초록
Conditions for formation of perovskite Pb(Zr$_{0.52}$Ti$_{0.48}$)O$_{3}$ phase by the hydrothermal synthesis are investigated. Pb(Zr$_{0.52}$ Ti$_{0.48}$)O$_{3}$ ceramics were synthesized by hydrothermal process above 180$^{\circ}C$ for 2 h reaction using 5$\~$30 M KOH solution as a mineralizer. Particle size increases in proportion to the mineralizer concentration. As a result of EOX analysis, PZT powders synthesized using 50 M of KOH as a mineralizer were considered as 2.42 mol$\%$ K doped-PZT powders. And 2.42 mol$\%$ K doped-PZT has much higher mechanical quality factor than undoped PZT ceramics. The sintering properties showed 7.987 g/cm$^{3}$ of sintered density and 3$\~$4 $\mu$m of grain size.