Browse > Article
http://dx.doi.org/10.5714/CL.2011.12.2.107

Effects of positive and negative stretching on the structure and properties of polyacrylonitrile fibers in the pre-oxidation process  

Wang, Liang (State Key Laboratory of Chemical Resource Engineering, Beijing University of Chemical Technology)
Lu, Wei (State Key Laboratory of Chemical Resource Engineering, Beijing University of Chemical Technology)
Zhang, Li (State Key Laboratory of Chemical Resource Engineering, Beijing University of Chemical Technology)
Xue, Liwei (State Key Laboratory of Chemical Resource Engineering, Beijing University of Chemical Technology)
Ryu, Seung-Kon (Department of Chemical Engineering, Chungnam National University)
Jin, Ri-guang (State Key Laboratory of Chemical Resource Engineering, Beijing University of Chemical Technology)
Publication Information
Carbon letters / v.12, no.2, 2011 , pp. 107-111 More about this Journal
Abstract
Polyacrylonitrile (PAN) fibers were pre-oxidized in a temperature range of 180-275$^{\circ}C$. The effects of positive and negative stretching on the structure and morphology of PAN fiber in the pre-oxidation process were studied by FTIR spectroscopy, XRD, and SEM. Mechanical property changes were also investigated. No changes in the movement and intensity of functional groups of PAN fibers were caused by positive stretching of up to 10% and negative stretching down to -8%. The crystal structure can be affected by the positive stretching and negative stretching. The maximum strength is 479.81 MPa when the stretching is positive, and the maximum strength is 420.55 MPa when the stretching is negative.
Keywords
polyacrylonitrile; positive stretching; negative stretching; pre-oxidation;
Citations & Related Records
연도 인용수 순위
  • Reference
1 Cato AD, Edie DD. Flow behavior of mesophase pitch. Carbon, 41, 1411 (2003). doi: 10.1016/s0008-6223(03)00050-2.   DOI
2 Rahaman MSA, Ismail AF, Mustafa A. A review of heat treatment on polyacrylonitrile fiber. Polym Degradation Stab, 92, 1421 (2007). doi: 10.1016/j.polymdegradstab.2007.03.023.   DOI   ScienceOn
3 Wang PH. Aspects on prestretching of PAN precursor: Shrinkage and thermal behavior. J Appl Polym Sci, 67, 1185 (1998). doi: 10.1002/(sici)1097-4628(19980214)67:7<1185::aid-app3>3.0.co;2-c.   DOI
4 Yu M, Wang C, Bai Y, Wang Y, Zhu B. Evolution of tension during the thermal stabilization of polyacrylonitrile fibers under different parameters. J Appl Polym Sci, 102, 5500 (2006). doi: 10.1002/app.23960.   DOI   ScienceOn
5 Wu G, Lu C, Ling L, Hao A, He F. Influence of tension on the oxidative stabilization process of polyacrylonitrile fibers. J Appl Polym Sci, 96, 1029 (2005). doi: 10.1002/app.21388.   DOI   ScienceOn
6 Dalton S, Heatley F, Budd PM. Thermal stabilization of polyacrylonitrile fibres. Polymer, 40, 5531 (1999). doi: 10.1016/s0032-3861(98)00778-2.   DOI
7 Wangxi Z, Jie L, Gang W. Evolution of structure and properties of PAN precursors during their conversion to carbon fibers. Carbon, 41, 2805 (2003). doi: 10.1016/s0008-6223(03)00391-9.   DOI
8 Yu M, Wang C, Bai Y, Zhu B, Ji M, Xu Y. Microstructural evolution in polyacrylonitrile fibers during oxidative stabilization. J Polym Sci, Part B: Polym Phys, 46, 759 (2008). doi: 10.1002/polb.21410.   DOI   ScienceOn
9 Hou Y, Sun T, Wang H, Wu D. Thermal-shrinkage investigation of the chemical reaction during the stabilization of polyacrylonitrile fibers. J Appl Polym Sci, 114, 3668 (2009). doi: 10.1002/app.30303.   DOI   ScienceOn
10 Bhat GS, Cook FL, Abhiraman AS, Peebles Jr LH. New aspects in the stabilization of acrylic fibers for carbon fibers. Carbon, 28, 377 (1990). doi: 10.1016/0008-6223(90)90011-m.   DOI
11 Ozbek S, Isaac DH. Strain-induced density changes in PAN-based carbon fibres. Carbon, 38, 2007 (2000). doi: 10.1016/s0008-6223(00)00060-9.   DOI