DOI QR코드

DOI QR Code

Study on Improvement of Corrosion Resistance and Wear Resistance by Anodizing and Sealing Treatment with Nano-diamond Powder on aluminum

알루미늄의 아노다이징과 나노 다이아몬드 분말 봉공처리에 의한 내식성과 내마모성 향상에 관한 연구

  • Kang, Soo Young (Dept. of Metallurgical & Material Engineering, Inha Technical College) ;
  • Lee, Dae Won (School of materials science and engineering, Inha University)
  • 강수영 (인하공업전문대학 금속재료과) ;
  • 이대원 (인하대학교 신소재공학부)
  • Received : 2014.06.10
  • Accepted : 2014.06.22
  • Published : 2014.06.30

Abstract

In this study, in order to improve corrosion resistance and wear resistance of aluminum, surface treatment was made by anodizing with oxalic acid solution and sealing with nano-diamond powder. Average size of nano-diamond powder was 30nm. Anodizing with oxalic acid made many pores in the aluminum oxide layer. Pore size and oxide thickness were investigated by scanning electron microscope (SEM). Pore size increased as temperature increased and voltage increased. It was possible to make oxide layer with pore diameter more than 50 nm. Oxide thickness increased as temperature and voltage and treatment time increased. Oxide layer with above $10{\mu}m$ thickness was made. Aluminum oxide layer with many pores was sealed by water with nano-diamond powder. Surface morphology was investigated by SEM. After sealing treatment with nano-diamond powder, corrosion resistance, wear resistance and hardness increased.

Keywords

References

  1. J. Malbella, A. Hornillos, J. M. Snaz, J. Elecrochem. Soc., 125 (1978) 1950. https://doi.org/10.1149/1.2131334
  2. D. Good, J. Elecrochem. Soc., 144 (1997) 1965. https://doi.org/10.1149/1.1837730
  3. T. Matsuzaki, T. Yamazaki, Fujitsu Scientific and Technical Journal, 6 (1980) 45.
  4. J. Flis, L. Kowalczyk, J. Appl. Electrochem., 25 (1995) 501.
  5. K. Hebert, R. Alkire, J. Electrochem. Soc., 135 (1988) 2447. https://doi.org/10.1149/1.2095356
  6. N. A. Hampson, N. Jackson, B. N. Stirrup,Surf. Technol., 5 (1977) 277. https://doi.org/10.1016/0376-4583(77)90030-9
  7. S. M. Moon, S. I. Pyun, J. Corr. Sci. Soc. of Korea, 26 (1997) 498.
  8. F. Keller, M. S. Hunter, D. L. Robinson, J. Electrochem. Soc., 100 (1953) 411. https://doi.org/10.1149/1.2781142
  9. Z. Ashitaka, G. E. Thompson, P. Skeldon, G. C. Wood, K. Shimizu, J. Electrochem. Soc., 146 (1999) 1380. https://doi.org/10.1149/1.1391774
  10. I. Serbrennikova, P. Vanysek, V. I. Birss, Electrochim. Acta, 42 (1997) 146.
  11. L. Hao, R. R. Cheng, Metal Finishing, 20 (2000) 8.
  12. J. P. Hoar, J. Phys. Chem. Solid, 9 (1959) 97. https://doi.org/10.1016/0022-3697(59)90199-4
  13. S. Y. Kang, D. W. Lee, J. Kor. Powd. Metall. Inst., 21 (2014) 114. https://doi.org/10.4150/KPMI.2014.21.2.114

Cited by

  1. Effect of Current Density on Porous Film Formation in Two-Step Anodizing for Al Alloy vol.49, pp.2, 2016, https://doi.org/10.5695/JKISE.2016.49.2.125
  2. Convergent Study of Aluminum Anodizing Method on the Thermal Fatigue vol.7, pp.5, 2016, https://doi.org/10.15207/JKCS.2016.7.5.169
  3. The study on the quality characteristics factor of medium-sized orbit scroll vol.17, pp.9, 2016, https://doi.org/10.5762/KAIS.2016.17.9.718
  4. Convergent Study of Texture on the Mechanical Properties of Electrodeposits vol.7, pp.6, 2016, https://doi.org/10.15207/JKCS.2016.7.6.193
  5. Non-nickel-based sealing of anodic porous aluminum oxide in NaAlO 2 vol.310, 2017, https://doi.org/10.1016/j.surfcoat.2016.11.100