Abstract
In order to synthesize the heat resistance ceramics of LAS system, we studied on preparing the fine powder with homogeneity by sol-gel method using metal alkoxide. Various results were obtained depending on the composition and process. When the amount of H2O added at initial stage is higher than 10mol/$\ell$, and when the amount of catalyst is 0.1mol/$\ell$, the particle size of synthesized hydrate becomes finer. On condition that partial prehydrolysis time of TEOS is more than 50 hours, the monosized fine powder is obtained(below 1${\mu}{\textrm}{m}$).