A Study on Numerical Analysis and Wall Thinning Effect in Accordance with the Eddy Current of MFIV Lower Body

주급수격리밸브 하부몸체의 와류현상에 따른 감육영향 및 수치해석 연구

  • 황경모 (한국전력기술(주)) ;
  • 진태은 (한국전력기술(주) 재료기술연구그룹) ;
  • 김경훈 (경희대학교 기계공학과)
  • Published : 2006.07.01

Abstract

A numerical analysis study has performed in terms of fluid dynamics to identify the wall thinning generated in the main feedwater isolation valve body of a nuclear power plant. To review the relations between flow characteristics and the wall thinning induced by flow accelerated corrosion (FAC), numerical analysis using FLUENT code and ultrasonic tests (UT) were performed. The local velocities according to the analysis results were compared with the distribution of the measured wall thickness by ultrasonic tests. The comparison results show that the local velocity in the x-direction had no correlation with the wall thinning but the local velocity in the y-direction and turbulence intensity had a great influence on that. These results provide a good match to those of the previous studies - locations colliding vertically against components undergo severe wall thinning. These results may be utilized to the design modification and the wall thinning management for main feedwater isolation valves for preventing the wall thinning degradation.

Keywords

References

  1. Stirzel, C. W., LaPay, W. S. and Kim, C. C., 1997, 'Aging Management Evaluation for Class 2, 3, and Nonsafety Class Valve Bodies, Pump Casings, Piping and Supports, and Ductwork,' Westinghouse, WCAP-14612, Rev.0, pp. 3-9-11
  2. NRC, 2000, 'Generic Aging Lessons Learned (GALL) Report,' NUREG-1801, Office of Nuclear Reactor Regulation
  3. BGE, 1998, 'CCNPP License Renewal Application,' TR-111031-CD
  4. Oconee, 1998, 'Application for Renewed Operating Licenses for Oconee Nuclear Station,' Units 1, 2, and 3
  5. FPL, 2000, 'Application for Renewed Operating Licenses,' Turkey Point Units 3&4
  6. KHNP, 2000, Technical Review Report for Thickness Verification of Feedwater Heater Shell Side of Kori Unit 1, Mechanical Department, Kori First Plant
  7. Keller, H., 1978, 'Corrosion and Erosion Problems in Saturated Steam Turbines,' AIM Conf., Liege, Belgium, pp. 22-28
  8. Bignold, G. J., et aI., 1981, 'Proc. 8th Intern. Congress Metallic Corrosion,' DECHEMA, West Germany, Vol. 2, p. 1548
  9. Dillon, C. P., 1986, 'Corrosion Control in the Chemical Process Industries,' McGraw-Hill, Inc
  10. ASME, 2004, 'Class 2 Components,' Valve Design NC-3500, pp. 121-129

Cited by

  1. Structural Integrity Evaluation of Large Main Steam Piping by Water Hammering vol.36, pp.9, 2012, https://doi.org/10.3795/KSME-A.2012.36.9.1103