THE EFFECT OF PRIMING ETCHED DENTIN WITH SOLVENT ON THE MICROTENSILE BOND STRENGTH OF HYDROPHOBIC DENTIN ADHESIVE  

Park, Eun-Sook (Department of Conservative Dentistry, School of Dentistry, Seoul National University)
Bae, Ji-Hyun (Department of Conservative Dentistry, Seoul National University Bundang Hospital)
Kim, Jong-Soon (Department of Conservative Dentistry, School of Dentistry, Seoul National University)
Kim, Jae-Hoon (Department of Conservative Dentistry, School of Dentistry, Seoul National University)
Lee, In-Bog (Department of Conservative Dentistry, School of Dentistry, Seoul National University)
Kim, Chang-Keun (Department of Chemical Engineering, Choongang University)
Son, Ho-Hyun (Department of Conservative Dentistry, School of Dentistry, Seoul National University)
Cho, Byeong-Hoon (Department of Conservative Dentistry, School of Dentistry, Seoul National University)
Publication Information
Restorative Dentistry and Endodontics / v.34, no.1, 2009 , pp. 42-50 More about this Journal
Abstract
Deterioration of long-term dentin adhesion durability is thought to occur by hydrolytic degradation within hydrophilic domains of the adhesive and hybrid layers. This study investigated the hypothesis that priming the collagen network with an organic solvent displace water without collapse and thereby obtain good bond strength with an adhesive made of hydrophobic monomers and organic solvents. Three experimental adhesives were prepared by dissolving two hydrophobic monomers, bisphenol-A-glycidylmethacrylate (Bis-GMA) and triethyleneglycol dimethacrylate (TEGDMA), into acetone, ethanol or methanol. After an etching and rinsing procedure, the adhesives were applied onto either wet dentin surfaces (wet bonding) or dentin surfaces primed with the same solvent (solvent-primed bonding). Microtensile bond strength (MTBS) was measured at 48 hrs, 1 month and after 10,000 times of thermocycles. The bonded interfaces were evaluated using a scanning electron microscope (SEM). Regardless of bonding protocols, well-developed hybrid layers were observed at the bonded interface in most specimens. The highest mean MTBS was observed in the adhesive containing ethanol at 48 hrs. With solvent-primed bonding, increased MTBS tendencies were seen with thermo cycling in the adhesives containing ethanol or methanol. However, in the case of wet bonding, no increase in MTBS was observed with aging.
Keywords
Dentin adhesive; Durability; Solvent priming; Hydrophobic monomer; Microtensile bond strength;
Citations & Related Records
Times Cited By KSCI : 3  (Citation Analysis)
연도 인용수 순위
1 Eliades G, Vougiouklakis G, Palaghias G. Heterogeneous distribution of single-bottle adhesive monomers in the resin-dentin interdiffusion zone. Dent Mater 17:277-283, 2001   DOI   ScienceOn
2 Spencer P, Wang Y, Lawrence K. Identification of collagen encapsulation at the dentin/adhesive interface. J Adhes Dent 6:91-95, 2004   PUBMED
3 Tay FR, Frankenberger R, Krejci I, Bouillaguet S, Pashley DH, Carvalho RM, Lai CNS. Single-bottle adhesives behave as permeable membranes after polymerization. I. In vivo evidence. J Dent 32:611-621, 2004   DOI   ScienceOn
4 Armstrong SR, Vargas MA, Qian F, Laffoon JE. Microtensile bond strength of a total-etch 3-step, total-etch 2-step, self-etch 2-step, and a self-etch 1-step dentin bonding system through 15-month water storage. J Adhes Dent 5:47-56, 2003   PUBMED
5 Tay FR, Hashimoto M, Pashley DH, Peters MC, Lai SCN, Yiu CKY, Cheong C. Aging affects two modes of nanoleakage expression in bonded dentin. J Dent Res 82:537-541, 2003   DOI   ScienceOn
6 Hashimoto M, Ohno H, Sano H, Kaga M, Oguchi H. In vitro degradation of resin-dentin bonds analyzed by microtensile bond test, scanning and transmission electron microscopy. Biomaterials 24:3795-3803, 2003   DOI   ScienceOn
7 Son SJ, Chang JG, Kang SH, Yoo HM, Cho BH, Son HH. The nanoleakage patterns of experimental hydrophobic adhesive after load cycling. J Kor Acad Cons Dent 33(1):9-19, 2008   DOI
8 Maciel KT, Carvalho RM, Ringle RD, Preson CD, Russell CM, Pashley DH. The effects of acetone, ethanol, HEMA, and air on the stiffness of human decalcified dentin matrix. J Dent Res 75:1851-1858, 1996   DOI   ScienceOn
9 Mohan B, Kandaswamy D. A confocal microscopic evaluation of resin-dentin interface using adhesive systems with three different solvents bonded to dry and moist dentin-An in vitro study. Quintessence Int 36:511-521, 2005
10 Miguez PA, Pereira MP, Swift EJ Jr. One-year tensile bond strengths of two self-etching primers to bovine enamel. J Esthet Restor Dent 16:243-248, 2004   DOI   ScienceOn
11 Armstrong SR, Vargas MA, Chung I, Pashley DH, Campbell JA, Laffoon JE, Qian F. Resin-dentin interfacial ultrastructure and microtensile dentin bond strength after five-year water storage. Oper Dent 29:705-712, 2004   PUBMED
12 Tarumi H, Imazato S, Ehara A, Kato S, Ebi N, Ebisu S. Post-irradiation polymerization of composites containing bis-GMA and TEGDMA. Dent Mater 15:238-242, 1999   DOI   ScienceOn
13 Frankenberger R, Strobel WO, Lohbauer U, Kramer N, Petschelt A. The effect of six years of water storage on resin composite bonding to human dentin. J Biomed Mater Res B Appl Biomater 69(1):25-32, 2004   DOI
14 Nakabayashi N, Watanabe A, Gendusa NJ. Dentin adhesion of 'modified'4-META/MMA-TBB resin: function of HEMA. Dent Mater 8:259-264, 1992   DOI   ScienceOn
15 Takahashi A, Inoue S, Kawamoto C, Ominato R, Tanaka T, Sato Y, Pereira PN, Sano H. In vivo longterm durability of the bond to dentin using two adhesive systems. J Adhes Dent 4:151-159, 2002   PUBMED
16 Nakabayashi N, Kojima K, Masuhara E. The promotion of adhesion by the infiltration of monomers into tooth substrates. J Biomed Mater Res 16:265-273, 1982   DOI   ScienceOn
17 Wang Y, Spencer P. Evaluation of the interface between one-bottle adhesive systems and dentin by Goldner's trichrome. Am J Dent 18:66-72, 2005   PUBMED
18 De Munck J, Van Meerbeek B, Yoshida Y, Inoue S, Vargas M, Suzuki K, Lambrechts P, Vanherle G. Fouryear water degradation of total-etch adhesives bonded to dentin. J Dent 82:136-140, 2003   DOI
19 Perdigao J, Frankenberger R. Effect of solvent and rewetting time on dentin adhesion. Qunitessence Int 32:385-390, 2001   PUBMED
20 Carvalho RM, Yoshiyama M, Brewer PD, Pashley DH. Dimensional changes of demineralized human dentine during preparation for scanning electron microscopy. Arch Oral Biol 41:379-386, 1996   DOI   ScienceOn
21 Fukuda K, Nezu T, Terada Y. The effects of alcoholic compounds on the stability of type I collagen studied by differential scanning calorimetry. Dent Mater J 19:221-228, 2000   DOI   PUBMED   ScienceOn
22 Spencer P, Wang Y. Adhesive phase separation at the dentin interface under wet bonding conditions. J Biomed Mater Res 62:447-456, 2002   DOI   ScienceOn
23 Cho BH, Dickens SH. Effects of the acetone content of single solution dentin bonding agents on the adhesive layer thickness and the microtensile bond strength. Dent Mater 20:107-115, 2004   DOI   ScienceOn
24 Kim YS, Park SH, Choi GW, Choi KK. Effect of intermediate resin hydrophilicity on bond strength of single step adhesive. J Kor Acad Cons Dent 32(5):445-458, 2007   DOI
25 Osorio R, Erhardt MC, Pimenta LA, Osorio E, Toledano M. EDTA treatment improves resin-dentin bonds' resistance to degradation. J Dent Res 5;84:736-740, 2005   DOI   ScienceOn
26 Tay FR, Pashley DH, Suh BI, Carvalho RM, Itthagarun A. Single-step adhesives are permeable membranes. J Dent 30:371-382, 2002   DOI   ScienceOn
27 Park JS, Kim JS, Kim MS, Son HH, Kwon HC, Cho BH. Aging effect on the microtensile bond strength of self-etching adhesives. J Kor Acad Cons Dent 31(6):415-426, 2006   DOI
28 Nakajima M, Okuda M, Ogata M, Pereira PN, Tagami J, Pashley DH. The durability of a fluoride-releasing resin adhesive system to dentin. Oper Dent 28:186-192, 2003
29 Nakajima M, Okuda M, Ogata M, Pereira PN, Tagami J, Pashley DH. The durability of a fluoride-releasing resin adhesive system to dentin. Oper Dent 28:186-192, 2003   PUBMED
30 Rosenblatt J, Devereux B, Wallace DG. Injectable collagen as a pH-sensitive hydrogel. Biomaterials 15:985-995, 1994   DOI   ScienceOn
31 Fukushima T, Inoue Y, Miyazaki K, Itoh T. Effect of primers containing N-methylolacrylamide or N-methylolmethacrylamide on dentin bond durability of a resin composite after 5 years. J Dent 29:227-234, 2001   DOI   ScienceOn
32 Asmussen E. Peutzfeldt A. Short- and Long-term bonding efficacy of a self-etching, one-step adhesive. J Adhes Dent 5:41-45, 2003   PUBMED
33 Rosales-Leal JI, Osorio R, Holgado-Terriza JA, Cabrerizo-Vilchez MA, Toledano M. Dentin wetting by four adhesive systems. Dent Mater 17:526-532, 2001   DOI   ScienceOn