sea shore. Journal of Archaeological Science: Reports 9: 73-86.   DOI
24 Ozgenc, O., Durmaz, S., Serdar, B., Boyaci, I.H., Eksi-Kocak, H., Ozturk, M. 2018. Characterization of fossil Sequoioxylon wood using analytical instrumental techniques. Vibrational Spectroscopy 96: 10-18.   DOI
25 Almkvist, G., Persson, I. 2008. Analysis of acids and degradation products related to iron and sulfur in the Swedish warship Vasa. Holzforschung 62(6): 694-703.   DOI
26 Colombini, M.P., Lucejko, J.J., Modugno, F., Orlandi, M., Tolppa, E.L., Zoia, L. 2009. A multi-analytical study of degradation of lignin in archaeological waterlogged wood. Talanta 80(1): 61-70.   DOI
27 Bjordal, C.G. 2012. Microbial degradation of waterlogged archaeological wood. Journal of Cultural Heritage 13(3): 118-122.
28 Bjordal, C.G., Nilsson, T., Daniel, G. 1999. Microbial decay of waterlogged archaeological wood found in Sweden applicable to archaeology and conservation. International Biodeterioration & Biodegradation 43(1-2): 63-73.   DOI
29 Broda, M., Mazela, B. 2017. Application of methyltrimethoxysilane to increase dimensional stability of waterlogged wood. Journal of Cultural Heritage 25: 149-156.   DOI
30 Cogulet, A., Blanchet, P., Landry, V. 2016. Wood degradation under UV irradiation: A lignin characterization. Journal of Photochemistry and Photobiology B: Biology 158: 184-191.   DOI
31 Gelbrich, J., Mai, C., Militz, H. 2008. Chemical changes in wood degradation by bacteria. International Biodeterioration & Biodegradation 61(1): 24-32.   DOI
32 Grattan, D.W. 1987. 3-Waterlogged wood. Conservation of Marine Archaeological Objects: 55-67.
33 Hadi, Y.S., Massijaya, M.Y., Abdillah, I.B., Pari, G., Arsyad, W.O.M. 2020. Color change and resistance to subterranean termite attack of mangium (Acacia mangium) and sengon (Falcataria moluccana) smoked wood. Journal of the Korean Wood Science and Technology 48(1): 1-11.   DOI
34 Park, Y., Han, Y., Park, J-H, Chung, H., Kim, H., Yang, S., Chang, Y-S, Yeo, H. 2018. Evaluation of deterioration of Larix kaempferi wood heat-treated by superheated steam through field decay test for 12 months. Journal of the Korean Wood Science and Technology 46(5): 497-510.   DOI