DOI QR코드

DOI QR Code

An Experimental Study on the Rheological Properties of the Combined Self-Compacting Concrete by Quality Variations

품질변동에 따른 병용계 자기충전 콘크리트의 유동특성에 관한 실험적 연구

  • Kwon, Yeong-Ho (Dept. of Architecture and Fire Service Administration, Dong Yang University)
  • 권영호 (동양대학교 건축소방행정학과)
  • Received : 2013.12.20
  • Accepted : 2014.02.17
  • Published : 2014.06.30

Abstract

The purpose of this study is to investigate experimentally the variation factors range having influence on the rheological properties of the combined self-compacting concrete according to materials quality, weighting error and site conditions. Two types cement (blast-furnace slag cement and belite cement), lime stone powder as binder and the optimum mix proportions in the preceded study are selected for this study. Also, variations for sensitivity test are as followings; (1) Concrete temperature 3 cases (2) Surface moisture of sand 5cases (3) Fineness modulus of sand 5cases (4) Specific surface of lime stone powder 3cases (5) Dosage of chemical admixture 5cases. Slump flow ($650{\pm}50mm$), 500 mm reaching time (($7{\pm}3sec$), V-type flowing time ($15{\pm}5sec$) and U-box height (min. 300 mm) are tested for sensitivity. As test results, the variations range for quality control are as followings. (1) Concrete temperature; $10{\sim}20^{\circ}C$(below $30^{\circ}C$) (2) Surface moisture of sand; $base{\pm}0.6%$ (3) Fineness modulus of sand; $2.6{\pm}0.2$ (4) Dosage of chemical admixture; $base{\pm}0.2%$ (5) Specific surface of lime stone powder $6000cm^2/g$. Compared with two types cement including based belite cement (binary type) and based slag cement (ternary type), the combined self-compacting concrete used belite cement type is most stable in the quality control because of high contents for lime stone powder and $C_2S$. It is to propose a control scheme of the combined self-compacting concrete in the actual construction work.

이 연구는 현장에서 사용하는 재료의 품질 및 계량오차, 현장조건 등에 따라 병용계 자기충전 콘크리트의 유동특성에 영향을 미치는 변동요인의 범위를 실험적으로 규명하기 위한 것이다. 병용계 자기충전 콘크리트의 재료는 벨라이트 시멘트와 석회석 미분말을 사용한 벨라이트계 및 슬래그 시멘트와 석회석 미분말을 사용한 슬래그계가 선정되었으며, 선행연구에서 제시된 최적배합 조건을 대상으로 하였다. 변동요인으로 (1) 콘크리트의 온도 3종류, (2) 잔골재의 표면수율 5종류, (3) 잔골재의 조립률 5종류, (4) 고성능AE감수제의 사용량 5종류, (5) 석회석 미분말의 분말도 3종류 등을 대상으로 민감도 시험을 실시하였다. 민감도 시험의 항목은 슬럼프 플로우, 500 mm 플로우 도달시간, V-깔대기 유하시간, U-box 충전성 높이를 대상으로 하였다. 실험 결과, (1) 콘크리트 온도는 $10{\sim}20^{\circ}C$ 범위, (2) 잔골재의 표면수율은 ${\pm}0.6%$ 범위, (3) 잔골재의 조립률 $2.6{\pm}0.2$ 범위, (4) 고성능AE감수제의 사용량은 ${\pm}0.2%$ 범위, (5) 석회석 미분말의 분말도는 $6000cm^2/g$ 범위에서 현장품질을 관리해야 한다. 벨라이트계 및 슬래그계에 따른 차이는 크지 않았지만, 석회석 미분말 및 $C_2S$ 함량이 높은 벨라이트계가 안정적인 경향을 나타내었다. 따라서 이러한 결과를 현장 시공현장에서 병용계 자기충전 콘크리트의 관리방안으로 제안하고자 한다.

Keywords

References

  1. Okamura, H. and Ouchi, M., "Self-Compacting Concrete, Development, Present and Future," Proceeding of the First International RILEM Symposium on Self Compacting Concrete, Sweden, Proc 7, 1999, pp. 3-14.
  2. Ozawa, K., Maekawa, K., and Okamura, H., "Development of the High Performance Concrete," Proceedings of the Japan Concrete Institute, Vol. 11, No. 1, 1989, pp. 699-704.
  3. Han, C. G., Kim, S. S., and Son, S. U., "Determination of Optimal Mixture Proportion of Segregation Reducing Type Superplasticizer for High Fluidity Concrete," Journal of the Korea Concrete Institute, Vol. 14, No. 3, 2002, pp. 275-282. https://doi.org/10.4334/JKCI.2002.14.3.275
  4. Choi, Y. W., Jeong, J. G., Kim, K. H., and Moon, D. J., "Flowability Properties of Combined High Flowing Self-Compacting Concrete to the Addition of Viscosity Agent," Proceedings of the Korea Concrete Institute, Vol. 20, No. 2, 2008, pp. 369-372. https://doi.org/10.4334/JKCI.2008.20.3.369
  5. Choi, Y. W., Jeon, J. Y., Kim, C. U., Jung, J. G., and Jung, W. Y., "Flowability Evaluation of Binary and Ternary Blended of Ultra Flowing Self-Compacting Concrete," Proceedings of the Korea Concrete Institute, Vol. 18, No. 2, 2006, pp. 485-488.
  6. Korea Gas Corporation, "The Report of Concrete Mix Design for Slurry Wall in Inchon LNG Terminal (TK-17, 18)," Obayashi Corporation Document No. 2C-C-SL-0005, 2000, pp. 1-40.
  7. Cho, J. D., Hong, S. H., Cho, B. Y., Jang, G. Y., and Han, C. G., "The Properties of High Flowing Concrete with the Kind and Content of Limestone Powder," Proceedings of the Korea Concrete Institute, Vol. 11, No. 2, 1999, pp. 267-270.
  8. Kwon, Y. H., "Optimum Mix Proportion and Characteristics of the Combined Self Compacting Concrete according to Cement Types," Journal of the Korea Concrete Institute, Vol. 21, No. 1, 2009, pp. 55-64. https://doi.org/10.4334/JKCI.2009.21.1.055
  9. Choi, Y. W., Kim, K. H., Park, S. J., and Jung, J. G., "High Fluidity Concrete," Magazine of the Korea Concrete Institute, Vol. 22, No. 1, 2010, pp. 45-47.
  10. Kim, J. G. and Choi, Y., "A Study on Rheological Property of Ultra-High Fluidity Concrete by Adding Viscosity Modifying Admixture," Proceedings of the Korea Concrete Institute, Vol. 19, No. 1, 2007, pp. 593-596.
  11. Korea Concrete Institute., Standard Specification for Concrete-Chapter 8 High Fluidity Concrete, 2009, pp. 111-118.
  12. JSCE, "A Task and State of the Report on the High Flowing Concrete," Japan Society of Civil Engineers, Concrete Engineering Series 15, December 1996, pp. 118-126.