Abstract
In this study, a super carburizing treatment was applied to improve roller pitting fatigue life. It produced excellent properties of surface hardness and temper softening resistance by forming precipitation of fine and spherodized carbides on a tempered marstensite matrix through the repeated process of carburization and diffusion after high temperature carburizing step 1. The cycle II performed two times carburizing/diffusion cycle (process) after super carburization at $1,000^{\circ}C$ had fine and spherodized carbides to subsurface $200{\mu}m$. In this case, the carbide was $(Fe,Cr)_3C$ and there was not any massive carbides. In the case of Cycle II, the roller pitting fatigue life had a 6.15 million cycles. It was improved 48% compared to normal gas carburizing treatment.
Keywords
super carburizing; fine and spherodized carbides; roller pitting fatigue life; temper softening;
Citations & Related Records
연도 인용수 순위
  • Reference
1 A. Chiba, T. Saito, and K. Yamaguchi, J. Japan Inst. Metals 47, 321(1983).   DOI
2 R. F. Kern, Heat Treatment 10, 36 (1986).
3 T. Shimomura, T. Morita, K. Inoue, and T. Hanyuda, Denki-Seiko 77, 11 (2006).   DOI   ScienceOn
4 L. D. Liu and F. S. Chen, Surface and Coatings Technology 183, 233 (2004).   DOI   ScienceOn
5 T. Shimomura and S. Nakamura, Denki-Seiko 65, 295 (1994).   DOI
6 T. Shimomura and K. Namiki, Denki-Seiko 63, 4 (1992).   DOI
7 S. Abe and M. Ikeda, R&D Kobe Steel Engineering Reports 54, 21 (2004).
8 T. Hanyuda and S. Nakamura, Denki-Seiko 71, 59 (2000).   DOI   ScienceOn
9 M. Kato and T. Kano, Denki-Seiko 77, 67 (2008).
10 D. Y. Kim and J. H. Jeong, Seah Besteel Research Report 23, 49 (2007).
11 K. S. Nam and K. J. Lee, J. Korea Soc. Heat Treatment 14, 124 (2001).
12 M. Y. Wey, T. Sakuma, and T. Nishizawa, Transactions of the Japan Institute of Metals 22, 733 (1981).   DOI
13 S. Matsumoto, Mitsubishi Heavy Industries Technical Report 11, 644(1974).
14 T. Kimura, H. Tanaka, and S. Nakamura, Denki-Seiko 69, 7 (1998).   DOI   ScienceOn