Acknowledgement
이 연구는 2020년도 정부(과학기술정보통신부)의 재원으로 한국연구재단의 지원을 받아 수행된 기초연구사업이다. (No.2015R1A5A 1037548)
For the development of high-fluidity concrete using low-binder, The effect of the use of the developed acrylic viscosity agent on the physical properties of concrete evaluated. The amount acrylic viscosity agent used was 0.28%, 0.29% and 0.30% based on the binder amount of 350kg/m3, and slump flow test, air volume measurement, U-Box passing test and strength compressive were conducted to determine the effect of the physical properties of concrete. it was judged that 0.29% of the cellulose type viscosity agent used in high-fluidity concrete using low-binder was most suitable.
이 연구는 2020년도 정부(과학기술정보통신부)의 재원으로 한국연구재단의 지원을 받아 수행된 기초연구사업이다. (No.2015R1A5A 1037548)