An Experimental Study on Compressive Strength and the Chloride Content of Concrete with Substitution Ratio of Recycled Fine Aggregate and Limestone Power

순환잔골재 및 석회석 미분말 치환율에 따른 콘크리트 강도와 염화물량에 관한 실험적 연구

  • Published : 2008.11.07

Abstract

Correspond in chloride content increase by sea sand uses of bad quality using recycled fine aggregate in this research. together, examined basic properties of matter for activation of been using recycled fine aggregate use definitely. Also, super fundamental principles that is shortcoming that blast furnace slag differential speech has prevents problem of decline and change of countenance limestone power differential speech by purpose to contribute in early age strength as Filler role special quality examine. As experiment result, compressive strength at recycled fine aggregate 10%, limestone power 20% metathesis the highest compressive strength value appear, According to recycled fine aggregate metathesis rate increase, the chloride content reduced by 0.127 ㎏/m$^3$s(metathesis rate 0%), 0.119 ㎏/m$^3$s (metathesis rate 10%), 0.112 ㎏/m$^3$s (metathesis rate l20%), 0.097 ㎏/m$^3$s (metathesis rate 30%).

본 연구에서는 순환잔골재를 사용하므로써 세척사 사용으로 인한 염화물량 증가에 대응하고 아울러 한정적으로 사용되고 있는 순환골재 사용의 활성화를 위해 기초적 물성을 검토하였다. 또한, 고로슬래그 미분말이 가지고 있는 단점인 초기강도 저하 및 변색의 문제점을 예방하기 위해 석회석 미분말을 Filler역할로써 초기강도에 기여할 목적으로 특성을 검토하였다. 실험방법으로는 예비실험을 통하여 세척사의 염화물량의 현수준 파악 및 LSP의 기초물성 실험을실시하여 치환율 범위를 설정하였으며. 본 실험에서는 배합인자를 16Factor로 나누어 슬럼프, 공기량,압축강도, 염화물 함유량을 측정하였다. 실험결과, 압축강도는 배합인자 B-b인 순환잔골재 10%, 석회석 미분말 20% 치환시 가장 높은 압축강도 값을 나타냈으며, 순환잔골재 치환율 증가에 따라 염화물량은 0.127㎏/m$^3$(치환율0%), 0.119㎏/m$^3$(치환율10%), 0.112㎏/m$^3$(치환율20%), 0.097㎏/m$^3$(치환율30%)로 저감되었다.

Keywords