Shear bond strength analysis of non beryllium PFM metal with degassing and opaque firing techniques

도재용착용 Non beryllium 합금의 degassing과 opaque의 소성술식에 따른 결합강도 분석

  • Im, Joong-Jae (Department of Convergence Engineering, Graduate School of Venture, Hoseo University) ;
  • Lee, Sang-Houck (Department of Convergence Engineering, Graduate School of Venture, Hoseo University)
  • 임중재 (호서대학교 벤처대학원 융합공학과) ;
  • 이상혁 (호서대학교 벤처대학원 융합공학과)
  • Received : 2015.04.14
  • Accepted : 2015.07.16
  • Published : 2015.07.31

Abstract

This study is to compare the differences of bonding strength based on the Degassing temperatures and various opaque materials for Ni-Cr alloy specimen which does not contain beryllium(Be). Numerous comparison tests have been performed to measure the bonding strength by experimenting 3-point flexural rigidity tests in order to find out ways of stabilization and enhancement of bonding strength between metal and porcelain. AVOVA, surface component observation experiment by SAM/EDS, and Tukey's HSAD posteriori tests results are as follows: First, The bonding strength in all groups has exceeded the minimum (25MPa) of ISO9693 bonding strength regulation for dental mental-porcelain specimen. Second, The bonding strength of Group V1 was $32.37{\pm}1.91MPa$, $38.25{\pm}1.38MPa$ in Group V2, $46.43{\pm}2.14MPa$ in Group V3 and $47.21{\pm}1.72MPa$ Group V4. The difference has been statistically meaningful. Tukey's HSAD posteriori tests results have shown that the bonding strength in Group V4 was higher than that of Group V1. Third, the bonding strength between metal and porcelain without degassing process was higher than that of with degassing process, and the bonding strength of powder opaque was higher than that of paste opaque. Fourth, Group V4 has ranked the highest on the comparison table of metal and porcelain bonding strength.

본 연구는 베릴륨 함유하지 않은 Ni-Cr계 도재용 금속에 전용도재를 도포, 소성된 시편을 3점 굴곡 시험으로 결합강도를 측정하고, SAM/EDS로 표면성분관찰 실험한 AVOVA와 Tukey HSAD 사후검정을 실시한 결과는 다음과 같은 결론을 얻었다. 첫째. 모든 군에서 ISO 9693의 치과용 금속-도재 시편의 최소 결합강도의 최소치인 25 MPa의 전단결합강도를 상위하며 안정적인 결과값을 나타냈다. 둘째. 결합 강도는 대조군 V1은 $32.37{\pm}1.91MPa$으로 나타났고, 실험군 V2 $38.25{\pm}1.38MPa$, 실험군 V3 $46.43{\pm}2.14MPa$, 그리고 실험군 V4 $47.21{\pm}1.72MPa$, 순으로 나타났으며 통계적으로 유의한 차이를 보였다. 사후 검정 (Tukey's HSD test) 결과, 결합강도 실험결과 실험군 V4는, 대조군 V1보다 높게 나타났다. 셋째. 금속-도재의 결합에서 산화처리를 시행한 군보다 시행하지 않고 불투명 도재를 도포하고 소성한 군이 높게 나타났으며, paste불투명 도재보다 분말 불투명도재의 사용에 따른 결합강도가 더 높게 나타났다. 넷째. 실험군 V4는 금속과 도재의 결합강도 비교에서 가장 높게 나타났다.

Keywords

References

  1. Moffa JP."Alternative dental casting alloys. Dent Clin North Am", 27:733-46, 1983.
  2. Grimaudo NJ. "Biocompatibility of nickel and cobalt dental alloys". Gen Dent, 49, 498-503, 2001.
  3. Johnston JF, "Dykema RW, Cunningham DM. The use and construction of gold crowns with a fused porcelain veneer", A progress report. J, Prosthet Dent, 6:811-21, 1956. https://doi.org/10.1016/0022-3913(56)90078-6
  4. Brecker SC. "Porcelain baked to gold a new medium in prosthodontics", J Prosthet Dent, 6:801-10, 1956. https://doi.org/10.1016/0022-3913(56)90077-4
  5. Knap FJ, Ryge G. Study of bond strength of dental porcelain fused to metal. J Prosthet Dent 1966;45:1047-51.
  6. Shell JS, Nielsen JP. "Study of the bond between gold alloys and porcelain". J Dent Res 41:14 24-37, 1962. https://doi.org/10.1177/00220345620410062101
  7. Vickery RC, Badinell LA. "Nature of attachment forces in porcelain-gold systems", J Dent Res 47(5):638-698, 1968.
  8. Anusavice K J, Cascone P,Phillips' "Science of Dental Materials", 11th ed., pp. 563-620, 2003.
  9. Mackert, J R., Ringle, R. D., Parry, E. E.,Evans, A. Land Fairhurst, C. W. "The relationship between oxide adherence and porcelain-metal bonding", J. Dent. Res., 67, 474-478, 1988. https://doi.org/10.1177/00220345880670020801
  10. Carpenter, M.A. and Good kind, R.J, "Effect of varying surface texture on bond strength of one semiprecious and one non precious ceramo-alloy", J.P rosthet. Dent. 42:86-95, 1979. https://doi.org/10.1016/0022-3913(79)90334-2
  11. Jae-Kwan Jung, Shear bond strength analysis of PFM metal and zirconia with different surface condition. Journal of the Korea Academia-Industrial cooperation Society, vol 15, 7pp 4329-4335, 2014. https://doi.org/10.5762/KAIS.2014.15.7.4329
  12. Choi E K. "Bond strength between dental porcelains and bas metal alloys - Influence of Be element and repeated firing", Department of Oral Health Graduate School of Public Health and Dankook University, 2011.
  13. Johnston, J.F., Mumford, G.and Dykema, R.W., "Modern practice in dental ceramics", W.B. Saunders Co. p. 195, 1967.
  14. A. S. Al-Jabob, "Low-melting Ternary Titanium Casting Alloy", Ph. D. Dissertation at Northwestern University, Chicago, 1992.