Evaluation of Fatigue Strength in Ductile Cast Iron by Maximum and Mean Size of Graphite  

Yoon, Myung-Jin (경일대학교 기계자동차학부)
Publication Information
Journal of the Korean Society of Manufacturing Process Engineers / v.11, no.1, 2012 , pp. 82-87 More about this Journal
Abstract
For different ferrite-pearlite matrix structure, contain more than 90% spheroidal ratio of graphite, GCD 45-3, GCD 50, GCD 60 series and 70%, 80%, 90% spheroidal ratio of graphite, GCD 40, GCD 45-1, GCD 45-2 series, this paper has carried out rotary bending fatigue test, estimated maximum and mean size of spheroidal graphite, investigated correlation. It was concluded as follows. (1) Fatigue limit in $10^7$cycles and numbers of spheroidal graphite per 1$mm^2$ was linear relation. (2) projection area of graphite can be used to predict fatigue limit of Ductile Cast Iron. The Statistical distribution of extreme values of projection area of defects may be used as a guideline for the control of inclusion size in the steelmaking processes.
Keywords
Maximum and Mean Size of Graphite; Ductile Cast Iron; Ferrite-Pearlite Matrix Structure; Fatigue Strength; Spheroidal Ratio of Graphite; Projection Area of Graphite;
Citations & Related Records
연도 인용수 순위
  • Reference
1 M. J. Yoon, K. M. Lee, "Effect of a Matrix Structure on the Initiation of Fatigue Crack and Fatigue Strength in Nodular Cast Iron", J. of the Korean Society of Machine Tool Engineers, Vol. 7, No. 5, pp. 66 - 71, 1998.
2 Smith R. A., "Short Fatigue Cracks, Fatigue mechanisms: Advances in Quantitative Measurement of Physical Damage", ASTM STP 811, J. Lankford, D. L. Davidson, W. L. Morris, and R. P. Wei, Eds., American Society for Testing and Materials, pp. 264-279, 1983.
3 T. Tanaka, H. Nakayama, A. Sakaida, T. Imamichi, "Evaluation of Weibull Parameters For Static Strengths of Ceramics Monte Carlo Simulation", MSRI. Vol. 1, No. 1, pp. 51-58, 1995.
4 Y. Murakami and S. Nemat-Nasser, "Growth and Stability of Interacting Surface Flaws of Arbitrary Shape", EFM. Vol. 17, No. 3-A, pp. 193-210, 1983.
5 Y. Murakami., Endo M., "Effects of Hardness and Crack Geometries on ${\Delta}Kth$ of Small Cracks Emanating from Small Defects", The Behaviour of Short Fatigue Cracks, EGF Pub. 1(Edited by K. J. Miller and E. R. de los Rios), pp. 275-293, 1986.
6 Kendall, J. M., James, M. N., and Knott, J. F., "The Behaviour of Physically Short Fatigue Cracks in Steels, The Behaviour of Short Fatigue Cracks", EGF Pub. 1 (Edited by K. J. Miller and E. R. de los Rios), pp. 241-258, 1986.
7 Hideo Kitagawa, Yuji Nakasone, and Satoru Miyashita, "Measurement of Fatigue Damage by Randomly Distributed Small Cracks Data", ASTM STP 811, pp. 233-263, 1983.
8 Nisitani, H. and Goto, M., "A Small-Crack Growth Law and its Application to the Evaluation of Fatigue Life, The Behaviour of Short Fatigue Cracks", EGF Pub. 1 (Edited by K. J. Miller and E. R. de los Rios), pp. 461-478, 1986.
9 M. Endo, Y. Murakami, "Effects of an Artificial Small Defect on Torsional Fatigue Strength of Steels", ASME. Vol. 109, pp. 124-129, 1987.   DOI
10 Y. Murakami, M. Endo, "Effects of Defects, inclusions and inhomogeneities on Fatigue Strength, Fatigue", Vol. 16, pp. 163-182, 1994.   DOI
11 Y. Murakami, "Effects of Small Defects and Nonmetallic Inclusions on The Fatigue Strength of Metals", JSME. Vol. 32, Mo. 2, pp. 167-180, 1989.
12 Y. Murakami, "Inclusion Rating by Statistics of Extreme Values and Its Application to Fatigue Strength Prediction and Quality Control of Materials", J. Res. Natl. Inst. Stand. Technol. Vol. 99, pp. 345-351, 1994.   DOI
13 M. J. Yoon, "Evaluation of Statistical Distribution of extreme values of Graphite in Ductile Cast Iron by Image Analyzer", The Korean Society of Manufacturing Process Engineers, Vol. 7, No. 6, pp. 66-71, 2010.