Abstract

In continuous galvanizing process, the mass of zinc deposited and its distribution are controlled by the air pressure, effective distance from the air knife nozzle to the steel strip surface and line speed. Coating defects are resulted from the unbalance of these control factors and the inaccuracy of coating equipments. This paper investigates the main cause of coating deviation and a new air knife system for control of coating thickness was developed. We investigate dynamic pressure variation by air knife types. It is found that the coating deviation is caused by the unbalance of dynamic pressure, the irregularity of strip position, and the strip vibration. Formulating a useful coating model by using present working condition, an optimal working condition is suggested. The productivity and coating quality are improved by applying the result of this research at the shop floor.

Keywords

References

  1. Iron steel Eng. DMC closed loop air knife control for galvanizing lines V.E.Harris(et al.)
  2. Iron Steel Eng. Integrated neural system for coating weight control of a hot dip galvanizing line S.W.Markward;Y.Z.Lu
  3. Proc.European Control Conf.,Grenoble,Paper No.32 Regulation of deposited zinc in hot-dip galvanizing Jacobs O.L.R;D.S.Chen
  4. Proc.Asia-Pacific Conf.on Measurement and Control Air Knife position skew control on hot-dip galvanizing line Chen.D.S
  5. Automatica v.31 no.5 Adaptive control of hot-dip Galvanizing Chen D.S https://doi.org/10.1016/0005-1098(94)00132-3
  6. 日立評論 v.57 no.5 連續亞鉛メツキ設備 梅田昭三;泰和宣;山口輝雄;今井辛義;江原勝也
  7. 鐵と鋼 v.66 no.7 연속식용융아연メツキの氣體絞り制御機構に關する檢討 阿部雅樹;失野秀勝;安谷屋武志
  8. 포항제철특별지원보고서 Edgeovercoaing 및 도금편차량 개선 배용환;최진원
  9. 서울대학교 정밀기계설계 공동연구소 보고서 Air Wiping Mechanism해석 이동호;남찬진