Ageing characteristics of RTV coating materials by corona discharge have been studied. The hydrophobicity recovery of RTV coating materials with 300${\mu}{\textrm}{m}$ thickness was identical with a bulk silicone materials. The RTV coating materials hydrophobicity has been almost lost when its were discharged during 40 seconds by corona discharge of 10㎸, and recovered after about 45 hours. The resistivity of RTV coating materials has not been recovered after 45 hours, though after 80 hours the initiation resistivity value has been recovered up to 95%. There was no critical change of compounds(such as Si and Al) on RTV surfaces by the corona discharge treatment until 100 seconds. In the test of arc erosion, it was seen that the coating sample with silicone rubber as a base material have more longer burn-out time than other samples with FRP or glass base.
Keywords
RTV silicone coating; corona discharge ageing; hydrophobic; arc erosion; tracking test;
Citations & Related Records
연도 인용수 순위
  • Reference
1 R. Hartings, 'The AC behavior of a hydrophilic and hydrophobic post insulator during rain', IEEE Trans, on Power Delivery, p1584-, 1994   DOI   ScienceOn
2 R. S. Gorur, T. Orbeck, 'Surface dielectric behavior of polymeric insulation under HV outdoor conditions', IEEE Trans. on Electrical Insulation, Vol 26, No. 5, pl064-, 1991   DOI   ScienceOn
3 ASTM D 257, 'Standard test methods for DC resistance or conductance of insulation materials', 1983
4 ASTM D 495, 'Standard test methods for high voltage, low current, dry arc resistance of solid electrical insulation', 1984
5 IEC 60587, 'Test methods for evaluating resistance to tracking and erosion of electrical insulating materials used under severe ambient conditions', 1984
6 H. Hillborg and U. W. Gedde, 'Hydrophobicity recovery of Polydimethylsiloxane after exposure to corona discharges', Polymer, Vol. 39, No. 10, pp. 1991-1998, 1998   DOI   ScienceOn
7 P. J. Smith, M. J. Owen, P. H. Holm and G. A. Toskey, 'Silicone studies of corona treated silicone rubber HV insulation', 1992 IEEE Conf. on Electrical Insulation and Dielectric Phenomena, Victoria, Canada, pp. 829-836, 1992
8 한동희, '실리콘 고무 복합재료의 전기 절연 특성', 박사 학위논문. 2001