Abstract
As engineered timber such as Glulam is seeing increasing use in tall timber buildings, building codes are adapting to allow for this. In order for this material to be used confidently and safely in one of these applications, there is a need to understand the effects that fire can have on an engineered timber structural member. The post-fire resilience aspect of glulam is studied herein. Two sets of experiments are performed to consider the validity of zero strength guidance with respect to short duration fire exposure on thin glulam members. Small scale samples were heated in a cone calorimeter to different fire severities. These samples illustrated significant strength loss but high variability despite controlled quantification of char layers. Large scale samples were heated locally using a controlled fuel fire in shear and moment locations along the length of the beam respectively. Additionally, reduced cross section samples were created by mechanically carving a way an area of cross section equal to the area lost to char on the heated beams. All of the samples were then loaded to failure in four-point (laterally restrained) bending tests. The beams that have been burnt in the shear region were observed as having a reduction in strength of up to 34.5% from the control beams. These test samples displayed relatively little variability, apart from beams that displayed material defects. The suite of testing indicated that zero strength guidance may be under conservative and may require increasing from 7 mm up to as much as 23 mm.
Keywords
Glulam; Radiant heat; Adhesive; Tall timber;
Citations & Related Records
연도 인용수 순위
  • Reference
1 CSA O86-14. (2016). Engineering design in wood, CSA Group, Mississauga, Canada.
2 DiDomizio, M. J., Mulherin, P., and Weckman, E. J. (2016). "Ignition of wood under time-varying radiant exposures." Fire Safety Journal 82. 131-144.   DOI
3 Emberley, R., Nicolaidis, A., Fernando, D., Torero, J. L. (2016). "Changing Failure Modes of Cross-Laminated Timber." Structures in Fire, Proceedings of the 9th international conference, New Jersey, USA. 643-649.
4 Frangi, A., Fontana, M. and Mischler, A. (2004). "Shear behaviour of bond lines in glued laminated timber beams at high temperatures." Wood Science and Technology 38. 119-126. doi:10.1007/s00226-004-0223-y   DOI
5 Gales, J., Zhou, A., Smith M., Braxton, N., Smith, C., and LaMalva, K. (2018). Chapter 11: Acceptance Criterion, Structural Fire Engineering Manual of Practice, ASCE, Virginia, USA. 15 pp.
6 Hadden, R. M., Bartlett, A. I., Hidalgo, J. P., Santamaria, S., Wiesner, F., Bisby, L. A., Deeny, S., Lane, B. (2017). "Effects of exposed cross laminated timber on compartment fire dynamics." Fire Safety Journal 91. 480-489.   DOI
7 Hopkin, D., Schmid, J., Friquin, K. (2016). "Timber Structures Subject to Non-Standard Fire Exposure - Advances and Challenges." WCTE. 12 pp.
8 Jeanneret, C., Smith, M., and Gales, J. (2017). "Fire safety towards enabling timber structures in Canada." Applications of Structural Fire Engineering.
9 National Research Council of Canada, Canadian Commission on Building and Fire Codes. (2015). National Building Code of Canada, National Research Council of Canada, Ottawa, ON.
10 Lange, D., Boström, L., Schmid, J., Albrektsson, J. (2015). "The Reduced Cross Section Method Applied to Glulam Timber Exposed to Non-standard Fire Curves." Fire Technology 51. 1311-1340. doi:10.1007/s10694-015-0485-y   DOI
11 Nicolaidis, A., Emberley, R., Fernando, D., Torero, J. L. (2016). "Thermally Driven Failure Mode Changes in Bonded Timber Joints." Proceedings of World Conference on Timber Engineering, WCTE 2016, Vienna, Austria.
12 Quiquero, H., Gales, J., and Hadjisophocleous, G. (2016). "Behaviour of Char Layer in Fire-Damaged Box Section Timber Beams." Interflam 2016. 1063-1074.
13 Stanier, S.A., Blaber, J., Take, W.A. and White, D.J. (2015). "Improved image-based deformation measurement for geotechnical applications." Canadian Geotechnical Journal, 53(5): 727-739   DOI
14 Quiquero, H. and Gales, J. (2017). "Comparing timber adhesive shear strength properties after fire damage." Fire and Materials, California, USA. 556-566.
15 Reszka, P. and Torero, J. L. (2008). "In-depth temperature measurements in wood exposed to intense radiant energy," Experimental Thermal and Fluid Science 32. 1405-1411. doi:10.1016/j.expthermflusci.2007.11.014   DOI
16 Spearpoint, M. J. and Quintiere, J. G. (2001). "Predicting the piloted ignition of wood in the cone calorimeter using an integral model - effect of species, grain orientation and heat flux." Fire Safety Journal 36. 391-415.   DOI
17 Su J., Lafrance P.S., Hoehler M., and Bundy M. (2018). Fire Safety Challenges of Tall Wood Buildings - Phase 2: Task 2 & 3 - Cross Laminated Timber Compartment Fire Tests. FPRF. 397 pp.
18 Yang, J. C. et al. (2015). International R&D Roadmap for Fire Resistance of Structures: Summary of NIST/CIB Workshop, National Institute of Standards and Technology, Maryland, USA.