This paper is a basic study to improve durability by imparting hydrophobicity to the surface and sphere of cement-based materials. A cement mortar to which a silane/siloxane-based mixed water repellent was added was prepared, and its initial hydration performance, flow performance, and compressive strength were measured. In addition, after the surface was abraded, the water contact angle and water absorption were measured. The flow of cement mortar to which the water repellent was added was found to decrease up to 1.5% in the addition amount of the water repellent agent, and increased at 3.0% in the addition amount. It was found that the setting time of the cement paste was delayed in both the initial setting and the termination when the water repellent was added. It was found that the compressive strength decreased from 3.0% of the maximum added amount of the water repellent to a maximum of 30%. The contact angle was found to increase when the water repellent was added to the cement mortar, and the contact angle after surface polishing was found to be larger than before surface polishing. The addition of the water repellent showed hydrophobicity not only on the surface but also on the surface and cross section damaged by polishing. The water absorption rate was found to decrease when the water repellent was added to the cement mortar, and the water absorption rate after surface polishing was found to be greater than before surface polishing.

본 논문은 시멘트계 재료의 표면 및 구체에 소수성을 부여하여 내구성을 향상시키기 위한 기초연구이다. 실란/실록산계 혼합형 발수제를 첨가한 시멘트 모르타르를 제조하고 초기 수화성능 및 유동성능, 재령별 압축강도를 측정하였다. 또한 표면연마 전후의 물접촉각 및 흡수율을 측정하였다. 실란/실록산계 혼합형 발수제를 첨가한 시멘트 모르타르의 플로우는 발수제 첨가량 1.5%까지는 감소하는 것으로 나타났으며 첨가량 3.0%에서는 증가하였다. 실란/실록산계 혼합형 발수제를 첨가할 경우 시멘트 페이스트의 응결시간은 초결 및 종결 모두 지연되는 것으로 나타났다. 압축강도는 발수제의 최대 첨가량 3.0%에서 최대 30%까지 감소하는 것으로 나타났다. 실란/실록산계 발수제를 시멘트 모르타르에 첨가할 경우 접촉각은 커지는 것으로 나타났으며, 표면연마 후 접촉각은 표면연마 전보다 커지는 것으로 나타났다. 실란/실록산계 혼합형 발수제의 첨가는 표면뿐만 아니라 연마로 인하여 손상된 표면과 단면에서도 소수성을 나타내었다. 실란/실록산계 혼합형 발수제를 시멘트 모르타르에 첨가할 경우 흡수율은 낮아지는 것으로 나타났으며, 표면연마 후 흡수율은 표면연마 전보다 커지는 것으로 나타났다.

Keywords

References

  1. Bader, T., Waldner, B. J., Unterberger, S. H., & Lackner, R. (2019). On the performance of film formers versus penetrants as water-repellent treatment of High-Performance Concrete (HPC) surfaces. Construction and Building Materials, 203, 481-490. https://doi.org/10.1016/j.conbuildmat.2019.01.089
  2. Bhushan, B., & Jung, Y. C. (2011). Natural and biomimetic artificial surfaces for superhydrophobicity, self-cleaning, low adhesion, and drag reduction. Progress in Materials Science, 56(1), 1-108. https://doi.org/10.1016/j.pmatsci.2010.04.003
  3. Chen, H., Feng, P., Du, Y., Jiang, J., & Sun, W. (2018). The effect of superhydrophobic nano-silica particles on the transport and mechanical properties of hardened cement pastes. Construction and Building Materials, 182, 620-628. https://doi.org/10.1016/j.conbuildmat.2018.06.146
  4. Falchi, L., Zendri, E., Muller, U., & Fontana, P. (2015). The influence of water-repellent admixtures on the behaviour and the effectiveness of Portland limestone cement mortars. Cement and Concrete Composites, 59, 107-118. https://doi.org/10.1016/j.cemconcomp.2015.02.004
  5. Gao, M. L., Zhao, S. Y., Chen, Z. Y., Liu, L., & Han, Z. B. (2019). Superhydrophobic/Superoleophilic MOF Composites for Oil-Water Separation. Inorganic chemistry, 58(4), 2261-2264. https://doi.org/10.1021/acs.inorgchem.8b03293
  6. Kim, W. S., & Lee, H. S. (2020). Mechanical Properties and Absorption of Mortars Containing Hybrid Water-Repellent. In Proceedings of the Korean Institute of Building Construction Conference (pp. 88-89). The Korean Institute of Building Construction.
  7. Kim, W. S., Yang, H. M., Kim, Y. K., & Lee, H. S. (2019). An Experimental Study on Physical Properties and Water Repellent Performance of Cement Mortar According to Mixing Method of Water Repellent. In Proceedings of the Korean Institute of Building Construction Conference (pp. 99-100). The Korean Institute of Building Construction.
  8. Kobayashi, K., & Kojima, Y. (2017). Effect of fine crack width and water cement ratio of SHCC on chloride ingress and rebar corrosion. Cement and Concrete Composites, 80, 235-244. https://doi.org/10.1016/j.cemconcomp.2017.03.006
  9. Li, Y., Zheng, M., Ma, L., Zhong, M., & Shen, W. (2008). Fabrication of hierarchical ZnO architectures and their superhydrophobic surfaces with strong adhesive force. Inorganic Chemistry, 47(8), 3140-3143. https://doi.org/10.1021/ic7021598
  10. Liu, H., Zhang, Q., Gu, C., Su, H., & Li, V. C. (2016). Influence of micro-cracking on the permeability of engineered cementitious composites. Cement and Concrete Composites, 72, 104-113. https://doi.org/10.1016/j.cemconcomp.2016.05.016
  11. Liu, S., Yang, J., Chen, X., Yang, G., & Cai, D. (2018). Application of mastic asphalt waterproofing layer in high-speed railway track in cold regions. Applied Sciences, 8(5), 667. https://doi.org/10.3390/app8050667
  12. Liu, K., & Jiang, L. (2012). Bio-inspired self-cleaning surfaces. Annual Review of Materials Research, 42, 231-263. https://doi.org/10.1146/annurev-matsci-070511-155046
  13. Ma, Z., Zhu, F., & Zhao, T. (2018). Effects of surface modification of silane coupling agent on the properties of concrete with freeze-thaw damage. KSCE Journal of Civil Engineering, 22(2), 657-669. https://doi.org/10.1007/s12205-017-1718-z
  14. Oltulu, M., & Sahin, R. (2014). Pore structure analysis of hardened cement mortars containing silica fume and different nano-powders. Construction and Building Materials, 53, 658-664. https://doi.org/10.1016/j.conbuildmat.2013.11.105
  15. Safiuddin, M., & Soudki, K. A. (2015). Water vapor transmission and waterproofing performance of concrete sealer and coating systems. Journal of Civil Engineering and Management, 21(7), 837-844. https://doi.org/10.3846/13923730.2014.893905
  16. Safiuddin, M. (2017). Concrete damage in field conditions and protective sealer and coating systems. Coatings, 7(7), 90. https://doi.org/10.3390/coatings7070090
  17. Soudki, K. A., Safiuddin, M., Jeffs, P., MacDonald, G., & Kroker, M. (2015). Chloride penetration resistance of concrete sealer and coating systems. Journal of Civil Engineering and Management, 21(4), 492-502. https://doi.org/10.3846/13923730.2014.890659
  18. Vazirinasab, E., Jafari, R., & Momen, G. (2018). Application of superhydrophobic coatings as a corrosion barrier: A review. Surface and Coatings Technology, 341, 40-56. https://doi.org/10.1016/j.surfcoat.2017.11.053
  19. Wang, L., & Li, S. (2014). Capillary absorption of concrete after mechanical loading. Magazine of Concrete Research, 66(8), 420-431. https://doi.org/10.1680/macr.13.00331
  20. Wang, W., Wang, S., Yao, D., Wang, X., Yu, X., & Zhang, Y. (2020). Fabrication of all-dimensional superhydrophobic mortar with enhanced waterproof ability and freeze-thaw resistance. Construction and Building Materials, 238, 117626. https://doi.org/10.1016/j.conbuildmat.2019.117626
  21. Wu, S., Cao, H., Yin, S., Zhang, X., & Chernow, V. (2009). Biomineralization and superhydrophobicity of BaCO3 complex nanostructures. Inorganic Chemistry, 48(21), 10326-10329. https://doi.org/10.1021/ic9014724
  22. Zheng, S., Li, C., Fu, Q., Li, M., Hu, W., Wang, Q., ... & Chen, Z. (2015). Fabrication of self-cleaning superhydrophobic surface on aluminum alloys with excellent corrosion resistance. Surface and Coatings Technology, 276, 341-348. https://doi.org/10.1016/j.surfcoat.2015.07.002