Abstract
In order to develop the end use of cylindrical laminated veneer lumber (LVL) such as wooden crafts, the water proof-bonding strength, the resistance to abrasion and the surface hardness by painting the surface of LVL were investigated. The study results were as follows; The water proof-bonding strength through 5 cyclic test by boiling in water immersion and drying were favorable without delamination of glue line. Then the formulation of glue was resorcinol resin (100) to hardener of paraformaldehyde (5) by mixed weight percentage. The resistance to abrasion was relatively higher at cross section than tangential section. When tangential section of LVL was painted by UV protection oil, the resistance to abrasion was improved. In case of an cross section of LVL, the higher surface hardness appeared at larch core than radiata pine LVL. Also, in case of an tangential section of LVL, the higher surface hardness appeared at glue line than veneer side.
Keywords
cylindrical laminated veneer lumber; water proof-bonding strength; resistance to abrasion; painting; surface hardness;
Citations & Related Records
Times Cited By KSCI : 1  (Citation Analysis)
연도 인용수 순위
1 강춘원, 김남훈, 김병로, 김영숙, 변희섭, 소원택, 여환명, 오승원, 이원희, 이화형. 2008. 신고 목재물리 및 역학. 향문사: 308-307.
2 오세창. 2011. 단판적층재(LVL)의 전단강도 시험방법 에 관한 비교 연구. 대한건축학회논문집 구조계 27(12): 41-48.
3 이남호, 김광철. 2011. 스킨팀버 제조기술 및 용도개발. 산림청.
4 한국표준협회. 2004. 목재의 경도시험 방법. KS F 2212.
5 한국표준협회. 2008. 천연무늬목 치장 마루판-내마모성 시험 방법. KS F 3111.
6 홍순일. 1999. 상대습도 변동하의 휨 모멘트가 작용하는 단판적층재 Drift Pin 결합부의 크리프 변형 거동. 임산에너지 19(2): 84-91.
7 Berard, P., P. Yang, H. Yamauchi, K. Umemura, and S. Kawai. 2011. Modeling of a cylindrical laminated veneer lumber I: mechnical properties of hinoki (Chamaecyparis obtusa) and the reliability of a nonlinear finite elements model of a four-point bending test. J Wood Sci 57: 100-106.   DOI
8 Berard, P., P. Yang, H. Yamauchi, K. Umemura, and S. Kawai. 2011. Modeling of a cylindrical laminated veneer lumber II: a nonlinear finite element model to improve the quality of the butt joint. J. Wood Sci. 57: 107-113.   DOI
9 Hata, T., K. Umemura, and S. Kawai. 1998. Continuous manufacturing of cylindrical-LVL by using "spiral-winding method". 47rd Annual meeting of Japan wood research society: 92-95.
10 Hata, T., K. Umemura, H. Yamauchi, A. Nakayama, S. Kawai, and H. Sasaki. 2001. Design and pilot production of a "spiral-winder" for the manufacture of cylindrical laminated veneer lumber. J. Wood Sci. 47: 115-123.   DOI   ScienceOn
11 Inaba, D., M. Morita, H. Nakano, A. Takenaka, and S. Kawai. 2003. Continuous manufacture of cylindrical laminated veneer lumber. 53rd Annual meeting of Japan wood research society: 19-20.
12 (財)日本合板檢査會. 2003. 構造用單板積層材の日本農林規格.