구상흑연주철재의 화상해석에 의한 흑연의 극치통계 평가

Evaluation of Statistical distribution of extreme values of Graphite in Ductile Cast Iron by Image Analyzer

  • 윤명진 (경일대학교 기계자동차학부)
  • 투고 : 2010.10.25
  • 심사 : 2010.12.02
  • 발행 : 2010.12.31

초록

Although the problems of defects and nonmetallic inclusion in metal fatigue are very complicated, it is particularly important to view these problems from the perspective that defects and inclusions are virtually equivalent to small cracks. This concept will help one to understand various fatigue phenomena caused by Ductile Cast Iron. For different ferrite-pearlite matrix structure, containing more than 90% spheroidal ratio of graphite, GCD 45-3, GCD 50, GCD 60 series and 70%, 80%, 90% spheroidal ratio of graphite, GCD 40, GCD 45-1, GCD 45-2 series, this paper has carried out image analyzer, estimated maximum and mean size of graphite, investigated correlation. It was concluded as follows. (1) A good quality of Ductile cast iron using in this experiment, the graphite was separated well. The effect of the interaction by graphite was verified by microscopic observation and by fracture mechanics investigation in surface, interior of the specimen. (2)${\sqrt{area}}_{max}$ of graphite can be used to predict fatigue limit of Ductile Cast Iron. The Statistical distribution of extreme values of ${\sqrt{area}}$ may be used as a guide line for the control of inclusion size in the steel making processes.

키워드

참고문헌

  1. 윤명진, "저탄소강의 표면결함의 영향에 의한 피로강도의 정량적 평가", 한국공작기계기술학회지, 제 4 권, 제 4 호, pp. 42-49, 1995.
  2. 윤명진, "중탄소강의 피로크랙 개폐구의 특성 및 피로강도의 평가", 한국공작기계기술학회지, 제 6 권, 제 1 호, pp. 45-50, 1997.
  3. 村上敬宣, 淸水眞佐男, "疲勞强度に及ぼす介在物, 微小缺陷, 微小き裂の影響", 日本機械學會論文集, 第 54卷, 第 499 號, pp. 413-425, 1988.
  4. Smith R. A., Short Fatigue Cracks, Fatigue Mechanisms: Advances in Quantitative Measurement of Physical Damage, ASTM STP 811, J. Lankford, D. L. Davidson, W. L. Morris, and R. P. Wei, Eds., American Society for Testing and Materials, pp. 264-279, 1983.
  5. Masahiro Endo, Yukitaka Murakami, Effects of an Artificial Small Defect on Torsional Fatigue Strength of Steels, ASME. Vol. 109, pp. 124-129, 1987.
  6. Yukitaka Murakami, M. Endo, Effects of Defects, inclusions and inhomogeneities on Fatigue Strength, Fatigue, Vol. 16, pp. 163-182, 1994. https://doi.org/10.1016/0142-1123(94)90001-9
  7. Yukitaka Murakami, Effects of Small Defects and Nonmetallic Inclusions on The Fatigue Strength of Metals, JSME. Vol. 32, No. 2, pp. 167-180, 1989.
  8. Y. Muraksmi, Inclusion Rating by Statistics of Extreme Values and Its Application to Fatigue Strength Prediction and Quality Control of Materials, J. Res. Natl. Inst. Stand. Technol. Vol. 99, pp. 345-351, 1994. https://doi.org/10.6028/jres.099.032
  9. Y. Murakami and S. Nemat-Nasser, Growth and Stability Of Interacting Surface Flaws Of Arbitrary Shape, EFM. Vol. 17, No .3-A, pp. 193-210, 1983.
  10. Murakami Y., Endo M., Effects of Hardness and Crack Geometries on ΔKth of Small Cracks Emanating from Small Defects, The Behaviour of Short Fatigue Cracks, EGF Pub. 1 (Edited by K. J. Miller and E. R. de los Rios), pp. 275-293, 1986.
  11. 遠藤正浩, 王羽兵, "最近の球狀黑鉛鑄鐵の疲勞强度におよぼす黑鉛と人工微小缺陷の影響", 材料, Vol. 43, No. 493, pp. 1245-1250, 1994.
  12. 西谷弘信外 3人, "球狀黑鉛鑄鐵切缺材の疲勞强度", 日本機械學會論文集 第 58 卷, 第 556 號, pp. 2280-2286, 1992.
  13. 윤명진, 이경모, 구상흑연 주철재의 피로 크랙 발생 및 피로강도에 미치는 기지조직의 영향, 한국공작기계학회지, 제 7 권, 제 5 호, pp. 66-71, 1998.
  14. 김민건, 김진학, 오스템퍼링처리한 구상흑연 주철의 피로한도에 미치는 기지조직인자와 역학인자의 영향, 대한기계학회논문집(A권), 제 23 권, 제 2 호, pp. 287-293, 1999.
  15. 지정근, 김민건, 김진학, 김정두, 초급속열처리 구상흑연 주철 FCD500의 피로파괴 특성, 대한기계학회논문집(A권), 제 26 권, 제 4 호, pp. 596-601, 2002.