MECHANICAL PROPERTIES OF LASER-WELDED CAST TITANIUM AND TITANIUM ALLOY  

Yun, Mi-Kyung (Department of Prosthodontics, College of Dentistry, Chonnam National University)
Kim, Hyun-Seung (Department of Prosthodontics, College of Dentistry, Chonnam National University)
Yang, Hong-So (Department of Prosthodontics, College of Dentistry, Chonnam National University)
Vang, Mong-Sook (Department of Prosthodontics, College of Dentistry, Chonnam National University)
Park, Sang-Won (Department of Prosthodontics, College of Dentistry, Chonnam National University)
Park, Ha-Ok (Department of Prosthodontics, College of Dentistry, Chonnam National University)
Lee, Kwang-Min (School of Materials Science and Engineering, Chonnam National University)
Publication Information
The Journal of Korean Academy of Prosthodontics / v.44, no.5, 2006 , pp. 642-653 More about this Journal
Abstract
Purpose : The purpose of this study was to investigate the effect of the output energy(voltage) of laser welding on the strength and properties of joint of cast titanium(CP Gr II) and titanium alloy(Ti-6Al-4V). Material and method : Cast titanium and its alloy rods(ISO6871) were prepared and perpendicularly cut at the center of the rod. After the cut halves were fixed in a jig, and the joints welded with a laser-welding machine at several levels of output voltage of $200V{\sim}280V$. Uncut specimens served as the non-welded control specimens The pulse duration and pulse spot size employed in this study were 10ms and 1.0mm respectively. Tensile testing was conducted at a crosshead speed of 0.5mm/min. The ultimate tensile strength(MPa) was recorded, and the data (n=6) were statistically analyzed by one-way analysis of variance(ANOVA) and Scheffe's test at ${\alpha}$=0.05. The fracture surface of specimens investigated by scanning electron microscope (SEM). Vickers microhardness was measured under 500g load of 15seconds with the optimal condition of output voltage 280V. Results : The results of this study were obtained as follows, 1. When the pulse duration and spot size were fixed at 10ms and 1.0mm respectively, increasing the output energy(voltage) increased UTS values and penetration depth of laser welded to titanium and titanium alloy. 2. For the commercial titanium grade II, ultimate tensile strength(665.3MPa) of the specimens laser-welded at voltage of 280V were not statistically(p>0.05) different from the non-welded control specimens (680.2MPa). 3. For the titanium alloy(Ti-6Al-4V), ultimate tensile strength(988.3MPa) of the specimens laser-welded at voltage of 280V were statistically(p<0.05) different from the non-welded control specimens (665.0MPa). 4. The commercial titanium grade II and titanium alloy(Ti-6Al-4V) were Vickers microhardness values were increased in the fusion zone and there were no significant differences in base metal, heat-affected zone.
Keywords
Titanium; Titanium alloy; Centrifugal Casting; Laser welding;
Citations & Related Records
연도 인용수 순위
  • Reference
1 Okazaki Y, Tateishi T, Kyo K, Ito Y. Effect of small quantity of oxygen nitrogen on mechanical properties new titanium alloys for medical implant. J Japan Inst Metals 1998:62:207
2 Bruce GJ, Hall WB. Nickel hypersensitivityrelated periodontitis. Compend Contin Educ Dent 1995:16:178,180-4:Quiz 186
3 Ida K. Dental application of titanium and its alloys. Dental Journal 1989:30:297
4 Chern Lin JH, Moser JB, Taira M, Greener EH. Cu-Ti, Co-Ti and Ni-Ti systems : Corrosion and microhardness. Oral Rehabil 1990:17:383-93   DOI
5 Moser JB, Lin JH, Taira M, Greener EH. Development of dental Pd-Ni alloys. Dent Mater 1985:1:37-40   DOI   ScienceOn
6 Henderson D. McCracken's removable partial prosthodontics. 7th ed., St. Louis, C. V. Mosby Co ., 1985
7 Lancaster JF. Metallurgy if welding. 5th ed. London : Chapman & Hall 1993 p.3855a,79-92b,157-8c
8 Wee AG, Aquilino SA, Schneider RL. Strategies to achieve fit in implant prosthodontics : a review of the literature. Int J Prostho 1999:12:167-178
9 Derand T. Porcelain bond to laser-welded titanium surface. Dent Mater 1995:11:93-95   DOI   ScienceOn
10 Gordon TE, Smith DL. Laser welding of prostheses-An initial report. J Prosthet Dent 1970:24:472-476   DOI   ScienceOn
11 Dawes C. Laser welding. Cambridge : Abington Publishing Ltd., in association with The welding Institute. 1992
12 Berg E, Wagnere WC, Davik G, Dootz ER. Mechanical properties of laser-welded cast and wrought titanium. J Prosthet Dent 1995:74:250-257   DOI   ScienceOn
13 Nabalung DP, Nicholls JI. Laser welding of a cobalt-chromium removable partial denture alloy. J Prosthet Dent 1998:79:285-290   DOI   ScienceOn
14 Kim JJ, Choi JK, Hong CP. Three Dimensional Prediction of Shrinkage Defects Considering Solidification Contraction. Kor Acad Indus Tech 1995:15:93
15 Hruska AR, Borelli P. Quality criteria for pure titanium casting, laboratory soldering, intraoral welding, and a device to aid in making uncontaminated castings. J Prosthet Dent 1991:66:561-565   DOI   ScienceOn
16 Taylor JC, Hondrum SO, Prasad A, Brodersen CA. Effects of joint configuration for the arc welding of cast Ti-6Al-4V alloy rods in argon. J Prosthet Dent 1998:79:291-297   DOI   ScienceOn
17 Taira M, Moser JB, Greener EH. Face coats for dental casting of titanium alloys. J Dent Res 1985:64:317
18 Mueller HJ, Giuseppetti AA, Waterstrat RM. Phosphate-bonded investment materials for titanium casting. J Dent Res 1990:69:367
19 Smith DL, Burnett AP, Gordon TE. Laser welding of gold alloy. J Dent Res 1972:51:161-167   DOI   ScienceOn
20 Hamanaka H, Doi H, Yoneyama T, Okuno O. Dental casting of titanium and Ni-Ti alloys by a new casting machine. J Dent Res 1989:68:1529-1533   DOI   ScienceOn
21 Bergendal B, Palmqvist S. Laser-welded titanium frameworks for fixed prostheses supported by osseointegrated implants : a 2year multicenter study report. Int J Oral Maxillofac Implant 1995:10:199-206
22 Sjogren G, Andersson M, Bergman M. Laser welding of titanium in dentistry. Acta Odontol Scand 1988:46:247-253   DOI
23 Chai T, Chou CK. Mechanical properties of laser-welded cast titanium joints under different conditions. J Prosthet Dent 1998:79:477-483   DOI   ScienceOn
24 Yamagishi T, Ito M, Oshida Y, Hashem A. Tensile strength and elongation of laserwelded titanium. J Dent Res 1993:72-131   DOI   ScienceOn
25 Roggensack M, Walter MH, Boning KW. Studies on laser-and plasma -welded titanium. Dent Mater 1993:9:104-107   DOI   ScienceOn
26 Song YG, Ha IS, Song KY. Tensile Strength of Laser Welded-Titanium and Gold Alloys. J Kor Acad Prostho 2000:38:200-213   과학기술학회마을
27 Riesgo O, Greener EH, Moser JB. Titanium alloys with dental porcelain. J Dent Res 1984:63:319
28 Watanabe I, Topham DS. Tensile strength and elogation of laser-welded Ti and Ti-6Al-7Nb. J Biomed Mater Res Part B, Appl Biomater 2004:71:46-51
29 Apotheker H, Nishimura I, Seerattan C. Laser-welded vs soldered nonprecious alloy dental bridges: A comparative study. Lasers in Surgery and Medicine 1984:4:207-213   DOI   ScienceOn
30 Lee JJ, Kim KS, Ahn SG, Bae TS, Park CW. Mechanical properties of laser welded titanium joints. J Korean Res Soc Dent Mater 2003:30:147-152
31 Lugowski SJ, Smith DC, McHugh AD, Loon V. Release of metal ions from dental implant materials in vivo: Determination of Al, Co, Cr, Mo, Ni, V and Ti in organ tissue. J Biomed Mater Res 1991:25:14431458
32 Bannon BP, Mild EE, Titanium alloys in surgical implants. ASTM STP 796, Philadelphia, Pa. 1981:7
33 Greener EH, Moser JB, Opp J, Szurgot K, Marker BC. Properties of centrifugally cast commercial Ti and Ti-6Al-4V. J Dent Res 1986:65:317
34 Brunette DM, Tengvall P, Textor M, Thomsen P. Titanium in Medicine. 2001
35 Smith DC. Acrylic denture: Mechanical evaluation of midline fracture. Br Dent J 1961:110:257-267
36 Ida K, Tsutsumi S, Togaya T. Titanium or titanium alloys for dental casting. J Dent Res 1980:59:985
37 Preston JD, Reisbick MH. Laser fusion of selected dental casting. J Dent Res 1975:54:232-238
38 Rubenstein JE. Stereo laser-welded titanium implant frameworks : Clinical and laboratory procedures with a summary of 1-year clinical trials. J Prosthet Dent 1995:74:284-293   DOI   ScienceOn
39 Hruska AR. A novel method for vaccum casting titanium. Int J Prosthodont 1990:3:142-145
40 Okuno O, Hamanaka H. Titanium and titanium alloy in dental use. Dental Journal 1989:30:317
41 Sunnerkrantz PA, Syverud M, Her H. Effect of casting atmosphere on the quality of Ticrowns. Scand J Dent Res 1990:98:268272
42 Togaya T, Shinosaki T, Hatano H. Application of laser welding for dental laboratory works, Optimization of laser beam parameters by laser joint strength tests. Quint Dent Tech 2002:Extra issue: 190-198
43 Lee SY, Chang IT, Heo SJ, Yim SH. Mechanical properties of titanium connectors treated by various welding techniques. J Kor Acad Prostho 1999:37:545-565   과학기술학회마을
44 Weber H. The clinical acceptance of dental nickel-chrome alloys. Int Dent J 1983:33:49-54
45 Meyer E. Non-precious alloys for metalceramics. ZWR. 1988:97:774-81
46 Takahashi J, Kimura H, Lautenschlager EP, Lin JH, Moser JB, Greener EH. Casting pure titanium into commercial phosphate bonded $SiO_2$ investment molds. J Dent Res 1990:69:1800-1805   DOI   ScienceOn
47 Boyer R, welsch G, Collings EW. Materials properties handbook -Titanium alloys. ASM 1994
48 Togaya T, Shinosaki T. Introduction to laser welding in density. Quint Dent Tech 1999:27:52-63
49 Linden B, Jemt T. Fixed implant-supported prostheses with welded titanium frameworks. Int J Periodont Rest Dent 1992:12:177-183