초록

Metallurgical characteristics of bonded region and high temperature mechanical properties of heat resistant alloy, Fe-35Ni-26Cr during liquid phase diffusion bonding were investigated employing AM17 insert metal. The insert metal for bonding, AM17 was newly developed Ni-base metal using interpolation method. Bonding of specimens were carried out at 1,403~1,463K for 600s in vacuum. The microconstituents in the bonded interlayer disappeared in the bonding temperature over 1,423K. The microstructures, alloying elements and hardness distribution in the base metal. The tensile strength and elongation of the joints at elevated temperatures were the same level as one of the base metal in the bonding temperature over 1,423K. The creep rupture strength and rupture lives of joints were almost identical to those of base metal.

키워드

참고문헌

  1. 鐵基耐熱鑄鋼 液相擴散接合繼手の高溫機械的特性の改善 望月
  2. 대한용접학회지 v.18 no.4 Fe-35Ni-26Cr주강 액상확산접함부의 고온기계적특성에 미치는 접합조건의 영향 김대업
  3. 대한용접학회지 v.18 no.5 액상확산접합용 인서트금속의 화학조성 최적화에 관한 연구 김대업;정승부;강정윤
  4. 日本金屬學會誌 v.49 no.4 鐵基ろら林を用いた耐熱鋼の液相擴散接合 中僑;鈴村;恩澤
  5. 溶接學會全國大會構演槪要 液相擴散接合の鋼管への應用 三浦
  6. 溶接學會論文集 v.8 no.2 Fe期およびNi基急冷凝固薄帶を用いたステンレス鋼管の接合 小溝;上野;富田;小川
  7. Weld. J. v.62 no.6 High Temperature Brazing of Stainleness Steel with Nickel-Base Filler Metals BNi-2, BNi-5 and BNi-7 E.Lugscheider
  8. 溶接學會論文集 v.9 no.4 合金粉末を用いた液相インサ-ト金屬散接合法の開發 中尾;西本;篠崎;姜;重田
  9. 대한용접학회지 v.13 no.3 Fe기내열합금의 액상확산접합용 삽입금속의 개발에 관한 여구 강정윤;김인배;이상래