Browse > Article
http://dx.doi.org/10.4047/jkap.2009.47.3.312

A study on the shear bond strengths of veneering ceramics to the colored zirconia core  

Kang, Sun-Nyo (Department of Dentistry, Graduate School, Pusan National University)
Cho, Wook (Department of Dentistry, Graduate School, Pusan National University)
Jeon, Young-Chan (Department of Dentistry, Graduate School, Pusan National University)
Jeong, Chang-Mo (Department of Dentistry, Graduate School, Pusan National University)
Yun, Mi-Jung (Department of Dentistry, Graduate School, Pusan National University)
Publication Information
The Journal of Korean Academy of Prosthodontics / v.47, no.3, 2009 , pp. 312-319 More about this Journal
Abstract
Statement of problem: Delamination of veneering porcelain from underlying ceramic substructures has been reported for zirconia-ceramic restorations. Colored zirconia cores for esthetics have been reported that their bond strength with veneered porcelain is weaker compared to white zirconia cores. Purpose: This study aimed to investigate the shear bond strength by manufacturing the veneering porcelain on the colored zirconia core, using the layering technique and heat-pressing technique, and to evaluate the clinical stability by comparing the result of this with that of conventional metal ceramic system. Material and methods: A Metal ceramic (MC) system was tested as a control group. The tested systems were Katana zirconia with CZR (ZB) and Katana Zirconia with NobelRondo Press (ZP). Thirty specimens, 10 for each system and control, were fabricated. Specimen disks, 3 mm high and 12 mm diameter, were fabricated with the lost-wax technique (MC) and the CAD-CAM (ZB and ZP). MC and ZB specimens were prepared using opaque and dentin veneering ceramics, veneered, 3 mm high and 2.8 mm in diameter, over the cores. ZP specimens were prepared using heat pressing ingots, 3 mm high and 2.8mm in diameter. The shear bond strength test was performed in a Shear bond test machine. Load was applied at a cross-head speed of 0.50 mm/min until failure. Mean shear bond strengths (MPa) were analyzed with the One-way ANOVA. After the shear bond test, fracture surfaces were examined by SEM. Results: The mean shear bond strengths (SD) in MPa were MC control 29.14 (2.26); ZB 29.48 (2.30); and ZP 29.51 (2.32). The shear bond strengths of the tested systems were not significantly different (P > .05). All groups presented cohesive and adhesive failures, and showed predominance of cohesive failures in ceramic veneers. Conclusion: 1. The shear bond strengths of the tested groups were not significantly different from the control group (P >.05). 2. There was no significant different between the layering technique and the heat pressing technique in the veneering methods on the colored zirconia core. 3. All groups presented cohesive and adhesive failures, and showed predominance of cohesive failures in ceramic veneers.
Keywords
colored zirconia; shear bond strength; heat pressing technique; layering technique;
Citations & Related Records
Times Cited By KSCI : 2  (Citation Analysis)
연도 인용수 순위
1 Guazzato M, Albakry M, Ringer SP, Swain MV. Strength, fracture toughness and microstructure of a selection of allceramic materials. Part II. Zirconia-based dental ceramics. Dent Mater 2004;20:449-56   DOI   ScienceOn
2 Potiket N, Chiche G, Finger IM. In vitro fracture strength of teeth restored with different all-ceramic crown systems. J Prosthet Dent 2004;92:491-5   DOI   ScienceOn
3 Strub JR, Beschnidt SM. Fracture strength of 5 different all-ceramic crown systems. Int J Prosthodont 1998;11:602-9   PUBMED   ScienceOn
4 Kim CH, Jeon YC, Joeng CM, Lim JS. Effect of surface treatments of zirconia ceramic on the bond strength of resin cements. J Korean Acad Prosthodont 2004;42:386-96   ScienceOn
5 Piconi C, Maccauro G. Zirconia as a ceramic biomaterial. Biomaterials 1999;20:1-25   DOI   ScienceOn
6 Vult von Steyern P, Carlson P, Nilner K. All-ceramic fixed partial dentures designed according to the DC-Zirkon technique. A 2-year clinical study. J Oral Rehabil 2005;32:180-7   DOI   ScienceOn
7 D$\ddot{u}$ndar M, Ozcan M, G$\ddot{o}$ke\c{c} B, C$\ddot{o}$mleko$\check{g}$lu E, Leite F, Valandro LF. Comparison of two bond strength testing methodologies for bilayered all-ceramics. Dent Mater 2007;23:630-6   DOI   ScienceOn
8 D$\ddot{u}$ndar M, Ozcan M, Co$\ddot{o}$mlekoglu E, G$\ddot{u}$ng$\ddot{o}$r MA, Artun$\c{c}$ C. Bond strengths of veneering ceramics to reinforced ceramic core materials. Int J Prosthodont 2005;18:71-2   PUBMED   ScienceOn
9 Al-Dohan HM, Yaman P, Dennison JB, Razzoog ME, Lang BR. Shear strength of core-veneer interface in bi-layered ceramics. J Prosthet Dent 2004;91:349-55   DOI   ScienceOn
10 Jeoung HC. Fracture strength of zirconia monolithic crowns. J Korean Acad Prosthdont 2006;44:157-64   과학기술학회마을   ScienceOn
11 Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Effect of zirconia type on its bond strength with different veneer ceramics. J Prosthodont 2008;17:401-8   DOI   ScienceOn
12 Denry Isabelle, Kelly JR. State of the art of zirconia for dental applications. Dent Mater 2008;24:299-307   DOI   ScienceOn
13 Gorman CM, Hill RG. Heat-pressed ionomer glass-ceramics. Part I: an investigation of flow and microstructure. Dent Mater 2003;19:320-6   DOI   ScienceOn
14 Gorman CM, Hill RG. Heat-pressed ionomer glass-ceramics. Part II. Mechanical property evaluation. Dent Mater 2004;20:252-61   DOI   ScienceOn
15 Peterson IM, Wuttiphan S, Lawn BR, Chyung K. Role of microstructure on contact damage and strength degradation of micaceous glass-ceramics. Dent Mater 1998;14:80-9   DOI   ScienceOn
16 ISO 9693. Metal-ceramic bond characterization (Schwickerath crack initiation test). Geneva, Switzerland: International Organization for standardization; 1999).
17 Shah K, Holloway JA, Denry IL. Effect of coloring with various metal oxides on the microstructure, color, and flexural strength of 3Y-TZP. J Biomed Mater Res B Appl Biomater 2008;87:329-37   DOI   PUBMED   ScienceOn
18 Devigus A, Lombardi G. Shading Vita In-ceram YZ substructures: influence on value and chroma, part II. Int J Comput Dent 2004;7:379-88   PUBMED   ScienceOn
19 Guazzato M, Albakry M, Swain MV, Ironside J. Mechanical properties of In-Ceram Alumina and In-Ceram Zirconia. Int J Prosthodont 2002;15:339-46   PUBMED   ScienceOn
20 Aboushelib MN, Kler M, Feilzer AJ. Effect of veneering method on the fracture and bond strength of bilayered zirconia restoration. Int J Prosthodont 2008;21:237-40   PUBMED   ScienceOn
21 Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Microtensile bond strength of different components of core veneered allceramic restorations. Part II: Zirconia veneering ceramics. Dent Mater 2006;22:857-63   DOI   ScienceOn
22 Chevalier J, Deville S, Mu ¨nch E, Jullian R, Lair F. Critical effect of cubic phase on aging in 3mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis. Biomaterials 2004;25:5539-45   DOI   ScienceOn
23 Guess PC, Kulis A, Witkowski S, Wolkewitz M, Zhang Y, Strub JR. Shear bond strengths between different zirconia cores and veneering ceramics and their susceptibility to thermocycling. Dent Mater 2008;24:1556-67   DOI   ScienceOn
24 Hara AT, Pimenta LA, Rodrigues AL Jr. Influence of crosshead speed on resin-dentin shear bond strength. Dent Mater 2001;17:165-9   DOI   ScienceOn