Abstract
Recently European Council(EU) published the RoHS(restriction of the use of certain hazardous substances in electrical and electronic equipment) which is prohibit the use of Pb, Hg, Cd, $Cr^{+6}$, PBB or PBDE in the electrical and electronic equipments. So EU member States shall ensure that, from 1 July 2006, new electrical and electronic equipment put on the market does not contain 6 hazardous substances. The one of the most important in electronics manufacturing process is soldering. Soldering process use the chemical substances which are applied in fluxing and cleaning processes and it can generate the malfunction of electronics caused by corrosion in the fields conditions. Therefore this study researched on the polarization and Tafel properties of Sn40Pb and Sn3.0Ag0.5Cu(SAC) solder based on the electrochemical theory. We prepared SnPb specimens which was aged in $150^{\circ}C,\;180^{\circ}C$ for 15 minutes ana Sn3.0Ag0.5Cu specimens that was aged in $180^{\circ}C,\;220^{\circ}C$ for 10 minutes. Experimental polarization curves were measured in distilled ionized water and $3.5 wt\%$, 1 mole NaCl electrolyte of $40^{\circ}C$, pH 7.5. Ag/AgCl and graphite were utilized by reference and counter electrode, respectively. To observe the electrochemical reaction, polarization test was conducted from -250 mV to +250 mV. From the polarization curves that were composed of anodic and cathodic curves, we obtained Tafel slop, reversible electrode potential(Ecorr) and exchange current density(Icorr). In these results, corrosion rate for two specimen were compared Sn3.0Ag0.5Cu with SnPb solders
Keywords
Pb-free soldering; SnAgCu; intermetallic compounds; corrosion rate; RoHS;
Citations & Related Records
Times Cited By KSCI : 1  (Citation Analysis)
연도 인용수 순위
1 Directive 2002/95/EC of the European Parliament and of the Council, Restriction of the Use of Certain Hazardous Substances in Electrical and Electronic Equipment, EU (2003)
2 D. A. Jones, Principles and Prevention of Corrosion, p.74, Macmillan Pub. Company, New York (1992)
3 M. G. Fontama, Corrosion Eng., 3rd Ed., McGraw-Hill Int. Ed., New York (1988)
4 K. Suganuma, S. H. Huh, K. Kim, N. and Y. Nakamura, Mater. Trans, JIM, 42, 286 (2001)   DOI   ScienceOn
5 Leda free soldering project final report, JEITA, Tokyo (2000)
6 JEITA, Lead Free Soldering Tech., Corona Pub. Co. Ltd., Tokyo (2003)
7 C. Wagner, W. Traund, Z. Electrochem., 44, 391 (1938)
8 K. S. Kim, S. H. Huh, K. Suganuma, Int. Conf. on Electronics Packaging, JIEP, p.89 (2002)
9 W. Moon, J. of Electron. Mater., 29(10), 1122 (2000)   DOI
10 J. W. Jang, P. G. Kim, K. N. Tu, D. R. Frear, P. Thompson, J. of Appl. Phys., 85, 8456 (1999)   DOI
11 R. Strauss, SMT Soldering Handbook, 2nd Ed., p.148, Newnes, Oxford (1998)
12 W. S. Hong, B. C. Kang, B. S. Song, K. B. Kim, Kor. J. of Mater. Res., 15(1), 54 (2005)   DOI   ScienceOn
13 K. Suganuma, Lead free soldering in electronics, p.57, Marcel Dekker Inc. New York (2004)