초록
The extraction of $Al_2O_3$ from the backed mixture of grinded aluminium silicates with $H_2SO_4$ and required heating energy for the baking process has been investigated. The extraction ration of $Al_2O_3$ from baked kaolin and alunite being mixed with 70-80% $H_2SO_4$ at 12$0^{\circ}C$ for 3 hours was more than 90%, the yield was based on alumina component in the ore by extracted with water. The required heating energy was 1782 cal/300gr (Alunite), that is, when alunite ore treated with equivalent amount of 80% $H_2SO_4$, also left it for 75 minites at 12$0^{\circ}C$, The required heating energy was 22, 553 cal/200gr(Alunite) when the above sample was heated again at 15$0^{\circ}C$ for 2 hours.