Glass-ceramics were fabricated by heat-treating a glass at $700^{\circ}C$/10hr which was obtained by melting a glass frit mixed with $40{\sim}80 wt%$ EAF dust at $1300^{\circ}C$/1hr. Dependence of crystal phase and bonding state change upon a compositional change and heat treatment condition were studied and the results was connected to the toxic characterization leaching procedure (TCLP) test data to investigate a chemical durability of the specimens. Increasing dust in a glass shifted the peak around $1000cm^{-1}$ to the lower frequency which was composed of two vibration peaks for the nonbridging oxygen at $960cm^{-1}$ and the bridging oxygen at $1050{\sim}1060cm^{-1}$. Also, the $B_2O_3$ structure of boroxol ring changed to a tetrhedral-, trigonal- and di-borate with dust addition. The Fe-O peaks in the glass-ceramics were observed which is consitent with XRD results of spinel formation. The surface of glass after TCLP test was severely cracked while there was no cracks on a glass-ceramics after TCLP test so the chemical durability of the glass-ceramics is superior than that of glass. The leaching concentration of Fe for the glass-ceramics containing EAF dust 80 wt% is 1/15 times lower than that of glass. The Zn leaching concentration fur the glass-ceramics containing dust < 70 wt% was higher than that of glass but its trend was reversed for the specimen of dust content > 80 wt% which could be concluded as correlated with occurrence of willemite phase.

붕규산염계 유리에 EAF Dust를 $40{\sim}80wt%$ 첨가하고 후 용융하여 유리를 제조한 후 $700^{\circ}C$/10hr으로 열처리하여 결정화유리 시편을 합성하였다. FT-IR, SEM, 그리고 EDS 분석을 통하여 조성 및 열처리 조건에 따른 시편내 결정상 및 결합상태 변화를 관찰하고, 이를 TCLP(Toxic Characterization Leaching Procedure) 실험에서 얻은 결과와 연계시켜 시편의 화학적 내구성을 연구하였다. 유리에 더스트 첨가량이 증가함에 따라 FT-IR 스펙트럼 상의 가교산소 진동피크($1050{\sim}1060cm^{-1}$)와 비가교산소 진동피크($960cm^{-1}$)가 합쳐진 넓은 피크($1000cm^{-1}$ 부근)가 저파수쪽으로 이동하였다. 동시에 boroxol ring의 $B_2O_3$ 구조가 tetrhedral-, trigonal- 그리고 di-borate로 변화되는 것을 확인하였다. 결정화유리 시편에서 Fe-O 피크가 확인되었으며 이는 spinel이 생성되었다는 XRD 결과와 일치하였다. TCLP를 행한 유리시편의 표면은 균열이 심하였으나 결정화유리는 큰 변화가 없어, 결정상 생성이 화학적 내구성을 향상시킴을 확인하였다. Fe의 용출량은 더스트가 80wt% 첨가된 결정화유리의 경우, 유리시편에 비하여 1/15로 감소하였다. Zn은 더스트 첨가량이 70wt% 이하인 결정화유리에서 용출량이 유리에 비해 높았으나 80wt% 이상 시편에서는 유리보다 감소하였고 이는 willemite 생성과 연관이 있는 것으로 사료된다.

Keywords

References

  1. T.W. Cheng, J.P. Chu, C.C. Tzeng and Y.S. Chen, 'Treatment and recycling of incinerated ash using thermal plasma technology', Waste Management 22 (2002) 485 https://doi.org/10.1016/S0956-053X(01)00043-5
  2. F.P. Glasser, 'Properties of cement waste composites', Waste Management 16 (1996) 159 https://doi.org/10.1016/S0956-053X(96)00059-1
  3. T.H. Um, Y.T Kim, K.G Lee, Y.J. Kim, S.G. Kang and J.H. Kim, 'Properties of heavy metal adsorption of clay minerals', J. Kor. Ceram. Soc. 39(7) (2002) 663 https://doi.org/10.4191/KCERS.2002.39.7.663
  4. T.C. Son, 'Recycling and soluble problem of EAF dust', Environment VIP Report 33 (1998) 1
  5. J.M. Rincon, M. Romero and A. R. Boccaccini, 'Micro-structural characterization of a glass and glass-ceramic obtained from municipal incinerator fly ash', J. Mater. Sci. 34 (1999) 4413 https://doi.org/10.1023/A:1004620818001
  6. T.W. Cheng, 'Effect of additional materials on the properties of glass-ceramic produced from incinerator fly ashes', Chemosphere 56 (2004) 127 https://doi.org/10.1016/j.chemosphere.2004.02.009
  7. T.W. Cheng and Y.S. Chen, 'On formation of CaO$Al_{2}O_{3}-SiO _{2}$ glass-ceramics by vitrification of incinerator fly ash', Chemosphere 51 (2003) 817 https://doi.org/10.1016/S0045-6535(03)00189-9
  8. Y.S. Ahn, S.G. Kang, Y.T Kim, G.K. Lee and J.H. Kim, 'Microstructure of borosilicate glass-ceramics containing EAF dust', J. Kor. Cryst. Growth and Cryst. Tech. 16(2) (2006)82
  9. H.T. Eun, S.G. Kang, Y.T Kim, G.G. Lee and J.H. Kim, 'Stabilization of heavy metals in glasses containing EAF Dust', Journal of the Korean Ceramic Society 41(11) (2004) 851 https://doi.org/10.4191/KCERS.2004.41.11.851
  10. H.S. Kim, S.G. Kang, Y.T Kim, G.G. Lee and J.H. Kim, 'Heavy metal leaching characteristics of silicate glass containing EAF dust', Journal of the Korean Ceramic Society 43 (2006) 136 https://doi.org/10.4191/KCERS.2006.43.2.136
  11. US Environmental Protection Agency, Toxicity Charac-terization Leaching Procedure (TCLP), 40 CFR 268, Appendix, US Federal Register
  12. Y.l. Jialing, 'Further studies on the IR spectra of silicate glasses', J. Non-Cryst. Solids 84 (1986) 114 https://doi.org/10.1016/0022-3093(86)90768-4
  13. C.M. Whang, J. Lee and l.K. Bae, 'Structural analysis of $Na_{2}O-Ga_{2}O_{3}-SiO_{2}$ system glasses by FT-IR and raman spectroscopy', J. Korean Ceram. Soc. 25(1) (1988) 27
  14. G.H. Lim, C.M. Whang and C.Y Kim, 'Investigation on structural and physical properties of bioglasses with various $P_{2}O_{5}$ content', J. Korean Ceram. Soc. 27(4) (1989) 559
  15. S.M. Abo-Naf, F.H. El Batal and M.A. Azooz, 'Characterization of some glasses in the system $SiO{2}$, $Na_{2}O.RO$ by infrared spectroscopy', Materials Chemistry and Physics 77 (2002) 846 https://doi.org/10.1016/S0254-0584(02)00215-8
  16. Y. Masauki, 'Glasses', Translated to Korean by W.H. Kang, et al., Chungmoongak, Korea (2002) 34
  17. E. Bright Wilson, Jr. 'Hanbook of Chemistry and Physics 74th Edition', CRC Press, USA (1993) 4112,113,137,140