Evaluation of marginal discrepancy of pressable ceramic veneer fabricated using CAD/CAM system: Additive and subtractive manufacturing  

Kang, Seen-Young (Department of Dental Laboratory Science and Engineering, College of Health Science, Korea University)
Lee, Ha-Na (Department of Dental Laboratory Science and Engineering, College of Health Science, Korea University)
Kim, Ji-Hwan (Department of Dental Laboratory Science and Engineering, College of Health Science, Korea University)
Kim, Woong-Chul (Department of Dental Laboratory Science and Engineering, College of Health Science, Korea University)
Publication Information
The Journal of Advanced Prosthodontics / v.10, no.5, 2018 , pp. 347-353 More about this Journal
Abstract
PURPOSE. The purpose of this study was to evaluate the marginal discrepancy of heat-pressed ceramic veneers manufactured using a CAD/CAM system. MATERIALS AND METHODS. The ceramic veneers for the abutment of a maxillary left central incisor were designed using a CAD/CAM software program. Ten veneers using a microstereolithography apparatus (AM group), ten veneers using a five-axis milling machine (SM group), and ten veneers using a traditional free-hand wax technique (TW group) were prepared according to the respective manufacturing method. The ceramic veneers were also fabricated using a heat-press technique, and a silicone replica was used to measure their marginal discrepancy. The marginal discrepancies were measured using a digital microscope (${\times}160$ magnification). The data were analyzed using a nonparametric Kruskal-Wallis H test. Finally, post-hoc comparisons were conducted using Bonferroni-corrected Mann-Whitney U tests (${\alpha}=.05$). RESULTS. The $mean{\pm}SD$ of the total marginal discrepancy was $99.68{\pm}28.01{\mu}m$ for the AM group, $76.60{\pm}28.76{\mu}m$ for the SM group, and $83.08{\pm}39.74{\mu}m$ for the TW group. There were significant differences in the total marginal discrepancies of the ceramic veneers (P<.05). CONCLUSION. The SM group showed a better fit than the AM and TW groups. However, all values were within the clinical tolerance. Therefore, CAD/CAM manufacturing methods can replace the traditional free-hand wax technique.
Keywords
Additive manufacturing; Subtractive manufacturing; Computer-aided design and computer-aided machining (CAD/CAM); Ceramic veneer; Heat pressing;
Citations & Related Records
연도 인용수 순위
  • Reference
1 Marchionatti AME, Wandscher VF, May MM, Bottino MA, May LG. Color stability of ceramic laminate veneers cemented with light-polymerizing and dual-polymerizing luting agent: A split-mouth randomized clinical trial. J Prosthet Dent 2017;118:604-10.
2 Peumans M, De Munck J, Fieuws S, Lambrechts P, Vanherle G, Van Meerbeek B. A prospective ten-year clinical trial of porcelain veneers. J Adhes Dent 2004;6:65-76.
3 Aboushelib MN, Elmahy WA, Ghazy MH. Internal adaptation, marginal accuracy and microleakage of a pressable versus a machinable ceramic laminate veneers. J Dent 2012;40: 670-7.   DOI
4 Shamseddine L, Mortada R, Rifai K, Chidiac JJ. Fit of pressed crowns fabricated from two CAD-CAM wax pattern process plans: A comparative in vitro study. J Prosthet Dent 2017;118: 49-54.   DOI
5 Ural C, Burgaz Y, Saraç D. In vitro evaluation of marginal adaptation in five ceramic restoration fabricating techniques. Quintessence Int 2010;41:585-90.
6 Homsy FR, Özcan M, Khoury M, Majzoub ZAK. Marginal and internal fit of pressed lithium disilicate inlays fabricated with milling, 3D printing, and conventional technologies. J Prosthet Dent 2018;119:783-90.   DOI
7 van Noort R. The future of dental devices is digital. Dent Mater 2012;28:3-12.   DOI
8 Stampfl J, Baudis S, Heller C, Liska R, Neumeister A, Kling R, Ostendorf A, Spitzbart M. Photopolymers with tunable mechanical properties processed by laser-based high-resolu- tion stereolithography. J Micromech Microeng 2008;18: 125014.   DOI
9 Hamza TA, Ezzat HA, El-Hossary MM, Katamish HA, Shokry TE, Rosenstiel SF. Accuracy of ceramic restorations made with two CAD/CAM systems. J Prosthet Dent 2013; 109:83-7.   DOI
10 Neves FD, Prado CJ, Prudente MS, Carneiro TA, Zancopé K, Davi LR, Mendonça G, Cooper LF, Soares CJ. Micro-computed tomography evaluation of marginal fit of lithium disilicate crowns fabricated by using chairside CAD/CAM systems or the heat-pressing technique. J Prosthet Dent 2014;112:1134-40.   DOI
11 Sulaiman F, Chai J, Jameson LM, Wozniak WT. A comparison of the marginal fit of In-Ceram, IPS Empress, and Procera crowns. Int J Prosthodont 1997;10:478-84.
12 Lin TM, Liu PR, Ramp LC, Essig ME, Givan DA, Pan YH. Fracture resistance and marginal discrepancy of porcelain laminate veneers influenced by preparation design and restorative material in vitro. J Dent 2012;40:202-9.   DOI
13 Park JY, Bae SY, Lee JJ, Kim JH, Kim HY, Kim WC. Evaluation of the marginal and internal gaps of three different dental prostheses: comparison of the silicone replica technique and three-dimensional superimposition analysis. J Adv Prosthodont 2017;9:159-69.   DOI
14 Kim DY, Jeon JH, Kim JH, Kim HY, Kim WC. Reproducibility of different arrangement of resin copings by dental microste- reolithography: Evaluating the marginal discrepancy of resin copings. J Prosthet Dent 2017;117:260-5.   DOI
15 Sakornwimon N, Leevailoj C. Clinical marginal fit of zirconia crowns and patients' preferences for impression techniques using intraoral digital scanner versus polyvinyl siloxane material. J Prosthet Dent 2017;118:386-91.   DOI
16 Association AD. ANSI/ADA Specification No. 8 for zinc phosphate cement. Guide to dental materials and devices. 5th ed Chicago; ADA; 1970-1.
17 McLean JW, von Fraunhofer JA. The estimation of cement film thickness by an in vivo technique. Br Dent J 1971;131: 107-11.   DOI
18 Al-Imam H, Gram M, Benetti AR, Gotfredsen K. Accuracy of stereolithography additive casts used in a digital workflow. J Prosthet Dent 2018;119:580-5.   DOI
19 Vojdani M, Torabi K, Farjood E, Khaledi A. Comparison the Marginal and Internal Fit of Metal Copings Cast from Wax Patterns Fabricated by CAD/CAM and Conventional Wax up Techniques. J Dent (Shiraz) 2013;14:118-29.
20 Abduo J, Lyons K, Bennamoun M. Trends in computer-aided manufacturing in prosthodontics: a review of the available streams. Int J Dent 2014;2014:783948.