Performance Evaluation of Repair Material and Method for Reinforced Concrete Structure by Long Term Exposure Experiment  

Kim, Moo-Han (Dept. of Architectural Engineering, Chungnam National University)
Kim, Gyu-Yong (Dept. of Architectural Engineering, Chungnam National University)
Cho, Bong-Suk (Dept. of Architectural Engineering, Chungnam National University)
Kim, Young-Duck (Dept. of Architectural Engineering, Chungnam National University)
Kim, Young-Sun (Dept. of Architectural Engineering, Chungnam National University)
Publication Information
Journal of the Korea Concrete Institute / v.19, no.1, 2007 , pp. 39-46 More about this Journal
Abstract
In this study, for the establishment of the performance evaluation methods and the quality control standards of durability recovery method, the quantitative exposure data by long term exposure test under the coast and normal atmosphere is accumulated and analyzed. Investigating and evaluating the result of exposure test during 30 months of exposure age under the coastal and normal atmosphere environment, carbonation depth and chloride-ion penetration depth very little penetrated than cover depth. It seems reasonable to conclude that main cause of Corrosion of reinforcing bar are chloride-ion and macro cell from the result of corrosion area and corrosion velocity. Therefore, it is considered to be applied as the fundamental data on the performance evaluation and quality control standards of repair material and method through continuous exposure test in the future.
Keywords
long-term exposure experiment; reinforced concrete structure; repair material and method; performance evaluation;
Citations & Related Records
연도 인용수 순위
  • Reference
1 건설교통부, '염해 및 탄산화 피해를 입은 콘크리트 구조물의 내구성 회복을 위한 보수공법 시스템 개발 및 실용화 방안', 건설기술연구개발사업 연차보고서, 2003. 4, pp.555-723
2 김무한, 조봉석, 김영덕, 윤종기, 김재환, 김용로, '표면 피복종휴에 따른 복합열화환경하의 철근콘크리트 부식 특성에 관한 실험적 연구', 한국콘크리트학회 가을학술 발표회 논문집, 15권 2호, 2003. 11, pp.86-89
3 기상청, http://www.kma.go.kr. 기후통계자료
4 정해문, 유환구, 류총현, 안태송, 김수만, 오병환, '해양 환경에 위치한 국내 고속도로 교량의 비래염분량 측정 결과', 한국콘크리트학회 봄학술발표회 논문집, 14권 1호, 2002. 5, pp.743-748
5 日本建築撃舎, 高耐久性鍛筋コンクリートの設計施工指針 (案) 同解説, 日本建築皐舎, 1991, pp.179-184
6 이종득, 철근부식진단, 도서출판 일광, 2001. 11, pp.1-12
7 日本コンクリート工率協合, コンクリート構造物の補修工 法研究委員舎報告書(III) 補修工法の性能評債のための暴 露貰験ー, 1996. 10, pp.1-44
8 lIS A 6203, セメント混和用ポリマーディスパーション及 ぴ再乳化形粉末樹脂ラITS, Japan, 1996
9 Jieyaing Zhang, et al, 'Corrosion of Concrete Reinforcement and Electrochemical Factors in Concrete Patch Repair', Canadian Journal of Civil, Vol.33, pp.785-793
10 C. Andrade, C. Alonso, and J. Sarr, 'Corrosion rate evolution on concrete structures exposed to the atmosphere', Cement & Concrete Composites, 2002, pp.55-64
11 須田久美子, S. Misra, et at, '腐食ひびわれ後生限界量に 閲する解樟的検討', コンクリート工事年次論文報告集, Vol.14, No.1, 1992, pp.751-756
12 武若耕司ほか, 'コンクリート中の銭筋腐食がRC部材の力 撃的性肢に及ぼす影響', 第6回コンク\)ート工準年三文講演 舎論文集, 1984
13 日本建築事合, 鍛筋コンクリート造建築物の耐久性調査 診断および補修指針(案) 同解説イす2.補修工法の補修殻呆 評償試験(案), 1997, pp.203-216