Browse > Article
http://dx.doi.org/10.9714/psac.2012.14.2.008

Determination of winding diameter based on bending strain analysis for REBCO coated conductor tapes  

Leon, M.B. De (Department of Mechanical Engineering, Andong National University)
Dedicatoria, M.J. (Department of Mechanical Engineering, Andong National University)
Shin, H.S. (Department of Mechanical Engineering, Andong National University)
Publication Information
Progress in Superconductivity and Cryogenics / v.14, no.2, 2012 , pp. 8-11 More about this Journal
Abstract
In order to recognize the allowable bending diameter in coils, the strain as function of diameters is evaluated. The irreversible strain limits of $I_c$ in the easy and hard bending modes were measured. Strains were calculated at the coating film in the easy bending and at outer edge or inner edge in the hard bending of the CC tape, respectively. The tape geometry subjected to bending procedures is considered from the current industrial spool winding operation. Through the linear superposition of strain induced in different bending modes regarding the expressions, the appropriate design for critical bending diameter is suggested. Results proved that the existence of buckling resulting from bending in hard direction when applied strain exceeded 0.6% is possible. The depicted results showed that the strain limit as a viable parameter should be considered for future purposes.
Keywords
Citations & Related Records
Times Cited By KSCI : 2  (Citation Analysis)
연도 인용수 순위
1 A. Mbaruku, "Electromechanical and fatigue properties of as-manufactured and quench damaged YBCO coated conductor," PhD Thesis, Florida State Univ., 2006.
2 W. D. Markiewicz, C. A. Swenson, "Winding strain analysis for YBCO coated conductors." Supercond. Sci. Technol, vol. 23, 045017, March 2010.   DOI   ScienceOn
3 A. V. Zlobin et al., "Modeling the high-field section of a Muon helical cooling channel," Proceedings of IPAC'10, Kyoto, Japan, pp. 391-393, 2010.
4 H. C. Jo et al., "Characteristic comparison of various winding methods of HTS magnets", IEEE Trans. Appl. Supercond., 2012, submitted for publication.
5 H. S. Shin, K. Katagiri, "Critical current degradation behavior in Bi-2223 superconducting tapes under bending and torsion strains". Supercond. Sci. Technol., vol. 16, pp. 1012-1018, 2003.   DOI   ScienceOn
6 H. S. Shin, M. J. Dedicatoria, N. J. Lee, S. S. Oh, "Effect of bending test procedure on the degradation behavior of critical current in ReBCO coated conductor tapes," KIASC Journal, vol. 11, no. 4, pp. 12-15, 2009   과학기술학회마을
7 H. S. Shin, J. R. C. Dizon, R. Bonifacio, J. S. Park, "Influence of bending strain on $I_c$ degradation behavior in YBCO coated conductor tapes processed using RABiTs /MOD," KIASC Journal, vol. 9, n0. 2, pp. 11-14, 2007.   과학기술학회마을
8 H. S. Shin, M. J. Dedicatoria, J. R. C. Dizon, H. S. Ha, S. S. Oh, "Bending strain characteristics of critical current in REBCO CC tapes in different modes," Physica C, vol. 469, pp. 1467-1471, 2009.   DOI   ScienceOn
9 D. C. van der Laan, J. W. Ekin, C. C. Clickner and T. C. Stauffer, "Delamination strength of YBCO coated conductors under transverse tensile stress," Supercond. Sci. Technol., vol. 20, pp. 765-770, 2007.   DOI   ScienceOn