The effet of cooling rate on the residual stresses in the veneer ceramics of zirconia-ceramic restorations: a literature review  

Chang, Jea-Seung (Department of Dentistry, Yong-In Severance Hospital, College of Dentistry, Yonsei University)
Kim, Sunjai (Department of Prosthodontics, Gangnam Severance Dental Hospital, College of Dentistry, Yonsei University)
Publication Information
The Journal of Korean Academy of Prosthodontics / v.52, no.2, 2014 , pp. 136-142 More about this Journal
Abstract
Nowadays, dental zirconia is widely used as a framework material for a fixed dental prosthesis as well as a single restoration. However, clinical studies have reported high incidence of veneer chipping of zirconia-ceramic restorations compared to that of metal-ceramics. Several factors were raised as the possible causes of veneer ceramic chipping, however, it is still in debate. Recently, residual stresses in the veneer ceramics after cooling process gathers attention as one possible cause of chipping and many studies reported that the rate of cooling significantly influenced the types and the amount of residual stress. The purpose of current review was to briefly describe the effect of cooling rate on the residual stress in zirconia-ceramics. It was also described that the different behavior of residual stress between zirconia-ceramics and metal-ceramics following different cooling rate.
Keywords
Zirconia, Veneer ceramic; Chipping; Residual stress; Cooling rate;
Citations & Related Records
연도 인용수 순위
  • Reference
1 Sax C, Hammerle CH, Sailer I. 10-year clinical outcomes of fixed dental prostheses with zirconia frameworks. Int J Comput Dent 2011;14:183-202.
2 Burke FJ, Crisp RJ, Cowan AJ, Lamb J, Thompson O, Tulloch N. Five-year clinical evaluation of zirconia-based bridges in patients in UK general dental practices. J Dent 2013;41:992-9.   DOI   ScienceOn
3 Aboushelib MN, Feilzer AJ, Kleverlaan CJ. Bridging the gap between clinical failure and laboratory fracture strength tests using a fractographic approach. Dent Mater 2009;25:383-91.   DOI   ScienceOn
4 Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Effect of zirconia type on its bond strength with different veneer ceramics. J Prosthodont 2008;17:401-8.   DOI   ScienceOn
5 Guess PC, Schultheis S, Bonfante EA, Coelho PG, Ferencz JL, Silva NR. All-ceramic systems: laboratory and clinical performance. Dent Clin North Am 2011;55:333-52.   DOI   ScienceOn
6 Christensen RP, Ploeger BJ. A clinical comparison of zirconia, metal and alumina fixed-prosthesis frameworks veneered with layered or pressed ceramic: a three-year report. J Am Dent Assoc 2010;141:1317-29.   DOI   ScienceOn
7 Kelly JR, Benetti P. Ceramic materials in dentistry: historical evolution and current practice. Aust Dent J 2011;56:84-96.   DOI   ScienceOn
8 Molin MK, Karlsson SL. Five-year clinical prospective evaluation of zirconia-based Denzir 3-unit FPDs. Int J Prosthodont 2008;21:223-7.
9 Tholey MJ, Swain MV, Thiel N. Thermal gradients and residual stresses in veneered Y-TZP frameworks. Dent Mater 2011;27: 1102-10.   DOI   ScienceOn
10 Meira JB, Reis BR, Tanaka CB, Ballester RY, Cesar PF, Versluis A, Swain MV. Residual stresses in Y-TZP crowns due to changes in the thermal contraction coefficient of veneers. Dent Mater 2013;29:594-601.   DOI   ScienceOn
11 Belli R, Monteiro S Jr, Baratieri LN, Katte H, Petschelt A, Lohbauer U. A photoelastic assessment of residual stresses in zirconia-veneer crowns. J Dent Res 2012;91:316-20.   DOI   ScienceOn
12 Bonfante EA, Rafferty BT, Silva NR, Hanan JC, Rekow ED, Thompson VP, Coelho PG. Residual thermal stress simulation in three-dimensional molar crown systems: a finite element analysis. J Prosthodont 2012;21:529-34.   DOI   ScienceOn
13 DeHoff PH, Anusavice KJ. Viscoelastic stress analysis of thermally compatible and incompatible metal-ceramic systems. Dent Mater 1998;14:237-45.   DOI   ScienceOn
14 Marshall DB, Lawn BR. An indentation technique for measuring stresses in tempered glass surfaces. J Am Ceram Soc 1977; 60:86-7.   DOI
15 Anusavice KJ, Hojjatie B. Effect of thermal tempering on strength and crack propagation behavior of feldspathic porcelains. J Dent Res 1991;70:1009-13.   DOI   ScienceOn
16 Coffey JP, Anusavice KJ, DeHoff PH, Lee RB, Hojjatie B. Influence of contraction mismatch and cooling rate on flexural failure of PFM systems. J Dent Res 1988;67:61-5.   DOI   ScienceOn
17 Pjetursson BE, Sailer I, Zwahlen M, Ha¨mmerle CH. A systematic review of the survival and complication rates of all-ceramic and metal-ceramic reconstructions after an observation period of at least 3 years. Part I: Single crowns. Clin Oral Implants Res 2007; 18:73-85.   DOI   ScienceOn
18 Guess PC, Kulis A, Witkowski S, Wolkewitz M, Zhang Y, Strub JR. Shear bond strengths between different zirconia cores and veneering ceramics and their susceptibility to thermocycling. Dent Mater 2008;24:1556-67.   DOI   ScienceOn
19 Go¨stemeyer G, Jendras M, Dittmer MP, Bach FW, Stiesch M, Kohorst P. Influence of cooling rate on zirconia/veneer interfacial adhesion. Acta Biomater 2010;6:4532-8.   DOI   ScienceOn
20 Guess PC, Bonfante EA, Silva NR, Coelho PG, Thompson VP. Effect of core design and veneering technique on damage and reliability of Y-TZP-supported crowns. Dent Mater 2013;29:307-16.   DOI   ScienceOn
21 Rues S, Kro¨ger E, Mu¨ller D, Schmitter M. Effect of firing protocols on cohesive failure of all-ceramic crowns. J Dent 2010;38:987-94.   DOI   ScienceOn
22 Silva NR, Bonfante EA, Rafferty BT, Zavanelli RA, Rekow ED, Thompson VP, Coelho PG. Modified Y-TZP core design improves all-ceramic crown reliability. J Dent Res 2011;90:104-8.   DOI   ScienceOn
23 Guazzato M, Walton TR, Franklin W, Davis G, Bohl C, Klineberg I. Influence of thickness and cooling rate on development of spontaneous cracks in porcelain/zirconia structures. Aust Dent J 2010;55:306-10.   DOI   ScienceOn
24 Mainjot AK, Schajer GS, Vanheusden AJ, Sadoun MJ. Influence of cooling rate on residual stress profile in veneering ceramic: measurement by hole-drilling. Dent Mater 2011;27:906-14.   DOI   ScienceOn
25 Anusavice KJ, DeHoff PH, Hojjatie B, Gray A. Influence of tempering and contraction mismatch on crack development in ceramic surfaces. J Dent Res 1989;68:1182-7.   DOI   ScienceOn
26 Swain MV. Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures. Acta Biomater 2009;5:1668-77.   DOI   ScienceOn
27 Sorrentino R, De Simone G, Tete S, Russo S, Zarone F. Five-year prospective clinical study of posterior three-unit zirconia-based fixed dental prostheses. Clin Oral Investig 2012;16:977-85.   DOI   ScienceOn
28 Sailer I, Gottnerb J, Kanelb S, Hammerle CH. Randomized controlled clinical trial of zirconia-ceramic and metal-ceramic posterior fixed dental prostheses: a 3-year follow-up. Int J Prosthodont 2009;22:553-60.
29 Sailer I, Pjetursson BE, Zwahlen M, Hammerle CH. A systematic review of the survival and complication rates of all-ceramic and metal-ceramic reconstructions after an observation period of at least 3 years. Part II: Fixed dental prostheses. Clin Oral Implants Res 2007;18:86-96.
30 Rinke S, Gersdorff N, Lange K, Roediger M. Prospective evaluation of zirconia posterior fixed partial dentures: 7-year clinical results. Int J Prosthodont 2013;26:164-71.   DOI
31 Koenig V, Vanheusden AJ, Le Goff SO, Mainjot AK. Clinical risk factors related to failures with zirconia-based restorations: an up to 9-year retrospective study. J Dent 2013;41:1164-74.   DOI   ScienceOn
32 Mainjot AK, Schajer GS, Vanheusden AJ, Sadoun MJ. Residual stress measurement in veneering ceramic by hole-drilling. Dent Mater 2011;27:439-44.   DOI   ScienceOn