Comparative analysis of strain according to the deposition of a constant temperature water bath of a denture-base artificial tooth produced using three-dimensional printing ultraviolet-curing resin

3D 프린팅용 광경화 수지를 사용하여 제작한 의치상용 인공치아의 항온수조 침적에 따른 변형률 비교 분석

  • Kim, Dong-Yeon (4RD Dental Laboratory) ;
  • Lee, Gwang-Young (Department of Dental Laboratory Technology, Wonkwang Health Science University) ;
  • Kim, Jae-Hong (Department of Dental Laboratory Science, College of Health Science, Catholic University of Pusan) ;
  • Yang, Cheon-Seung (Department of Dental Laboratory, Donga University of Health)
  • 김동연 (폴드 치과기공소) ;
  • 이광영 (원광보건대학교 치기공과) ;
  • 김재홍 (부산가톨릭대학교 보건과학대학 치기공학과) ;
  • 양천승 (동아보건대학교 치기공과)
  • Received : 2020.07.17
  • Accepted : 2020.08.28
  • Published : 2020.09.30

Abstract

Purpose: This study is a comparative analysis of the strain according to deposition in a constant temperature water bath after manufacturing ultraviolet (UV)-cured artificial teeth. Methods: As a control group, 10 ready-made artificial teeth were selected as the first molar on the right side of the maxilla (RT group). Silicone was used as a duplicate of the artificial denture teeth. Experimental teeth were prepared in two groups using the prepared silicone mold. In the first experimental group, the UV-cured resin was injected into the negative silicone, followed by irradiation with a UV-curing machine for 5 minutes (5M group). In the second experimental group, the UV-cured resin was injected into the negative silicone, and then irradiated for 30 minutes using a UV-curing machine (30M group). The one-way ANOVA was performed, and post-test was analyzed by Tukey. Results: When immersed in a water bath for 15 days, it was found to be -0.3% in the RT group, -0.6% in the 5M group, and -0.7% in the 30M group. The results revealed -0.2% in the RT group, 0.2% in the 5M group, and -0.2% in the 30M group when they were in the bath for 30 days. Conclusion: In the water bath, the swelling was greater when deposited for 1 to 15 days, but was less when deposited for 15 to 30 days.

Keywords

References

  1. Kim DY, Jeong ID, Kim JH, Kim HY, Kim WC. Reproducibility of different coping arrangements fabricated by dental micro-stereolithography: evaluation of marginal and internal gaps in metal copings. J Dent Sci. 2018;13:220-225. https://doi.org/10.1016/j.jds.2017.06.006
  2. Kim DY, Kim JH, Kim HY, Kim WC. Comparison and evaluation of marginal and internal gaps in cobalt-chromium alloy copings fabricated using subtractive and additive manufacturing. J Prosthodont Res. 2018;62:56-64. https://doi.org/10.1016/j.jpor.2017.05.008
  3. Kang W, Lee HK. A study of three-dimensional evaluation of the accuracy of resin provisional restorations fabricated with the DLP printer. J Kor Aca Den Tec. 2020;42:35-41. https://doi.org/10.14347/kadt.2020.42.1.35
  4. Do HS, Kim DJ, Kim HJ. Application of UV-curable materials. J Adhes Interface. 2003;4:41-51.
  5. Kim DY. Difference between shrinkage rate of irradiation amount of 3D printing UV curable resin and shrinkage rate according to a constant temperature water bath. J Kor Aca Den Tec. 2020;42:113-120. https://doi.org/10.14347/KADT.2020.42.2.113
  6. Kim MJ, Kim KH, Yeo DH. Fabrication of computeraided design/computer-aided manufacturing complete denture and conventional complete denture: case report. J Dent Rehabil Appl Sci. 2016;32:141-148. https://doi.org/10.14368/jdras.2016.32.2.141
  7. Lee S, Hong SJ, Paek J, Pae A, Kwon KR, Noh K. Comparing accuracy of denture bases fabricated by injection molding, CAD/CAM milling, and rapid prototyping method. J Adv Prosthodont. 2019;11:55-64. https://doi.org/10.4047/jap.2019.11.1.55
  8. Jeong DG, Oh KC, Shim JS, Park JM. Rehabilitation with implant-supported fixed dental prostheses using digital duplication technique on customized artificial tooth, interim denture and implant surgical template: a case report. J Korean Acad Prosthodont. 2019;57:397-404. https://doi.org/10.4047/jkap.2019.57.4.397
  9. Choi YS, Lee JS, Cho IH. Comparative study on wear resistance and hardness of several artificial resin teeth. J Dent Rehabil Appl Sci. 2008;24:129-146.
  10. Kim WC, Kim JH, Lee WS, Kim KB, Kim JH, Jeon JH, et al. Dental materials. 4th ed. Seoul: Daihak Publishing Company, 2015.
  11. Wimmer T, Gallus K, Eichberger M, Stawarczyk B. Complete denture fabrication supported by CAD/CAM. J Prosthet Dent. 2016;115:541-546. https://doi.org/10.1016/j.prosdent.2015.10.016
  12. Chen SG, Yang J, Jia YG, Lu B, Ren L. TiO2 and PEEK reinforced 3D printing PMMA composite resin for dental denture base applications. Nanomaterials (Basel). 2019;9:1049. https://doi.org/10.3390/nano9071049
  13. Park KM. Study on shear bond strength of various composite resins to artificial denture teeth. J Kor Aca Den Tec. 2014;36:171-177. https://doi.org/10.14347/kadt.2014.36.3.171
  14. Kim JY, Kim HS, Pae AR. Considerations for increasing denture stability: a case report. J Korean Acad Prosthodont. 2012;50:311-317. https://doi.org/10.4047/jkap.2012.50.4.311
  15. ASTM International. ASTM C326-09, standard test method for drying and firing shrinkages of ceramic whiteware clays. West Conshohocken (PA): ASTM International, 2009.
  16. Kang SY, Park JH, Kim JH, Kim WC. Accuracy of provisional crowns made using stereolithography apparatus and subtractive technique. J Adv Prosthodont. 2018;10:354-360. https://doi.org/10.4047/jap.2018.10.5.354
  17. Park JS, Park MG. Effect of aging treatment on the flexural properties of polymer provisional restoration materials. Korean J Dent Mater. 2013;40:215-221.
  18. Kim DY, Park JY, Bae SY, Kang HW, Kim JH, Kim WC. Evaluation of fitness according to application of glass fiber reinforcement for lower jaw complete denture. J Kor Aca Den Tec. 2018;40:201-207.
  19. Park DR, Bae JM. Mechanical properties and biocompatibility of experimental 3D printing denture base resin. Korean J Dent Mater. 2019;46:253-262. https://doi.org/10.14815/kjdm.2019.46.4.253
  20. Kim DY, Jung ID, Park JY, Kang SY, Kim JH, Kim WC. Accuracy evaluation of resin complete denture made with glass fiber mesh reinforcement before and after curing. J Kor Aca Den Tec. 2017;39:25-33.