Abstract

Surface treatments act as a barrier between the environment and the concrete, preventing or retarding the entry of harmful substances and cutting off the transportation path into concrete. The effectiveness of a surface protection preventing the permeation depends on how close and strongly connected are the resin molecules. This work intends to contribute to a better understanding of the performance of protected concrete in chemically aggressive environments, by presenting results of ion diffusion and resistance to aggressive solutions of several hydrophobic agents and coatings used to protect concrete. Three different types of surface protections were tested: silicone hydrophobic agent, acrylic and epoxy coatings. The obtained results indicate that the overall performance of epoxy resin was better than the other selected types of protections.

Keywords

References

  1. Rodrigues, M. P., Costa, M. R. N., Mendes, A. M., and Marques, M. I. E., "Effectiveness of Surface Coatings to Protect Reinforced Concrete in Marine Environments," Materials and Structures, Vol. 33, 2000, pp. 618-626 https://doi.org/10.1007/BF02480601
  2. Swamy, R. N., Suryavanshi, A. K., and Tanikawa, S., "Protective Ability of an Acrylic-Based Surface Coating System against Chloride and Carbonation Penetration into Concrete," ACI Materials Journal, 1998, pp. 101-112
  3. Kreijger, P. C., "The Skin of Concrete, Composition and Properties," Materials and. Structures, Vol. 17, 1984, pp. 275-283 https://doi.org/10.1007/BF02479083
  4. Pfeifer, D. W. and Scali, M. J., Concrete Sealers for Protection of Bridge Structures, Department of Transportation, NCHRP 244, Washington D.C., 1981, 138 pp
  5. CEN, European Committee for Standardization, Products and Systems for the Protection and Repair of Concrete Structures. Definitions, Requirements, Quality Control and Evaluation of Conformity. Part 2: Surface protection systems for concrete, EN 1504-2, Brussels, Belgium, 2004
  6. Swamy, R. N. and Tanikawa, S., "Surface Coatings to Preserve Concrete Durability," Proceedings of International Conference on Protection of Concrete, Edited by R. K. Dhir and J. W. Green, E & FN Spon, London, 1990, pp. 149-165
  7. Hawkins, P. J., "The Use of Surface Coatings to Minimize Carbonation in the Middle East," Proceedings of 1st International Conference on Deterioration and Repair of Reinforced Concrete in the Arabian Gulf, Bahrain, 1985, pp. 273-285
  8. Almusallam, A., Khan, F. M., and Maslehuddin, M., "Performance of Concrete Coatings under Varying Exposure Conditions," Materials and Structures, Vol. 35, 2002, pp. 487-494 https://doi.org/10.1007/BF02483136
  9. Moreira, P. M., Aguiar, J. B., and Camoes, A., "Systems for Superficial Protection of Concretes," Proceedings of the International Symposium Polymers in Concrete, University of Minho, Guimaraes, Portugal, 2006, pp. 225-236
  10. Luping, T., Chloride Transport in Concrete, Measurement and Prediction, Doctoral Thesis, Chalmers University of Technology, Gotemborg, Sweden, 1996
  11. ASTM, American Society for Testing and Materials, Standard Test Method for Soundness of Aggregates by Use of Sodium Sulfate or Magnesium Sulfate, C 88, West Conshohocken, USA,1999
  12. CEN, European Committee for Standardization, Products and Systems for the Protection and Repair of Concrete Structures. Test Methods. Resistance to Severe Chemical Attack, EN 13529, Brussels, Belgium, 2003
  13. CEN, European Committee for Standardization, Products and Systems for the Protection and Repair of Concrete Structures. Test Methods. Reference Concretes for Testing, EN 1766, Brussels, Belgium, 2000
  14. ISO, International Organization for Standardization, Paints and Varnishes. Evaluation of Degradation of Coatings. Designation of Quantity and Size of Defects, and of Intensity of Uniform Changes in Appearance. Part 2: Assessment of Degree of Blistering, ISO 4628-2, Geneva, Switzerland, 2003
  15. ISO, International Organization for Standardization, Paints and Varnishes. Evaluation of Degradation of Coatings. Designation of Quantity and Size of Defects, and of Intensity of Uniform Changes in Appearance. Part 4: Assessment of Degree of Cracking, ISO 4628-4, Geneva, Switzerland, 2003
  16. ISO, International Organization for Standardization, Paints and Varnishes. Evaluation of Degradation of Coatings. Designation of Quantity and Size of Defects, and of Intensity of Uniform Changes in Appearance. Part 5: Assessment of Degree of Flaking, ISO 4628-5, Geneva, Switzerland, 2003
  17. ISO, International Organization for Standardization, Paints and Varnishes. Evaluation of Degradation of Paint Coatings. Designation of Intensity, Quantity and Size of Common Types of Defects. Part 6: Rating of Degree of Chalking by Tape Method, ISO 4628-6, Geneva, Switzerland, 1990
  18. ASTM, American Society for Testing and Materials, Standard Test Method for Pull-off Strength of Coatings Using Portable Adhesion testers, D 4541, West Conshohocken, USA, 2002
  19. Almusallam, A., Khan, F. M., and Maslehuddin, M., "Performance of Concrete Coatings under Varying Exposure Conditions," Materials and Structures, Vol. 35, 2002, pp. 487-494 https://doi.org/10.1007/BF02483136

Cited by

  1. Making solutions for choosing industrial concrete floors and expedience of reliability evaluation vol.16, pp.3, 2010, https://doi.org/10.3846/jcem.2010.37
  2. Analysis of inhibition of concrete steel-rebar corrosion by Na2Cr2O7 concentrations: Implications for conflicting reports on inhibitor effectiveness vol.20, pp.12, 2013, https://doi.org/10.1007/s11771-013-1898-8