Effects of plasma arc curing lights on the surface hardness of the composite resins

플라즈마 광중합기가 복합레진 중합에 미치는 영향

  • Lee, Soo-Won (Department of Pediatric Dentistry, College of Dentistry, Chonnam National University and Dental Research Institute) ;
  • Yang, Kyu-Ho (Department of Pediatric Dentistry, College of Dentistry, Chonnam National University and Dental Research Institute) ;
  • Kim, Seon-Mi (Department of Pediatric Dentistry, College of Dentistry, Chonnam National University and Dental Research Institute) ;
  • Choi, Nam-Ki (Department of Pediatric Dentistry, College of Dentistry, Chonnam National University and Dental Research Institute)
  • 이수원 (전남대학교 치과대학 소아치과학교실 및 치의학 연구소) ;
  • 양규호 (전남대학교 치과대학 소아치과학교실 및 치의학 연구소) ;
  • 김선미 (전남대학교 치과대학 소아치과학교실 및 치의학 연구소) ;
  • 최남기 (전남대학교 치과대학 소아치과학교실 및 치의학 연구소)
  • Published : 2006.11.30

Abstract

In recent years, xenon plasma arc lamp was introduced for high-intensity curing of composite filling materials in direct resin restorations. In this study, two types of restorative materials, namely composites point $4^{(R)}$ and $Z250^{(R)}$ were selected and curing was conducted using a conventional halogen light and two plama curing lights. Two different resin composites were cured using the different units($Flipo^{(R)}$, Ultra-lite 180A, and $TriLight^{(R)}$) and tested for microhardness. The purpose of this study was to test the hypothesis that exposure to a plasma curing lamp for 3, 6. 9 seconds is equivalent to 20 or 40 seconds of irradiation using a conventional halogen curing unit. 1. $Flipo^{(R)}$ and Ultra-lite 180A were able to polymerize point $4^{(R)}$ at 6 seconds to a degree equal to that of the $TriLight^{(R)}$(control) at 40 seconds. 2. $Flipo^{(R)}$ was able to polymerize $Z250^{(R)}$ at 9 seconds to a degree equal to that of the $TriLight^{(R)}$(control) on the bottom surface at 20 seconds. whereas Ultra-lite 180A could not do. 3. Two plasma curing units were able to cure the test-composites with bottom/top ratios approximately 61% to 96% at 3 to 9 seconds. There were some differences between the two composite brands, with $Z250^{(R)}$ displaying less difference between top and bottom hardness values. For point $4^{(R)}$ and $Z250^{(R)}$, at least 6 or 9 seconds were necessary to produce microhardness equivalent to that of the $TriLight^{(R)}$ curing at 20 or 40 seconds.

기존에 사용하고 있는 할로겐 광중합기는 여러 가지 장점에도 불구하고 중합시간이 오래 걸린다는 문제 때문에 시술시간이 길어지는 단점이 있는데, 최근에 개발된 플라즈마 광중합기는 매우 짧은 시간에 중합시킬 수 있다고 제조회사는 주장하고 있다. 본 연구에서는 임상에서 흔히 상용하고 있는 복합 레진을 광중합 할 때, 할로겐 광중합으로 얻을 수 있는 플라즈마 광중합기의 적절한 중합시간을 알아보고자 한다. 2mm 두께의 레진 샘플을 만들어 광중합 하고 24 시간 후 상, 하면의 미세경도를 측정하였다. point $4^{(R)}$에서는 플라즈마 광중합기로 6초간 중합했을 때 할로겐과 유사한 경도를 얻었지만, $Z250^{(R)}$에서는 $Flipo^{(R)}$만 9초간 중합시 할로겐과 유사한 광중합을 나타냈다. 이번 연구에서 사용한 플라즈마 광중합기는 적어도 6초 혹은 9초정도 광중합 했을 때 할로겐과 유사한 중합을 얻을 수 있다는 것을 알 수 있었다.