Porous concrete has good permeability sine it contains about 10∼20 % of voids, had has been introduced to korea in early 1980's. It, however, has problems such as a lack of optimized mixture, low strength and durability, and etc. It is thus Interesting to manufacture high-performance porous concrete satisfying the mechanical characteristics to be supplied In practical construction. The results of this study were as follows : the compressive strength was 132∼221 kgf/$\textrm{cm}^2$, the splitting tensile strength was 15∼25 kgf/$\textrm{cm}^2$, the flexural strength was 36∼54 kgf/$\textrm{cm}^2$, and the coefficient permeability was 1.05${\times}$10$\^$-1/ ∼ 9.20${\times}$10$\^$-2/ cm/sec. In order to change the maximum size of aggregate, It is believed that other mixtures should be studied further.
Keywords
porous concrete; coefficient permeability; strength; durability;
Citations & Related Records
연도 인용수 순위
  • Reference
1 大友武臣 外, "透水性コンクリ-トの開發に關する硏究", 第45回セメント技術大會 講連集, 1991, pp.750-755.
2 出村克宣外, "ポリマ-混入透水コンクリ-トの開發," セメント .コンクリ-ト論文集, No.47, 1993, pp.226-231.
3 한국콘크리트학회, 최신 콘크리트공학, 1994.
4 Charles J. Kohomen, "Porous Portland Cement Concrete as an Airport Runway Overlay," USACERL, 1989.
5 安崎 裕 外, "透水性コンクリ-ト鋪裝の適用性に關する實驗", 道路建設, 1988, pp.52-56.
6 松尾伸二 外, "超泡劑を用いた透水性コンクリ-トの特性," 第46回セメント技術大會 講連集, 1992, pp.948-953.
7 管原賢司, 田中耕作, 排水性鋪裝の耐久性向上の一例, 建設圖書(株), 1995.
8 松尾伸二外, "透水性コンクリ-トの透水 . 透濕 . 吸音特性," コンクリ-ト工學年次論文報告集, Vol.15, 1993, pp.525-530.
9 한국건자재시험연구원, 투수콘크리트의 성능평가, 1996
10 高橋知生 外, "透水性コンクリ-トの開發", コンクリ-ト工學年次論文報告集, Vol.14, 1992, p.351-356.