산성 용액에서 고크롬 주철의 전면 부식 거동

General Corrosion Behavior of High Chromium Cast Iron in an Acid Solution

  • 이준섭 (국립창원대학교 신소재공학부) ;
  • 이준형 (국립창원대학교 소재융합시스템공학과) ;
  • 오준석 (국립창원대학교 신소재공학부) ;
  • 이재현 (국립창원대학교 신소재공학부)
  • Lee, Jun-Seob (Materials Science and Engineering, Changwon National University) ;
  • Lee, Jun-Hyung (Materials Convergence and System Engineering, Changwon National University) ;
  • Oh, Jun-Seok (Materials Science and Engineering, Changwon National University) ;
  • Lee, Je-Hyun (Materials Science and Engineering, Changwon National University)
  • 투고 : 2021.11.11
  • 심사 : 2021.11.22
  • 발행 : 2021.12.31

초록

The effect of carbon addition on the general corrosion behavior of high-chromium cast iron (HCCI) was studied by a scanning electron microscope with energy dispersive spectroscopy (SEM-EDS) or electron back-scattered diffraction (EBSD), or electrochemical polarization techniques in 0.1 mol dm-3 H2SO4 + 0.05 mol dm-3 HCl at room temperature. The addition of 2.1-2.8 wt% carbon to HCCI increased the fraction of eutectic austenite and eutectic carbide phases, while that of HCCI decreased the fraction of the primary austenitic phase. Potentiostatic polarization of the HCCI at -0.35 VSSCE or 0.0 VSSCE resulted in preferential general corrosion of the primary austenitic or eutectic austenitic phases, respectively. The decrease in corrosion current density and the shift in noble corrosion potential direction with increasing carbon content in the HCCI indicated that the fraction and the chemical composition of austenitic (primary and eutectic) and carbide phases were strongly related to the general corrosion behavior of the HCCI.

키워드

과제정보

이 논문은 2021~2022년도 창원대학교 자율연구과제 연구비 지원으로 수행된 연구결과임

참고문헌

  1. Y. Zheng, W. Liu, Z. Yao, and W. Ke, Damage mechanisms and metallic materials development in multiphase flow, Corrosion Science and Technology, 1, 41 (2002). https://www.j-cst.org/opensource/pdfjs/web/pdf_viewer.htm?code=C00010100041
  2. C. K. Kim, S. Lee, and J. Y. Lee, Wear Resistance and Fracture Toughness of Heat-treated Duo-cast Materials Composed of High-Chromium White Cast Iron and Low-Chromium Steel, The Korean Journal of Metals and Materials, 42, 877 (2004). Doi: http://kjmm.or.kr/past/view_kiss.asp?a_key=2382457
  3. R. Lee, and Y. S. Kim, Effect of Heat treatment on Hardness and Corrosion Resistance of Super Cast Iron, The Korean Journal of Metals and Materials, 52, 511 (2013) Doi: https://doi.org/10.3365/KJMM.2014.52.7.511
  4. H. W. Jo, J. H. Do, W. J. Jo, H. D. Chung, J. H. Lee, and C. Y. Jo, Effect of Primarily Solidified Structure on the Microstructure and the Mechanical Properties of High Cr White Iron, Journal of Korea Foundry Society, 35, 178 (2015). Doi: http://dx.doi.org/10.7777/jkfs.2015.35.6.178
  5. U. P. Nayak, M. A. Guitar, and F. Mucklich, A Comparative Study on the Influence of Chromium on the Phase Fraction and Elemental Distribution in As-Cast High Chromium Cast Irons: Simulation vs. Experimentation, Metals, 10, 30 (2019) Doi: https://doi.org/10.3390/met10010030
  6. ASM International, ASM Specialty Handbook Cast Irons, pp.107-122 (1996).
  7. S. K. Yu, A Study on the Solidification Structure, Heat-Treated Microstructure and Mechanical Property of Multi-Component White Cast Iron for Hot Forged Roller, Korean Journal of Materials Research, 8, 436 (1998). http://journal.mrs-k.or.kr/journal/article.php?code=23096
  8. J. U. Kwon, C. S. Park, and M. H. Kim, Effects of Ti addition on the Microstructure and Mechanical Properties of High Chromium White Cast Iron, Journal of Korea Foundry Society, 18, 48 (1998). https://kiss.kstudy.com/thesis/thesis-view.asp?key=173853
  9. R. J. Chung, X. Tanga, D. Y. Li, B. Hinckley, and K. Dolman, Effects of titanium addition on microstructure and wear resistance of hypereutectic high chromium cast iron Fe-25wt.%Cr-4wt.%C, Wear, 267, 356 (2009). Doi: https://doi.org/10.1016/j.wear.2008.12.061
  10. C. P. Tabrett, I. R. Sare, and M. R. Ghomashchi, Microstructure-property relationships in high chromium white iron alloys, International Materials Reviews, 41, 59 (1996). https://doi.org/10.1179/imr.1996.41.2.59
  11. I. Chakrabarty, and A. Basak, Structural study of Cr-MnCu white cast irons, Journal of Materials Science Letters, 6, 1399 (1987). https://link.springer.com/content/pdf/10.1007/BF01689301.pdf
  12. J. Wang, W. Shi, S. Xiang, and R. G. Ballinger, Study of the corrosion behaviour of sensitized 904L austenitic stainless steel in Cl- solution, Corrosion Science, 181, 109234 (2021). Doi: https://doi.org/10.1016/j.corsci.2020.109234
  13. N. Fu, X, Tang, D. Y. Li, L. Parent, and H. Tian, In situ investigation of local corrosion at interphase boundary under an electrochemical-atomic force microscope, Journal of Solid State Electrochemistry, 19, 374 (2015) Doi: https://doi.org/10.1007/s10008-014-2601-1