Effect of Surface Preparation and Curing Condition on the Interfacial Bond Strength between Ultra High Performance Concrete and Normal Strength Concrete  

Kang, Sung-Hoon (서울대학교 건축학과)
Hong, Sung-Gul (서울대학교 건축학과)
Publication Information
Journal of the Korea institute for structural maintenance and inspection / v.19, no.3, 2015 , pp. 149-160 More about this Journal
Abstract
This study reports the interfacial bond strength between Ultra High Performance Concrete (UHPC) and Normal Strength Concrete (NSC). While previous studies have focused on the interfacial strength between NSC substrate and UHPC overlay, this study use precast UHPC for enhanced constructability and replacement of formwork. The factors affecting the interface strength are comprehensively reviewed. It can be classified into: interface shape, degree of hardening and moisture condition of UHPC before combining with NSC, and curing condition of composite materials. Conducted experiments verify the effects of each factor on the interface strength and, accordingly show different failure modes. In particular, a new failure mode of the failure of a part of UHPC was firstly found in the case of sample with rough interface between UHPC and NSC. The other factors of the degree of hardening and the moisture and curing conditions of UHPC were discussed. This research will provide a valuable foundation to utilize the UHPC as a composite material.
Keywords
Ultra high performance concrete (UHPC); Bond strength; Permanent formwork; Composite structure; Interface;
Citations & Related Records
Times Cited By KSCI : 2  (Citation Analysis)
연도 인용수 순위
1 Abu-Tair, A. I., Rigden, S. R., and Burley, E. (1996), Testing the Bond between Repair Materials and Concrete Substrate, ACI Material Journal, 93(6), 553-558.
2 Austin, S. A., and Robins, P. J., (1993), Development of a Patch Test to Study the Behaviour of Shallow Concrete Patch Repairs, Magazine of Concrete Research, 45(164), 221-229.   DOI   ScienceOn
3 Austin, S., Robins, P., and Pan, Y. (1995), Tensile Bond Testing of Concrete Repairs, Material and Structures, RILEM, 28(5), 249-259.   DOI
4 Austin, S., Robins, P., and Pan, Y. (1999), Shear Bond Testing of Concrete Repairs, Cement and Concrete Research, Elsevier, 29(7), 1067-1079.   DOI   ScienceOn
5 Beushausen, H. D. (2005), Long-Term Performance of Bonded Overlays Subjected to Differential Shrinkage, Ph.D. Thesis, University of Cape Town, South Africa, 27-49.
6 Bissonnette, B., Vaysburd, A. M., and von Fay, K. F. (2012), Best Practices for Preparing Concrete Surfaces Prior to Repairs and Overlays, Transportation Research Board of the National Academies, TRB, Washington, D.C., 1-17.
7 Carbonell, M. A., Harris, D. K., Shann, S. V., and Ahlborn, T. M. (2012), Bond Strength between UHPC and Normal Strength Concrete (NSC) in accordance with Split Prism and Freeze-Thaw Cycling Tests, Proceedings of Hipermat 2012, 3rd International Symposium on UHPC and Nanotechnology for High Performance Construction Materials, Kassel, 377-384.
8 Cho, C. G., Han, B. C., Lee J. H., and Kim, Y. Y. (2010), Flexural Test on Composite Deck Slab Produced with Extruded ECC Panel, Journal of the Korea Concrete Institute, KCI, 22(5), 695-702 (in Korean, with English abstract).   DOI   ScienceOn
9 Espeche, A. D., and Leon, J. (2011), Estimation of Bond Strength Envelopes for Old-to-New Concrete Interfaces Based on a Cylinder Splitting Test, Construction and Building Materials, Elsevier, 25(3), 1222-1235.   DOI   ScienceOn
10 Fehling, E., Schmidt, M., Walraven, J., Leutbecher, T., and Frohlech, S. (2013), Ultra-High Performance Concrete UHPC: Fundamental, Design, Examples, Ernst & Sohn, Kassel, 17-18.
11 Gai, X., Darby, A., Ibell, T., and Evernden, M. (2012), Experimental Investigation into a Ductile FRP Stay-In-Place Formwork System for Concrete Slab, Construction and Building Materials, Elsevier, 49, 1013-1023.
12 Gillette, R. W. (1964), A 10-Year Report on Performance of Bonded Concrete Resurfacing, Highway Research Record (94), Highway Research Board, 61-76.
13 Kang, S. H., and Hong, S. G. (2014), Performance of Fresh and Hardened Ultra High Performance Concrete without Heat Treatment, Journal of the Korea Concrete Institute, KCI, 26(1), 23-34 (in Korean, with English abstract).   DOI   ScienceOn
14 Harris, D. K., Sarkar, J., and Ahlborn, T. M. (2011), Characterization of Interface Bond of Ultra-High-Performance Concrete Bridge Deck Overlays, Journal of the Transportation Research Board, TRB, 40-49.
15 Hong, S. G., and Kang, S. H. (2013), Formwork Development using UHPFRC, Proceedings of the RILEM-fib-AFGC International Sympsium on Ultra-High Performance Fibre-Reinforced Concrete, RILEM, Marseille, 197-206.
16 Kamen, A. (2006), Time Dependent Behaviour of Ultra-High Performance Fibre Reinforced Concrete (UHPFRC), 6th International Ph.D. Symposium in Civil Engineering, Zurich, 1-8.
17 Kang, S. T., Park, J. J., Ryu, G. S., and Kim, S. W. (2010), The Effect of Steel-Fiber Reinforcement on the Compressive Strength of Ultra High Performance Cementitious Composites (UHPCC), Journal of The Korea Institute for Structural Maintenance and Inspection, JKSMI, 14(5), 110-118 (in Korean, with English abstract).
18 Kim, G. B., Pilakoutas, K., and Waldron, P. (2008), Development of Thin FRP Reinforced GFRC Permanent Formwork Systems, Construction and Building Materials, Elsevier, 22(11), 2250-2259.   DOI   ScienceOn
19 Kono, K., Musha, H., Kawaguchi, T., Eriguchi, A., Tanaka, S., Kobayashi, T., and Ikeda, A. (2013), Durability Study of the First PC Bridge Constructed with Ultra High Strength Fiber Reinforced Concrete in Japan, Proceedings of the RILEM-fib-AFGC International Sympsium on Ultra-High Performance Fibre-Reinforced Concrete, RILEM, Marseille, 239-248.
20 Korean Agency for Technology and Standards (2006), Method of Test for Splitting Tensile Strength of Concrete, KS F 2423, Seoul, 1-16.
21 Kuder, K. G., Gupta, R., Harris-Jones, C., Hawksworth, R., Henderson, S., and Whitney, J. (2009), Effect of PVC Stay-In-Place Formwork on Mechanical Performance of Concrete, Journal of Materials in Civil Engineering, ASCE, 21(7), 309-315.   DOI   ScienceOn
22 Korean Agency for Technology and Standards (2007), Method of Test for Slump of Concrete, KS F 2402, Seoul, 1-10.
23 Korean Agency for Technology and Standards (2009), Method of Test for Slump Flow of Fresh Concrete, KS F 2594, Seoul, 1-8.
24 Korean Agency for Technology and Standards (2010), Standard Test Method for Compressive Strength of Concrete, KS F 2405, Seoul, 1-10.
25 Leung, C. K. Y., and Cao, Q. (2010), Development of Pseudo-Ductile Permanent Formwork for Durable Concrete Structures, Material and Structures, RILEM, 43(7), 993-1007.   DOI
26 Li, G., Xie, H., and Xiong, G. (2001), Transition Zone Studies of New-to-Old Concrete with Different Binders, Cement Concrete Composites, Elsevier, 23(4-5), 381-387.   DOI   ScienceOn
27 Mehta, P. K., and Monteiro, P. J. M. (2006), Concrete: Microstructure, Properties, and Materials 3rd edition, McGraw-Hill, New York, 21-84.
28 Mirmoghtadaei, R., Mohammadi, M., Samani, N. A., and Mousavi, S. (2015), The Impact of Surface Preparation on the bond Strength of Repaired Concrete by Metakaolin Containing Concrete, Construction and Building Materials, Elsevier, 80, 76-83.   DOI   ScienceOn
29 Momayez, A., Ehsani, M. R,, Ramezanianpour, A. A., and Rajaie, H. (2005), Comparison of Method for Evaluating Bond Strength between Concrete Substrate and Repair Materials, Cement and Concrete Research, Elsevier, 35(4), 748-757.   DOI   ScienceOn
30 Nelson, M., and Fam, A. (2014), Full Bridge Testing at Scale Constructed with Novel FRP Stay-In-Plave Structural Forms for Concrete Deck, Construction and Building Materials, Elsevier, 50, 368-376.   DOI   ScienceOn
31 Omar, B., Fattoum, K., Maissen, B., and Farid, B. (2010), Influence of the Roughness and Moisture of the Substrate Surface on the Bond between Old and New Concrete, Contemporary Engineering Sciences, 3(3), 139-147.
32 Pigeon, M., and Saucier, F. (1992), Durability of Repaired Concrete Structures, Proceedings of International Symposium on Advances in Concrete Technology, Athens, 741-773.
33 Richard, P., and Cheyrezy, M. (1995), Composition of Reactive Powder Concretes, Cement and Concrete Research, 25(7), 1501-1511.   DOI   ScienceOn
34 Santos, P. M. D., and Julio, E. N. B S. (2011), Factors Affecting Bond between New and Old Concrete, ACI Materials Journal, ACI, 108(4), 449-456.
35 Shin, H. C., and Wan, Z. (2010), Interfacial Shear Bond Strength between Old and New Concrete, Fracture Mechanics of Concrete and Concrete Structures - Assessment, Durability, Monitoring and Retrofitting of Concrete Structures, KCI, Seoul, 1195-1200.
36 Tawab, A. A., Fahmy, E. H., and Shaheen, Y. B. (2012), Use of Permanent Ferrocement Forms for Concrete Beam Construction, Material and Structures, RILEM, 45(9), 1319-1329.   DOI   ScienceOn
37 Tayeh, B. A., Abu Bakar, B. H., and Megat Johari, M. A., (2013), Characterization of the Interfacial Bond between Old Concrete Substrate and Ultra High Performance Fiber Concrete Repair Composite, Material and Structures, RILEM, 46(5), 743-753.   DOI
38 Wan, Z. (2011), Interfacial Shear Bond Strength between Old and New Concrete, M. S. Thesis, Louisiana State University, 1-21.
39 Tayeha, B. A., Abu Bakara, B. H., Megat Johari, M. A., and Voo, Y. L. (2012), Mechanical and Permeability Properties of the Interface Between Normal Concrete Substrate and Ultra High Performance Fiber Concrete Overlay, Construction and Building Materials, Elsevier, 36, 538-548.   DOI   ScienceOn
40 Thanoon, W. A., Yardim, Y., Jaafar, M. S., and Noorzaei, J. (2010), Structural Behavior of Ferrocement-Brick Composite Floor Slab Panel, Construction and Building Materials, Elsevier, 24(11), 2224-2230.   DOI   ScienceOn
41 Wirojjanapirom, P., Matsumoto, L., Kono, K., and Niwa, J. (2013), Experimental Investigation of Shear Behavior of RC Beam using UFC U-Shaped Permanent Formwork, Proceedings of the RILEM-fib-AFGC International Sympsium on Ultra-High Performance Fibre-Reinforced Concrete, RILEM, Marseille, 187-196.