The Surface Property and Shear Bonding Strength according to Composition of Ni-Cr alloy for Porcelain Fused to Metal Crown

도재용착주조관용 Ni-Cr계 합금의 조성에 따른 표면특성 및 전단결합강도 관찰

  • 김갑진 (부산가톨릭대학교 보건과학대학 치기공학과) ;
  • 정인성 (부산가톨릭대학교 보건과학대학 치기공학과) ;
  • 최성민 (부산가톨릭대학교 보건과학대학 치기공학과)
  • Received : 2013.04.25
  • Accepted : 2013.06.26
  • Published : 2013.07.01

Abstract

Purpose: This study was to observe surface property and bonding strength according to composition of Ni-Cr alloy for porcelain fused to metal crown. The two kinds of Ni-Cr alloy with different composition ratio of parent metal were observed general properties and chemical properties of each alloy surface and measured the shear bonding strength between ceramic and each alloys. The aim of study was to suggest the material for design of parent metal's composition ratio to development of alloy for porcelain fused to metal crown. Methods: The two kinds of alloy as test specimen was Ni(71wt.%)-Cr(12wt.%) and Ni(63wt.%)-Cr(23wt.%) alloy. The oxide on surface was observed by SEM and EDX. And the shear test was performed by MTS. Results: The surface property and oxide characteristic analysis of oxide layer, weight percentage of Element O within $Ni_{71}Cr_{12}$ alloy measured 12.74wt.%, but $Ni_{63}Cr_{23}$ alloy was measured 15.91wt.%. And the maximum shear bonding strength was measured 106.14MPa between $Ni_{71}Cr_{12}$ alloy and vintage halo (VV group). Conclusion: The surface property and oxide characteristic of $Ni_{71}Cr_{12}$ alloy was similar to $Ni_{63}Cr_{23}$ alloy. And VV group has the strongest shear bonding strength.

Keywords

References

  1. Ahn JS, Ko EK, Joo KJ. Comparlson of shear bond strength of ceramic fused to Ni-Cr and Co-Cr alloy by heat treatment. The journal of korean academy of dental technology, 33(3), 185-192, 2011.
  2. Azer SS, Ayash GM, Johnston WM, Khalil MF, Rosenstiel SF. Effect of esthetic core shades on the final color of IPS Empress all-ceramic crowns. J Prosthet Dent, 96, 397-401, 2006. https://doi.org/10.1016/j.prosdent.2006.09.020
  3. Baran GR. Oxidation kinetics of some Ni-Cr alloys. J Dent Res, 62, 51-55, 1983. https://doi.org/10.1177/00220345830620011101
  4. Chong IS, Kim CY. Shear bond strength and interfacial characterization of ceramic to Beryllium free Nonprecious alloys for porcelain fused to metal crown. The korea contents society, 10(11), 229-234, 2010. https://doi.org/10.5392/JKCA.2010.10.5.229
  5. Choi YJ, Yook JI, Chung MK. Cytotoxicity of dental cast base metal alloys on human oral keratinocytes. The journal of korean academy of prosthodontic society, 37(6), 717-729, 1999.
  6. Han CS, Chun GS. A cytotoxic study of dental casting gold alloy on normal human gingival fibroblast. The korean journal of oral and maxillofacial pathology, 29(4), 271-282, 2005.
  7. ISO 9693: Dental metal-ceramin restoration material, ISO.
  8. Jung KC, Handbook of industrial poisoning, shingwang, Inc., 1995
  9. Kim KW. Comparison of Shear Bond Strength of Ceramics Fused to Co-Cr and Ni-Cr Alloy for Porcelain Fused Metal Crown. Major of Dental Laboratory Science, Graduated School, Catholic University of Pusan, 2009.
  10. Kim MJ. The Influence of Bonding Agent and Veneer Ceramics on the Bond Strength of Metal-Ceramic Restorations. Major of Dental Laboratory Science, Graduated School, Catholic University of Pusan,, 2012.
  11. Kim CY. The effect of Nb on interfacial characteristics of Ni-Cr alloy for porcelain fused to metal crown,. Department of Biomedical Engineering, Graduate school Inje university, 2004.
  12. Kim HJ and Kim BS, The study on comparison evaluation of shear bond strength of Co-Cr base alloy using for porcelain fused metal. The journal of korean academy of dental technology, 32(3), 195-207, 2010.
  13. Naji A, Harmand MF. Study of the effect of the surface state on the cyctocompatability of a Co-Cr alloy using human osteoblasts and fibroblasts. J Biomed. Mater. Res., 24(7), 861-871, 1990.
  14. McLean JW. Dental ceramics proceedings of the first international symposium on ceramics. 467, 1973.
  15. Pisani-Proenca J, Erhardt MC, Valandro LF, Guitierrez-Aceves G, Bolanos-Carmona MV, Del Castillo-Salmeron R, Bottino MA. Influence of ceramic surface conditioning and resin cements onicrotensile bond strength to a glass ceramic. J Prosthet Dent. 94, 412-417, 2006.
  16. Yamamoto M, Metal-ceramics, Quintessence Pub. Co., Tokyo, 1985.