References
- Phoenix RD. Denture base materials. Dent Clin North Am 1996;40:113-20.
- Darbar UR, Huggett R, Harrison A. Denture fracture-a survey. Br Dent J 1994;176:342-5. https://doi.org/10.1038/sj.bdj.4808449
- Beyli MS, von Fraunhofer JA. An analysis of causes of fracture of acrylic resin dentures. J Prosthet Dent 1981;46:238-41. https://doi.org/10.1016/0022-3913(81)90206-7
- Rodford RA, Braden M. Further observations on high impact strength denture-base materials. Biomaterials 1992;13:726-8. https://doi.org/10.1016/0142-9612(92)90135-B
- Jagger DC, Jagger RG, Allen SM, Harrison A. An investigation into the transverse and impact strength of "high strength" denture base acrylic resins. J Oral Rehabil 2002;29:263-7. https://doi.org/10.1046/j.1365-2842.2002.00830.x
- Khan Z, von Fraunhofer JA, Razavi R. The staining characteristics, transverse strength, and microhardness of a visible light-cured denture base material. J Prosthet Dent 1987;57:384-6. https://doi.org/10.1016/0022-3913(87)90319-2
- Pfeiffer P, Rosenbauer EU. Residual methyl methacrylate monomer, water sorption, and water solubility of hypoallergenic denture base materials. J Prosthet Dent 2004;92:72-8. https://doi.org/10.1016/j.prosdent.2004.04.003
- Pfeiffer P, Rolleke C, Sherif L. Flexural strength and moduli of hypoallergenic denture base materials. J Prosthet Dent 2005;93:372-7. https://doi.org/10.1016/j.prosdent.2005.01.011
- Jagger DC, Alshumailin YR, Harrison A, Rees JS. The effect of the addition of poly (methyl methacrylate) fibres on the transverse strength of repaired heat-cured acrylic resin. J Oral Rehabil 2003;30:903-8. https://doi.org/10.1046/j.1365-2842.2003.01078.x
- Ali IL, Yunus N, Abu-Hassan MI. Hardness, flexural strength, and flexural modulus comparisons of three differently cured denture base systems. J Prosthodont 2008;17:545-9. https://doi.org/10.1111/j.1532-849X.2008.00357.x
- Memon MS, Yunus N, Razak AA. Some mechanical properties of a highly cross-linked, microwave-polymerized, injection-molded denture base polymer. Int J Prosthodont 2001;14:214-8.
- Vallittu PK. The effect of void space and polymerization time on transverse strength of acrylic-glass fibre composite. J Oral Rehabil 1995;22:257-61. https://doi.org/10.1111/j.1365-2842.1995.tb00083.x
- Ogle RE, Sorensen SE, Lewis EA. A new visible light-cured resin system applied to removable prosthodontics. J Prosthet Dent 1986;56:497-506. https://doi.org/10.1016/0022-3913(86)90397-5
- Fellman S. Visible light-cured denture base resin used in making dentures with conventional teeth. J Prosthet Dent 1989;62:356-9. https://doi.org/10.1016/0022-3913(89)90350-8
- Khan Z, Haeberle CB. One-appointment construction of an immediate transitional complete denture using visible light-cured resin. J Prosthet Dent 1992;68:500-2. https://doi.org/10.1016/0022-3913(92)90418-A
- Johnston EP, Nicholls JI, Smith DE. Flexure fatigue of 10 commonly used denture base resins. J Prosthet Dent 1981;46:478-83. https://doi.org/10.1016/0022-3913(81)90232-8
- Dixon DL, Breeding LC. The transverse strengths of three denture base resins reinforced with polyethylene fibers. J Prosthet Dent 1992;67:417-9. https://doi.org/10.1016/0022-3913(92)90261-8
- Machado C, Sanchez E, Azer SS, Uribe JM. Comparative study of the transverse strength of three denture base materials. J Dent 2007;35:930-3. https://doi.org/10.1016/j.jdent.2007.09.006
- Uzun G, Hersek N. Comparison of the fracture resistance of six denture base acrylic resins. J Biomater Appl 2002;17:19-29. https://doi.org/10.1177/0885328202017001597
- Diaz-Arnold AM, Vargas MA, Shaull KL, Laffoon JE, Qian F. Flexural and fatigue strengths of denture base resin. J Prosthet Dent 2008;100:47-51. https://doi.org/10.1016/S0022-3913(08)60136-5
Cited by
- Influence of Different Repair Acrylic Resin and Thermocycling on the Flexural Strength of Denture Base Resin vol.56, pp.2, 2011, https://doi.org/10.3390/medicina56020050
- Comparison of Mechanical Properties of PMMA Disks for Digitally Designed Dentures vol.13, pp.11, 2011, https://doi.org/10.3390/polym13111745