Literature review on the experimental method and interpretation of the edge chipping test (ECT)  

Song, Min-Gyu (Department of Prosthodontics, College of Dentistry, Gangneung-Wonju National University)
Ko, Kyung-Ho (Department of Prosthodontics, College of Dentistry, Gangneung-Wonju National University)
Huh, Yoon-Hyuk (Department of Prosthodontics, College of Dentistry, Gangneung-Wonju National University)
Park, Chan-Jin (Department of Prosthodontics, College of Dentistry, Gangneung-Wonju National University)
Cho, Lee-Ra (Department of Prosthodontics, College of Dentistry, Gangneung-Wonju National University)
Publication Information
The Journal of Korean Academy of Prosthodontics / v.60, no.1, 2022 , pp. 9-18 More about this Journal
Abstract
In vitro studies are essential to predict the clinical performance of ceramic widely used as restorative materials. Traditional experiments such as fracture toughness and flexural strength have been used to evaluate the properties of brittle ceramics. However, these experiments have a limitation that the load conditions, failure patterns, and load values at which failure occurs are not similar to human occlusal force ranges or clinical failures. On the other hand, the edge chipping test (ECT), which was recently introduced to study chipping fracture of ceramics, has similar failure patterns to clinical trials. In addition, the failure loads from ECT were similar to human occlusal force. ECT can be usefully used in the study of ceramic properties. In this literature review, a more clinically meaningful experimental study of ceramics by examining the meaning and limitations of traditional ceramic failure tests and comparing them with ECT.
Keywords
Ceramic; Chipping fracture; Edge chipping test; Flexural strength; Fracture toughness;
Citations & Related Records
Times Cited By KSCI : 4  (Citation Analysis)
연도 인용수 순위
1 Cesar PF, Della Bona A, Scherrer SS, Tholey M, van Noort R, Vichi A, Kelly R, Lohbauer U. ADM guidance-Ceramics: Fracture toughness testing and method selection. Dent Mater 2017;33:575-84.   DOI
2 Baroudi K, Silikas N, Watts DC. Edge-strength of flowable resin-composites. J Dent 2008;36:63-8.   DOI
3 Ereifej N, Silikas N, Watts DC. Edge strength of indirect restorative materials. J Dent 2009;37:799-806.   DOI
4 Quinn GD, Giuseppetti AA, Hoffman KH. Chipping fracture resistance of dental CAD/CAM restorative materials: part 2. Phenomenological model and the effect of indenter type. Dent Mater 2014;30:e112-23.
5 Brandeburski SBN, Vidal ML, Collares K, Zhang Y, Della Bona A. Edge chipping test in dentistry: A comprehensive review. Dent Mater 2020;36:e74-84.   DOI
6 Comleko lu ME, Tekero lu F, Dundar Comleko lu M, Ozcan M, Turkun L , Paken G. Clinical wear and quality assessment of monolithic and lithium disilicate layered zirconia restorations. Aust Dent J 2021 Jul 28. doi: 10.1111/adj.12869.   DOI
7 Jo EH, Huh YH, Ko KH, Park CJ, Cho LR. Effect of different ceramic materials and substructure designs on fracture resistance in anterior restorations. J Prosthet Dent 2020 Dec 31:S0022-3913(20)30724-1.
8 Felberg RV, Bassani R, Pereira GKR, Bacchi A, Silva-Sousa YTC, Gomes EA, Sarkis-Onofre R, Spazzin AO. Restorative possibilities using zirconia ceramics for single crowns. Braz Dent J 2019;30:446-52.   DOI
9 Kern T, Tinschert J, Schley JS, Wolfart S. Five-year clinical evaluation of all-ceramic posterior FDPs made of In-Ceram Zirconia. Int J Prosthodont 2012;25:622-4.
10 Zurcher AN, Hjerppe J, Studer S, Lehner C, Sailer I, Jung RE. Clinical outcomes of tooth-supported leucite-reinforced glass-ceramic crowns after a follow-up time of 13-15 years. J Dent 2021;111:103721.   DOI
11 Limones A, Molinero-Mourelle P, Azevedo L, Romeo-Rubio M, Correia A, Gomez-Polo M. Zirconia-ceramic versus metal-ceramic posterior multiunit tooth-supported fixed dental prostheses: A systematic review and meta-analysis of randomized controlled trials. J Am Dent Assoc 2020;151:230-8.   DOI
12 Pjetursson BE, Valente NA, Strasding M, Zwahlen M, Liu S, Sailer I. A systematic review of the survival and complication rates of zirconia-ceramic and metal-ceramic single crowns. Clin Oral Implants Res 2018;29:199-214.
13 Stawarczyk B, Liebermann A, Rosentritt M, Povel H, Eichberger M, Lumkemann N. Flexural strength and fracture toughness of two different lithium disilicate ceramics. Dent Mater J 2020;39:302-8.   DOI
14 ISO 6872. Dentistry - ceramic materials. International Standards Organization (ISO); Geneva; Switzerland, 2015.
15 Kim SH, Choi YS, Kang KH, Att W. Effects of thermal and mechanical cycling on the mechanical strength and surface properties of dental CAD-CAM restorative materials. J Prosthet Dent 2021 Feb 2:S0022-3913(20)30727-7.
16 Catramby MF, do Vale AL, Dos Santos HES, Elias CN. Effect of sintering process on microstructure, 4-point flexural strength, and grain size of yttria-stabilized tetragonal zirconia polycrystal for use in monolithic dental restorations. J Prosthet Dent 2021;125:1-8.   DOI
17 Anusavice KJ. Standardizing failure, success, and survival decisions in clinical studies of ceramic and metal-ceramic fixed dental prostheses. Dent Mater 2012;28:102-11.   DOI
18 Kelly JR. Clinically relevant approach to failure testing of all-ceramic restorations. J Prosthet Dent 1999;81:652-61.   DOI
19 Wierichs RJ, Kramer EJ, Reiss B, Schwendicke F, Krois J, Meyer-Lueckel H, Wolf TG. A prospective, multi-center, practice-based cohort study on all-ceramic crowns. Dent Mater 2021;37:1273-82.   DOI
20 Anusavice KJ, Kakar K, Ferree N. Which mechanical and physical testing methods are relevant for predicting the clinical performance of ceramic-based dental prostheses? Clin Oral Implants Res 2007;18:218-31.   DOI
21 Reale Reyes A, Dennison JB, Powers JM, Sierraalta M, Yaman P. Translucency and flexural strength of translucent zirconia ceramics. J Prosthet Dent 2021 Jul 22:S0022-3913(21)00336-X.
22 Quinn JB. Material properties of ceramics for dental applications. College Park: University of Maryland; 2000.
23 Cha MS, Huh YH, Cho LR, Park CJ. A comparative study of the wear of dental alloys against monolithic zirconia. J Prosthet Dent 2020;123:866-73.   DOI
24 Varga S, Spalj S, Lapter Varga M, Anic Milosevic S, Mestrovic S, Slaj M. Maximum voluntary molar bite force in subjects with normal occlusion. Eur J Orthod 2011;33:427-33.   DOI
25 Kim SH, Watts DC. In vitro study of edge-strength of provisional polymer-based crown and fixed partial denture materials. Dent Mater 2007;23:1570-3.   DOI
26 Watts DC, Issa M, Ibrahim A, Wakiaga J, Al-Samadani K, Al-Azraqi M, Silikas N. Edge strength of resin-composite margins. Dent Mater 2008;24:129-33.   DOI
27 Quinn GD, Giuseppetti AA, Hoffman KH. Chipping fracture resistance of denture tooth materials. Dent Mater 2014;30:545-53.   DOI
28 Pfeilschifter M, Preis V, Behr M, Rosentritt M. Edge strength of CAD/CAM materials. J Dent 2018;74:95-100.   DOI
29 Quinn GD. On edge chipping testing and some personal perspectives on the state of the art of mechanical testing. Dent Mater 2015;31:26-36.   DOI
30 Chai H, Lee JJ, Lawn BR. On the chipping and splitting of teeth. J Mech Behav Biomed Mater 2011;4:315-21.   DOI
31 Zhang Y, Chai H, Lee JJ, Lawn BR. Chipping resistance of graded zirconia ceramics for dental crowns. J Dent Res 2012;91:311-5.   DOI
32 Taufer C, Della Bona A. Edge chipping resistance of ceramics bonded to a dentine analogue. J Mech Behav Biomed Mater 2019;90:587-90.   DOI
33 Kim JH, Ko KH, Huh YH, Park CJ, Cho LR. Effects of the thickness ratio of zirconia-lithium disilicate bilayered ceramics on the translucency and flexural strength. J Prosthodont 2020;29:334-40.   DOI
34 Quinn GD, Giuseppetti AA, Hoffman KH. Chipping fracture resistance of dental CAD/CAM restorative materials: part I-procedures and results. Dent Mater 2014;30:e99-111.