Browse > Article
http://dx.doi.org/10.4047/jap.2013.5.4.382

The effect of alumina and aluminium nitride coating by reactive magnetron sputtering on the resin bond strength to zirconia core  

Kulunk, Tolga (Ondokuz Mayis University, Faculty of Dentistry, Department of Prosthodontics)
Kulunk, Safak (Ondokuz Mayis University, Faculty of Dentistry, Department of Prosthodontics)
Baba, Seniha (Ondokuz Mayis University, Faculty of Dentistry, Department of Prosthodontics)
Ozturk, Ozgur (Ondokuz Mayis University, Faculty of Dentistry, Department of Prosthodontics)
Danisman, Sengul (Erciyes University, Faculty of Engineering, Department of Mechanical Engineering)
Savas, Soner (Erciyes University, Faculty of Engineering, Department of Mechanical Engineering)
Publication Information
The Journal of Advanced Prosthodontics / v.5, no.4, 2013 , pp. 382-387 More about this Journal
Abstract
PURPOSE. Although several surface treatments have been recently investigated both under in vitro and in vivo conditions, controversy still exists regarding the selection of the most appropriate zirconia surface pre-treatment. The purpose of this study was to evaluate the effect of alumina (Al) and aluminium nitride (AlN) coating on the shear bond strength of adhesive resin cement to zirconia core. MATERIALS AND METHODS. Fifty zirconia core discs were divided into 5 groups; air particle abrasion with 50 ${\mu}m$ aluminum oxide particles ($Al_2O_3$), polishing + Al coating, polishing + AlN coating, air particle abrasion with 50 ${\mu}m$ $Al_2O_3$ + Al coating and air particle abrasion with 50 ${\mu}m$ $Al_2O_3$ + AlN coating. Composite resin discs were cemented to each of specimens. Shear bond strength (MPa) was measured using a universal testing machine. The effects of the surface preparations on each specimen were examined with scanning electron microscope (SEM). Data were statistically analyzed by one-way ANOVA (${\alpha}$=.05). RESULTS. The highest bond strengths were obtained by air abrasion with 50 ${\mu}m$ $Al_2O_3$, the lowest bond strengths were obtained in polishing + Al coating group (P<.05). CONCLUSION. Al and AlN coatings using the reactive magnetron sputtering technique were found to be ineffective to increase the bond strength of adhesive resin cement to zirconia core.
Keywords
Air abrasion; Magnetron sputtering; Coating; Zirconia;
Citations & Related Records
연도 인용수 순위
  • Reference
1 Kern M. Resin bonding to oxide ceramics for dental restorations. J Adhes Sci Techno 2009;23:1097-111.   DOI   ScienceOn
2 Ozcan M, Kerkdijk S, Valandro LF. Comparison of resin cement adhesion to Y-TZP ceramic following manufacturers' instructions of the cements only. Clin Oral Investig 2008;12: 279-82.   DOI   ScienceOn
3 Kitayama S, Nikaido T, Maruoka R, Zhu L, Ikeda M, Watanabe A, Foxton RM, Miura H, Tagami J. Effect of an internal coating technique on tensile bond strengths of resin cements to zirconia ceramics. Dent Mater J 2009;28:446-53.   DOI
4 Casucci A, Mazzitelli C, Monticelli F, Toledano M, Osorio R, Osorio E, Papacchini F, Ferrari M. Morphological analysis of three zirconium oxide ceramics: Effect of surface treatments. Dent Mater 2010;26:751-60.   DOI   ScienceOn
5 Ozcan M, Nijhuis H, Valandro LF. Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging. Dent Mater J 2008;27:99-104.   DOI   ScienceOn
6 Piascik JR, Swift EJ, Thompson JY, Grego S, Stoner BR. Surface modification for enhanced silanation of zirconia ceramics. Dent Mater 2009;25:1116-21.   DOI   ScienceOn
7 Blatz MB, Sadan A, Kern M. Resin-ceramic bonding: a review of the literature. J Prosthet Dent 2003;89:268-74.   DOI   ScienceOn
8 Atsu SS, Kilicarslan MA, Kucukesmen HC, Aka PS. Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin. J Prosthet Dent 2006;95:430-6.   DOI   ScienceOn
9 Matinlinna JP, Lassila LV, Vallittu PK. Pilot evaluation of resin composite cement adhesion to zirconia using a novel silane system. Acta Odontol Scand 2007;65:44-51.   DOI   ScienceOn
10 Tsukakoshi M, Shinya A, Gomi H, Lassila LV, Vallittu PK, Shinya A. Effects of dental adhesive cement and surface treatment on bond strength and leakage of zirconium oxide ceramics. Dent Mater J 2008;27:159-71.   DOI   ScienceOn
11 Tsuo Y, Yoshida K, Atsuta M. Effects of alumina-blasting and adhesive primers on bonding between resin luting agent and zirconia ceramics. Dent Mater J 2006;25:669-74.   DOI   ScienceOn
12 Nagayassu MP, Shintome LK, Uemura ES, Araújo JE. Effect of surface treatment on the shear bond strength of a resinbased cement to porcelain. Braz Dent J 2006;17:290-5.   DOI   ScienceOn
13 Kern M, Thompson VP. Bonding to glass infiltrated alumina ceramic: adhesive methods and their durability. J Prosthet Dent 1995;73:240-9.   DOI   ScienceOn
14 Ozcan M, Vallittu PK. Effect of surface conditioning methods on the bond strength of luting cement to ceramics. Dent Mater 2003;19:725-31.   DOI   ScienceOn
15 Derand T, Molin M, Kvam K. Bond strength of composite luting cement to zirconia ceramic surfaces. Dent Mater 2005; 21:1158-62.   DOI   ScienceOn
16 Aboushelib MN, Feilzer AJ, Kleverlaan CJ. Bonding to zirconia using a new surface treatment. J Prosthodont 2010;19: 340-6.   DOI   ScienceOn
17 Nothdurft FP, Motter PJ, Pospiech PR. Effect of surface treatment on the initial bond strength of different luting cements to zirconium oxide ceramic. Clin Oral Investig 2009; 13:229-35.   DOI
18 Della Bona A, Anusavice KJ, Hood JA. Effect of ceramic surface treatment on tensile bond strength to a resin cement. Int J Prosthodont 2002;15:248-53.
19 de Oyagüe RC, Monticelli F, Toledano M, Osorio E, Ferrari M, Osorio R. Influence of surface treatments and resin cement selection on bonding to densely-sintered zirconium-oxide ceramic. Dent Mater 2009;25:172-9.   DOI   ScienceOn
20 Amaral R, Ozcan M, Bottino MA, Valandro LF. Microtensile bond strength of a resin cement to glass infiltrated zirconiareinforced ceramic: the effect of surface conditioning. Dent Mater 2006;22:283-90.   DOI   ScienceOn
21 Wolfart M, Lehmann F, Wolfart S, Kern M. Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods. Dent Mater 2007;23:45-50.   DOI   ScienceOn
22 Blatz MB, Chiche G, Holst S, Sadan A. Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia. Quintessence Int 2007;38:745-53.
23 Zhang S, Kocjan A, Lehmann F, Kosmac T, Kern M. Influence of contamination on resin bond strength to nanostructured alumina-coated zirconia ceramic. Eur J Oral Sci 2010;118:396-403.   DOI   ScienceOn
24 Guazzato M, Quach L, Albakry M, Swain MV. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic. J Dent 2005;33:9-18.   DOI   ScienceOn
25 Amaral R, Ozcan M, Valandro LF, Balducci I, Bottino MA. Effect of conditioning methods on the microtensile bond strength of phosphate monomer-based cement on zirconia ceramic in dry and aged conditions. J Biomed Mater Res B Appl Biomater 2008;85:1-9.
26 Oblak C, Jevnikar P, Kosmac T, Funduk N, Marion L. Fracture resistance and reliability of new zirconia posts. J Prosthet Dent 2004;91:342-8.   DOI   ScienceOn
27 Guazzato M, Proos K, Quach L, Swain MV. Strength, reliability and mode of fracture of bilayered porcelain/zirconia (Y-TZP) dental ceramics. Biomaterials 2004;25:5045-52.   DOI   ScienceOn
28 Zhang Y, Lawn BR, Malament KA, Van Thompson P, Rekow ED. Damage accumulation and fatigue life of particle-abraded ceramics. Int J Prosthodont 2006;19:442-8.
29 Ruddell DE, Thompson JY, Stoner BR. Mechanical properties of a dental ceramic coated by RF magnetron sputtering. J Biomed Mater Res 2000;51:316-20.   DOI   ScienceOn
30 Tanaka K, Kimoto K, Sawada T, Toyoda M. Shear bond strength of veneering composite resin to titanium nitride coating alloy deposited by radiofrequency sputtering. J Dent 2006;34:277-82.   DOI   ScienceOn
31 Liu GT, Duh JG, Chung KH, Wang JH. Mechanical characteristics and corrosion behavior of (Ti,Al)N coatings on dental alloys. Surf Coat Technol 2005;200:2100-5.   DOI   ScienceOn
32 Tek Z, Gügör MA, Çal E, Sonugelen M, Artunç C, Oztarhan A. A study of the mechanical properties of TiN coating of Cr-Ni alloy. Surf Coat Technol 2005;196:317-20.   DOI   ScienceOn
33 Teixeira EC, Piascik JR, Stoner BR, Thompson JY. Dynamic fatigue behavior of dental porcelain modified by surface deposition of a YSZ thin film. J Prosthodont 2008;17:527-31.   DOI   ScienceOn
34 Jevnikar P, Krnel K, Kocjan A, Funduk N, Kosmac T. The effect of nano-structured alumina coating on resin-bond strength to zirconia ceramics. Dent Mater 2010;26:688-96.   DOI   ScienceOn
35 Teixeira EC, Piascik JR, Stoner BR, Thompson JY. Effect of YSZ thin film coating thickness on the strength of a ceramic substrate. J Biomed Mater Res B Appl Biomater 2007;83:459-63.
36 Ferraris M, Verné E, Appendino P, Moisescu C, Krajewski A, Ravaglioli A, Piancastelli A. Coatings on zirconia for medical applications. Biomaterials 2000;21:765-73.   DOI   ScienceOn
37 McCrory PV, Tinston S, Piddock V, Kelly P, Combe EC, Arnell RD. Tin oxide coating of aluminous porcelain by reactive ion plating. J Dent 1991;19:171-5.   DOI   ScienceOn
38 McCrory PV, Piddock V, Combe EC, Tinston S, Arnell RD, Weglicki P, Owen J. Evaluation of a potential dental application of vapour deposition techniques for coating alumina with tin oxide. J Mater Sci 1994;5:543-50.
39 Beuer F, Aggstaller H, Edelhoff D, Gernet W, Sorensen J. Marginal and internal fits of fixed dental prostheses zirconia retainers. Dent Mater 2009;25:94-102.   DOI   ScienceOn
40 Kassner H, Siegert R, Hathiramani D, Vassen R, Stoever D. Application of suspension plasma spraying (SPS) for manufacture of ceramic coatings. J Therm Spray Technol 2008;17: 115-23.   DOI
41 Reichelt K, Jiang X. The preparation of thin films by physical vapour deposition methods. Thin Solid Films 1990;191: 91-126.   DOI   ScienceOn