A bag filter system was partially burnt down during a trial run of waste wood incineration boiler. This brought about unburned hydrocarbon which caused a rapid deactivation of low temperature SCR catalyst set up in two stage after the bag filter. The deactivated catalyst was investigated in order to trace the origin by several characterization methods such as XRD, EDX, BET, TGA, SEM. The deactivated catalyst was regenerated by different methods such as acid washing, water washing in ultrasonication, and calcination treatment under air condition. It is found the calcination treatment under air condition at $450^{\circ}C$ for 2 hours to be the best regeneration method. The catalytic activity was measured in the form of 2 cm ${\times}$ 2 cm ${\times}$ 10 cm (catalyst weight 10 g) honeycomb type. A deNOx efficiency of the regenerated catalyst showed 100% at $180^{\circ}C$ which is the same level of fresh one.
Keywords
NOx; SCR Catalyst; Deactivation; Regeneration; Carbon Deposition;
Citations & Related Records
Times Cited By KSCI : 2  (Citation Analysis)
연도 인용수 순위
1 Pasel, J., Kassner, P., Montanari, B., Gazzano, M., Vaccari, A., Makowski, W. Lojewski, T., Dziembaj, R. and Papp, H., "Transition metal oxides supported on active carbons as low temperature catalysts for the selective catalytic reduction (SCR) of NO with $NH_3$," Appl. Catal. B, 18(3-4), 199-213(1998).   DOI   ScienceOn
2 Pearson, I. M., Ryu, H., Wong, W. C. and Nobe, K., "Chemical Mixed' catalysts," Ind. Eng. Chem. Prod. Res. Dev., 22(2), 381-382(1983).   DOI
3 Baiker, A., Dollenmeier, P. and Glinski, M., "Selective Catalytic Reduction of Nitric Oxide with Ammonia. I. Monolayer and Multilayer of Vanadia Supported on Titania," Appl. Catal., 35(2), 351-364(1987).   DOI   ScienceOn
4 Bond, G. C., Zurita, J. P., Flamerz, S., Gellings, P. J., Bosch, H., van Ommen, J. G. and Kip, B. J., "Structure and Reactivity of Titania Supported Oxides; Part 1. Vanadium Oxides on Titania in the sub- and super-Monolayer Regions," Appl. Catal., 22, 361-378(1986).   DOI   ScienceOn
5 Forzatti, P., "Present status and perspectives in de-NOx SCR catalysis," Appl. Catal. A, 222(1-2), 221-236(2001).   DOI   ScienceOn
6 최병선 외 21인, "화력발전소의 환경종합대책수립 연구, 최종보고서," 한국전력공사 기술연구원(1989).
7 Hughes, R., Deactivation of Catalysts, Academic Press(1984).
8 Forzatti, P. and Lietti, L., "Catalyst deactivation," Catal. Today, 52(2-3), 165-181(1999).   DOI   ScienceOn
9 Khodayari, R. and Odenbrand, C.U.I., "Regeneration of commercial SCR catalysts by washing and sulphation: effect of sulphate groups on the activity," Appl. Catal. B, 33, 277-291(2001).   DOI   ScienceOn
10 Zheng, Y., Jensen, A. D. and Johnsson, J. E., "Deactivation of $V_2O_5-WO_3-TiO_2$ SCR catalyst at a biomass-fired combined heat and power plant," Appl. Catal. B, 60, 253-264 (2005).   DOI   ScienceOn
11 문일식, 조규진, "배연 탈질용 폐촉매의 재생에 관한 연구," 공업화학, 10(2), 263-267(1999).
12 이상진, 홍성창, "소각로 SCR 폐탈질 촉매의 피독과 효율 재생에 관한 연구," 공업화학, 19(3), 259-263(2008).
13 US Patent 6,387,836, 14 May 2002, SaarEnergie GmbH, Saarbruken, Germany.
14 Nojima, S., Iida, K., Nobayashi, N. and Naito, O., "Development of NOx removal SCR catalyst for low $SO_2$ oxidation," Mitsubishi Heavy Industries, Ltd. Technical review, 38(2), 89-91(2001).
15 Kiyoura, R. and Urano, K., "Mechanism, Kinetics, and Equilibrium of Thermal Decomposition of Ammonium Sulfate," Ind. Eng. Chem. Prod. Res. Dev., 9(4), 489-494(1970).   DOI
16 김진영, 김봉수, 가명진, 이진구, 이주헌, "폐 SCR 촉매의 재생 특성," 한국대기환경학회 2005 춘계학술대회 논문집, PD1(2005).
17 Khodayari, R. and Odenbrand, C. U. I., "Regeneration of commercial $TiO_2-V_2O_5-WO_3$ SCR catalysts used in bio fuel plants," Appl. Catal. B, 30, 87-99(2001).   DOI   ScienceOn
18 박혜경, "질소산화물 제거용 상용 $V_2O_5-WO_3/TiO_2$ SCR 폐 촉매의 재생 효과 고찰", 대한환경공학회지, 27(8), 859-869 (2005).