Synthesis and Luminescence Enhancement of Strontium Aluminate Green Phosphor via Spray Pyrolysis

분무열분해 공정을 이용하여 스트론튬 알루미네이트 녹색 형광체의 합성 및 발광 특성 개선

  • Kim, Mi Na (Department of Chemical Engineering, Kongju National University) ;
  • Jung, Kyeong Youl (Department of Chemical Engineering, Kongju National University)
  • 김미나 (공주대학교 화학공학부) ;
  • 정경열 (공주대학교 화학공학부)
  • Published : 2011.10.01

Abstract

$SrAl_2O_4:Eu$ green phosphor was prepared by spray pyrolysis and its luminescence properties were controlled by replacing the Al sites with boron and using organic modifier or drying control chemical additive. It was clear that the substitution of B into the Al sites was helpful to obtain pure monoclinic $SrAl_2O_4$ phase and greatly enhance the emission intensity. In terms of the emission intensity, the optimal content of boron was about 1 at% with respect to the aluminum element. The luminescence intensity of $Sr_{0.9}Al_{1.98}B_{0.02}O_4:Eu_{0.1}$ phosphor could be improved by the use of 0.2 M organic additives in the spray solution. Futhermore, using 0.5 M dimethylformamide(DMF) as a drying control chemical with organic additives made it possible to improve about 172% the emission intensity of $Sr_{0.9}Al_{1.98}B_{0.02}O_4:Eu_{0.1}$ phosphor. According to XRD analysis, the organic additive and DMF used enhanced the crystallinity without any change in the crystal phase. When used only the organic additive without DMF, the surface area of the prepared $Sr_{0.9}Al_{1.98}B_{0.02}O_4:Eu_{0.1}$ phosphor became enlarged. The use of DMF with the organic additive resulted in significant reduction in the surface area. It was concluded that the increase of the crystallinity as well as the reduction of surface area mainly contribute to the improvement in the luminescence intensity of $Sr_{0.9}Al_{1.98}B_{0.02}O_4:Eu_{0.1}$ phosphor prepared using DMF and organic additives.

분무열분해 공정을 이용하여 $SrAl_2O_4:Eu$ 녹색 형광체를 제조함에 있어 붕소의 치환, 유기첨가제 및 건조 조절제의 사용에 따른 발광 특성을 조사하였다. Al 자리에 붕소를 치환시켜 줌으로써 결정상은 순수해지고 발광강도는 크게 향상됨을 확인하였다. 휘도 측면에서 붕소의 함량은 약 1 at%로 하는 것이 가장 바람직하였다. 유기첨가제의 함량 변화에 따른 $Sr_{0.9}Al_{1.98}B_{0.02}O_4:Eu_{0.1}$ 형광체의 휘도 변화를 조사한 결과 0.2M을 사용했을 때 가장 높은 휘도를 얻었다. 유기첨가제와 함께 건조 조절제로 DMF 0.5M을 함께 사용함으로써 $Sr_{0.9}Al_{1.98}B_{0.02}O_4:Eu_{0.1}$ 형광체의 휘도는 약 172% 향상되었다. XRD 분석 결과에 의하면 사용한 유기첨가제와 DMF의 사용은 $Sr_{0.9}Al_{1.98}B_{0.02}O_4:Eu_{0.1}$ 형광체의 결정상 변화 없이 결정성을 크게 향상시켰다. 유기 첨가제만을 사용할 경우 형광체의 표면적은 커졌지만 DMF를 함께 사용함으로써 현저히 줄어들었다. 따라서 유기첨가제와 DMF를 동시에 사용하여 합성한 형광체의 휘도가 크게 향상된 것은 결정성 증가와 표면적 감소에 기인한 것이라고 결론지었다.

Keywords

References

  1. Kang, H. S., Park, S. B., Koo, H. Y. and Kang, Y. C., "The Photoluminescence Characteristics of $Ba_{2-x}Sr_{x}SiO_{4}:Eu^{2+}$ Phosphor Particles Prepared by Spray Pyrolysis," Korean Chem. Eng. Res. (HWAHAK KONGHAK), 44, 609-613(2006).
  2. Iwaya, M., Terao, S., Sano, T., Nakamura, R., Kamiyama, S., Amano, H. and Akasaki, I., "Suppression of Phase Separation of AlGaN During Lateral Growth and Fabrication of Hihg-efficiency UV-LED on Optimized AlGaN," J. Cryst. Growth, 237, 951-955(2002).
  3. Hu, Y., Zhuang, W., Ye, H., Wang, D., Zhang, S. and Huang, X., "A Novel Red Phosphor for White Light Emitting Diodes," J. Alloys Compd., 390, 226-229(2005). https://doi.org/10.1016/j.jallcom.2004.07.063
  4. Kim, J. S., Jeon, P. E., Choi, J. C. and Park, H. L., "Emission Color Variation of $M_{2}SiO_{4}:Eu^{2+}$(M=Ba, Sr, Ca) Phosphor for Lightemitting Diodes," Solid State Commun., 133, 187-190(2005). https://doi.org/10.1016/j.ssc.2004.10.017
  5. Jiang, L., Chang, C., Mao, D. and Feng, C., "Concentration Quenching of $Eu^{2+}$ in $Ca_{2}MgSi_{2}O_{7}:Eu^{2+}$ Phosphor," Mater. Sci. Eng., B, 103, 271-275(2003). https://doi.org/10.1016/S0921-5107(03)00261-7
  6. Zhang, X. and Liu, X., "Luminescence Properties and Energy Transfer of $Eu^{2+}$ Doped $Ca_{8}Mg(SiO_{4})_{4}Cl_{2}$ Phosphors," J. Electrochem. Soc., 139, 622-625(1992). https://doi.org/10.1149/1.2069268
  7. Tang, Z., Zhang, F., Zhang, Z., Huang, C. and Lin, Y., "Luminescent Properties of $SrAl_{2}O_{4}$: Eu, Dy Material Prepared by the Gel Method," J. Eur. Ceram. Soc., 20, 2129-2132(2000). https://doi.org/10.1016/S0955-2219(00)00092-3
  8. Kim, J.-S., "Synthesis of the Nano-sized $SrAl_{2}O_{4}$ Phosphors by Wet Processing and its Photoluminescence Properties," J. Korean Ceram. Soc., 45, 477-481(2008). https://doi.org/10.4191/KCERS.2008.45.8.477
  9. Yoshida, H., Fujino, S. and Kajiwara, T., "Afterglow Luminance Property of Phosphorescent Phosphor $SrAl_{2}O_{4}:Eu^{2+}$, $Dy^{3+}$-glass Composites," J. Ceram. Soc. Jpn., 118, 784-787(2010). https://doi.org/10.2109/jcersj2.118.784
  10. Clabau, F., Rocquefelte, X., Jobic, S., Deniard, P., Whangbo, M.-H., Garcia, A. and Mercier, T., "On the Phosphorescence Mechanism in $SrAl_{2}O_{4}:Eu^{2+}$ and Its Codoped Derivatives," Solid State Sci., 9, 608-612(2007). https://doi.org/10.1016/j.solidstatesciences.2007.03.020
  11. Kang, Y. C., Jung, K. Y. and Park, S. B., "Preparation of Fluorescence Particles by Spray Pyrolysis," Korean Chem. Eng. Res. (HWAHAK KONGHAK), 44, 235-242(2006).
  12. Lee, S.-H., Yi, J. H., Kim, J. H., Ko, Y. N. and Kang, Y. C., "Characteristics of $Eu^{2+}$-doped Ca-$\alpha$-SiAlON Phosphor Powders Prepared by Spray Pyrolysis," Opt. Mater., 33, 538-542(2011). https://doi.org/10.1016/j.optmat.2010.10.051
  13. Jung, K. Y. and Jung, H.-K., "Luminescence Optimization of Eudoped $LnAl_{3}(BO_{3})_{4}$(Ln=Y,Gd) Red Phosphor Using Spray Pyrolysis," J. Lumin., 130, 1970-1974(2010). https://doi.org/10.1016/j.jlumin.2010.05.014
  14. Park, K., Nam, S. W. and Heo, M. H., "VUV Photoluminescence Properties of $Y_{1-x}Gd_{x}VO_{4}$:Eu Phosphors Prepared by Ultrasonic Spray Pyrolysis," Ceram. Int., 36, 1541-1544(2010). https://doi.org/10.1016/j.ceramint.2010.02.019
  15. Clabau, F., Rocquefelte, X., Jobic, S., Deniard, P., Whangbo, M.-H., Garcia, A. and Mercier, T., "Mechanism of Phosphorescence Appropriate for the Long-Lasting Phosphors $Eu^{2+}$-doped $SrAl_{2}O_{4}$ with Codopants $Dy^{3+}$ and $B^{3+}$," Chem. Mater., 17, 3904-3912(2005). https://doi.org/10.1021/cm050763r
  16. Singh, V., Rao, T. K. and Zhu, J.-J., "Preparation, Luminescence and Defect Studies of $Eu^{2+}$-activated Strontium Hexa-aluminate Phosphor Prepared via Combustion Method," J. Solid State Chem., 179, 2589-2594(2006). https://doi.org/10.1016/j.jssc.2006.04.053
  17. Jung, K. Y. and Han, K. H., "Densification and Photoluminescence Improvement of $Y_{2}O_{3}$ Phosphor Particles Prepared by Spray Pyrolysis," Electrochem. Solid-State Lett., 8, H17-H20(2005). https://doi.org/10.1149/1.1849111

Cited by

  1. Phosphors by Solid State Reaction and Its Luminescent Properties vol.23, pp.12, 2013, https://doi.org/10.3740/MRSK.2013.23.12.727
  2. Green Phosphor Prepared by Spray Pyrolysis vol.53, pp.5, 2015, https://doi.org/10.9713/kcer.2015.53.5.620
  3. long afterglow phosphors synthesized solid state reaction and polymerized complex method vol.26, pp.5, 2016, https://doi.org/10.6111/JKCGCT.2016.26.5.193
  4. SrAl2O4: Eu2+, Dy3+ 축광안료의 고온안정성에 관한 연구 vol.51, pp.6, 2011, https://doi.org/10.4191/kcers.2014.51.6.618