Browse > Article
http://dx.doi.org/10.4047/jkap.2010.48.4.251

The influence of surface conditioning on the shear bond strength of self-adhesive resin cement to zirconia ceramics  

Jung, Ji-Hye (Department of Dentistry, Graduate School, Wonkwang University)
Jung, Seung-Hyun (Department of Dentistry, Graduate School, Wonkwang University)
Cho, Hye-Won (Department of Dentistry, Graduate School, Wonkwang University)
Kim, Yu-Lee (Department of Dentistry, Graduate School, Wonkwang University)
Publication Information
The Journal of Korean Academy of Prosthodontics / v.48, no.4, 2010 , pp. 251-258 More about this Journal
Abstract
Purpose: To evaluate the effect of surface conditioning on the shear bond strength of zirconium-oxide ceramic to 4 luting agents. Materials and methods: A total of 120 diskshaped zirconium-oxide ceramic blocks (3Y-TZP, Kyoritsu, Japan) were treated as follows: (1) Sandblasting with $110\;{\mu}m$ aluminum-oxide ($Al_2O_3$) particles; (2) tribochemical silica coating (Rocatec) using $110\;{\mu}m$ $Al_2O_3$ particles modified by silica; (3) no treatment. Then zirconium-oxide ceramic blocks bonded with 4 luting cements (RelyX luting (3M ESPE), Maxcem (Kerr), Nexus3 (Kerr), Rely X Unicem (3M ESPE)). Each group was tested in shear bond strengths by UTM. A 1-way analysis of variance and 2-way analysis of variance was used to analyze the data ($\alpha$ = .05). Results: RelyX unicem in combination tribochemical silica-coating produced a highest bond strength (P < .05). Air abrasion group and Rocatec treatment groups resulted in significantly higher than no conditioning group (P < .05). RelyX Luting groups showed lower bond strength than other groups. There were significant differences among groups (P < .05). Conclusion: Within the limitation of this study, RelyX Unicem cement provided the highest bond strength and Rocatec treatment enhanced the bond strength.
Keywords
Surface conditioning; Zirconia; Resin cement; Shear bond strength;
Citations & Related Records
연도 인용수 순위
  • Reference
1 Bindl A, Lu¨thy H, Mo¨rmann WH. Thin-wall ceramic CAD/CAM crown copings: strength and fracture pattern. J Oral Rehabil 2006;33:520-8.   DOI   ScienceOn
2 Ozcan M, Nijhuis H, Valandro LF. Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging. Dent Mater J 2008;27:99-104.   DOI   ScienceOn
3 Lu¨thy H, Loeffel O, Hammerle CH. Effect of thermocycling on bond strength of luting cements to zirconia ceramic. Dent Mater 2006;22:195-200.   DOI   ScienceOn
4 Chaiyabutr Y, McGowan S, Phillips KM, Kois JC, Giordano RA. The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic. J Prosthet Dent 2008;100:194-202.   DOI   ScienceOn
5 Ozcan M, Vallittu PK. Effect of surface conditioning methods on the bond strength of luting cement to ceramics. Dent Mater 2003;19:725-31.   DOI   ScienceOn
6 Radovic I, Monticelli F, Goracci C, Vulicevic ZR, Ferrari M. Selfadhesive resin cements: a literature review. J Adhes Dent 2008;10:251-8.
7 Senyilmaz DP, Palin WM, Shortall AC, Burke FJ. The effect of surface preparation and luting agent on bond strength to a zirconiumbased ceramic. Oper Dent 2007;32:623-30.   DOI   ScienceOn
8 Ernst CP, Cohnen U, Stender E, Willershausen B. In vitro retentive strength of zirconium oxide ceramic crowns using different luting agents. J Prosthet Dent 2005;93:551-8.   DOI   ScienceOn
9 Blatz MB, Sadan A, Martin J, Lang B. In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconiumoxide ceramic after long-term storage and thermal cycling. J Prosthet Dent 2004;91:356-62.   DOI   ScienceOn
10 Janda R, Roulet JF, Wulf M, Tiller HJ. A new adhesive technology for all-ceramics. Dent Mater 2003;19:567-73.   DOI   ScienceOn
11 Phark JH, Duarte S Jr, Blatz M, Sadan A. An in vitro evaluation of the long-term resin bond to a new densely sintered high-purity zirconium-oxide ceramic surface. J Prosthet Dent 2009;101:29-38   DOI   ScienceOn
12 Palacios RP, Johnson GH, Phillips KM, Raigrodski AJ. Retention of zirconium oxide ceramic crowns with three types of cement. J Prosthet Dent 2006;96:104-14.   DOI   ScienceOn
13 Manicone PF, Rossi Iommetti P, Raffaelli L. An overview of zirconia ceramics: basic properties and clinical applications. J Dent 2007;35:819-26.   DOI   ScienceOn
14 Aboushelib MN, Matinlinna JP, Salameh Z, Ounsi H. Innovations in bonding to zirconia-based materials: Part I. Dent Mater 2008;24:1268-72.   DOI   ScienceOn
15 Derand P, Derand T. Bond strength of luting cements to zirconium oxide ceramics. Int J Prosthodont 2000;13:131-5.
16 Blixt M, Adamczak E, Linde′n LA, Ode′n A, Arvidson K. Bonding to densely sintered alumina surfaces: effect of sandblasting and silica coating on shear bond strength of luting cements. Int J Prosthodont 2000;13:221-6.
17 Kosmac T, Oblak C, Jevnikar P, Funduk N, Marion L. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic. Dent Mater 1999;15:426-33.   DOI   ScienceOn
18 Willer J, Rossbach A, Weber HP. Computer-assisted milling of dental restorations using a new CAD/CAM data acquisition system. J Prosthet Dent 1998;80:346-53.   DOI   ScienceOn
19 Wolfart M, Lehmann F, Wolfart S, Kern M. Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods. Dent Mater 2007;23:45-50.   DOI   ScienceOn
20 Blatz MB, Phark JH, Ozer F, Mante FK, Saleh N, Bergler M, Sadan A. In vitro comparative bond strength of contemporary self-adhesive resin cements to zirconium oxide ceramic with and without air-particle abrasion. Clin Oral Investig 2010;14:187-92.   DOI   ScienceOn
21 de Oyague RC, Monticelli F, Toledano M, Osorio E, Ferrari M, Osorio R. Influence of surface treatments and resin cement selection on bonding to densely-sintered zirconium-oxide ceramic. Dent Mater 2009;25:172-9.   DOI   ScienceOn
22 Kumbuloglu O, Lassila LV, User A, Vallittu PK. Bonding of resin composite luting cements to zirconium oxide by two air-particle abrasion methods. Oper Dent 2006;31:248-55.   DOI   ScienceOn
23 Kern M, Wegner SM. Bonding to zirconia ceramic: adhesion methods and their durability. Dent Mater 1998;14:64-71.   DOI   ScienceOn
24 Blatz MB, Chiche G, Holst S, Sadan A. Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia. Quintessence Int 2007;38:745-53.
25 Derand T, Molin M, Kvam K. Bond strength of composite luting cement to zirconia ceramic surfaces. Dent Mater 2005;21:1158-62.   DOI   ScienceOn
26 Spohr AM, Borges GA, Ju′nior LH, Mota EG, Oshima HM. Surface modification of In-Ceram Zirconia ceramic by Nd:YAG laser, Rocatec system, or aluminum oxide sandblasting and its bond strength to a resin cement. Photomed Laser Surg 2008;26:203-8.   DOI   ScienceOn